EFFECTS OF SO42- ON THE CORROSION BEHAVIOR OF NiCu LOW ALLOY STEEL IN DEAERATED BICARBONATE SOLUTIONS

  • Yunfei LU ,
  • Junhua DONG ,
  • Wei KE
Expand
  • 1 Environmental Corrosion Center, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
    2 Wuhan the Second Ship Design and Research Institute, Wuhan 430064

Online published: 2015-07-16

Supported by

Supported by National Natural Science Foundation of China (No.51471175)

Abstract

High level radioactive waste (HLW) is an extremely dangerous by-product of the global nuclear industry. Due to its intensely radioactive nature and ultra long half-life, HLW has to be safely managed and disposed for thousands of years, isolated from the biosphere. Deep geological repository (DGR) is considered to be the most feasible option worldwide because of its operability, stability, durability, environmental protection and so on. Basically, DGR relies on a multibarrier system and it consists of metallic canisters, backfill materials and a stable geologic formation. Since radionuclides could be moved into the biosphere by action of groundwater, both the geologic formation and backfill materials have to be of very low hydraulic permeability and metal canisters have to be corrosion resistant and prevent contact between the groundwater and the radioactive waste for as long as possible. Low carbon steel has been selected and studied as a candidate canister material in many countries because its long industrial experience, high-strength, low cost and it is less prone to localized corrosion than materials that passivity, but its larger corrosion rate may also set an insuperable barrier for the practical application. Recently, our studies revealed that NiCu low alloy steel is a more promising candidate for the canister material compared with the popular one, low carbon steel, since the former performs a more acceptable corrosion rate without increasing much cost and has better resistance to localized corrosion in environments with high concentration of Cl-. In this work, effects of SO42-, another ubiquitous species in deep groundwater, on the corrosion behavior of NiCu low alloy steel during immersion in simulated deep groundwater environments were investigated by in situ electrochemical measurements and surface analysis techniques. Results show that the addition of SO42- can promote the substrate dissolution during the initial stage of immersion. In the later stage, SO42- weakens the protectiveness of formed films and consequently, active dissolution prevails on the electrode surface rather than the prepassivation. Concentrated SO42- and HCO3- can both promote the formation of Fe6(OH)12CO3. The main components of corrosion products are a-FeOOH, Fe3O4 and Fe6(OH)12CO3, and uniform corrosion is observed.

Key words: low alloy steel; rust; HCO3-; SO42-

Cite this article

Yunfei LU , Junhua DONG , Wei KE . EFFECTS OF SO42- ON THE CORROSION BEHAVIOR OF NiCu LOW ALLOY STEEL IN DEAERATED BICARBONATE SOLUTIONS[J]. Acta Metall Sin, 2015 , 51(9) : 1067 -1076 . DOI: 10.11900/0412.1961.2015.00133

References

[1] Taniguchi N, Suzuki H, Kawasaki M, Naito M, Kobayashi M, Takahashi R, Asano H. Corros Eng Sci Technol, 2011; 46: 117
[2] Kursten B, Druyts F, Macdonald D D, Smart N R, Gens R, Wang L, Weetjens E, Govaerts J, Corros Eng Sci Technol, 2011; 46: 91
[3] Macdonald D D, Urquidi-Macdonald M, Engelhardt G R, Azizi O, Saleh A, Almazooqi A, Rosas-Camacho O. Corros Eng Sci Technol, 2011; 46: 98
[4] Féron D, Crusset D, Gras J M. J Nucl Mater, 2008; 379: 16
[5] Bennett D G, Gens R. J Nucl Mater, 2008; 379 : 1
[6] King F, Padovani C. Corros Eng Sci Technol, 2011; 46: 82
[7] King F. Corrosion, 2013; 69: 986
[8] Guo Y H, Wang J, Lv C H, Liu S F, Zhong Z H. Earth Sci Front, 2005; 12( Suppl): 117 (郭永海, 王 驹, 吕川河, 刘淑芬, 钟自华. 地学前缘, 2005; 12(特刊): 117)
[9] Cao G L, Li G M, Chen S, Chang W S, Chen X Q. Acta Metall Sin, 2011; 47: 145 (曹国良, 李国明, 陈 珊, 常万顺, 陈学群. 金属学报, 2011; 47: 145)
[10] Matsushima I,Translated by Jing Y K. Low-Alloy Corrosion Resistant Steels: A History of Development, Application and Research. Beijing: Metallurgic Industry Press, 2004: 100 (松岛 岩著,靳裕康译. 低合金耐蚀钢——开发、发展及研究. 北京: 冶金工业出版社, 2004: 100)
[11] Kihira H, Kimura M. Corrosion, 2011; 67: 1
[12] Yang J F, Dong J H, Ke W. Acta Metall Sin, 2011; 47: 1321 (阳靖峰, 董俊华, 柯 伟. 金属学报, 2011; 47: 1321)
[13] Wen H L, Dong J H, Ke W, Chen W J, Yang J F, Chen N. Acta Metall Sin, 2014; 50: 275 (文怀梁, 董俊华, 柯 伟, 陈文娟, 阳靖峰, 陈 楠. 金属学报, 2014; 50: 275)
[14] Lu Y F, Yang J F, Dong J H, Ke W. Acta Metall Sin, 2015; 51: 440 (卢云飞, 阳靖峰, 董俊华, 柯 伟. 金属学报, 2015; 51: 440)
[15] Lu Y F, Dong J H, Ke W. J Mater Sci Technol, accepted.
[16] Lu Y F, Dong J H, Ke W. J Mater Sci Technol, doi:
[17] Dong J H, Nishimura T, Kodama T. MRS Symp Process, 2002; 713: 105
[18] Bockris J O M, Drazic D, Despic A R. Electrochim Acta, 1961; 4: 325
[19] Davies D H, Burstein G T. Corrosion, 1980; 36: 416
[20] Burstein G T, Davies D H. Corros Sci, 1980; 20: 1143
[21] Cao C N,Zhang J Q. Introduction of Electrochemical Impedance Spectroscopy. Beijing: Science Press, 2002: 135 (曹楚南,张鉴清. 电化学阻抗谱导论. 北京: 科学出版社, 2002: 135)
[22] Sherar B W A, Keech P G, Qin Z, King F, Shoesmith D W. Corrosion, 2010; 66: 045001-1
[23] Genin J M R, Bourrie G, Trolard F, Abdelmoula M, Jaffrezic A, Refait P, Maitre V, Humbert B, Herbillon A. Environ Sci Technol, 1988; 32: 1058
[24] Larroumet D, Greenfield D, Akid R, Yarwood J. J?Raman?Spectrosc, 2008; 39: 1740
[25] Drissi S H, Refait P, Abdelmoula M, Genin J M R. Corros Sci, 1995; 37: 2025
Outlines

/

〈 〉