STUDY ON THE PREPARATION PROCESS OF T2 ALLOY IN THE Mo-Si-B SYSTEM

  • Kunming PAN ,
  • Laiqi ZHANG ,
  • Shizhong WEI ,
  • Jiwen LI ,
  • Hao LI ,
  • Junpin LIN
Expand
  • 1 Engineering Research Center of Tribology and Materials Protection, Ministry of Education, Henan University of Science and Technology, Luoyang 471023
    2 State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083
    3 School of Materials Science and Engineering, Luoyang Institute of Science and Technology, Luoyang 471023

Online published: 2015-07-07

Supported by

Supported by National Natural Science Foundation of China (Nos.50871012 and U1504514), Program for Changjiang Scholars and Innovative Research Team in University (No.IRT1234) and Science & Technology Project of Henan Province (No.20140401)

Abstract

Mo5SiB2 (T2) can be used as a promising elevated-temperature structural material because of its high melting temperature (about 2200 ℃), and excellent resistance to oxidation and creep. The Mo5SiB2 (T2) alloy was prepared by both spark plasma sintering (SPS) and tube furnace sintering (TFS), and then the microstructures were characterized by XRD, SEM-EDS and TEM. The results show that the rapid heating rate is one of important dynamic conditions responsible for the synthesis of T2. Compared with traditional methods, SPS can provide the fast synthesis in a particular way of labilized plasma sintering so that the sample can be heated to the expected temperature of 1500 ℃ with a short period. The melted Si can rapidly react with Mo and B to synthesize T2 in the solid-liquid state prior to the formation of binary phases (Mo3Si, Mo5Si3, MoB, etc.) in the solid state in the range of 600~1200 ℃. The average size of grains is equal to 1.44 μm. The boundaries are clear and have the shape of a straight line without transition zones. Moreover, no defects such as dislocations were found in the T2 alloys prepared by SPS.

Cite this article

Kunming PAN , Laiqi ZHANG , Shizhong WEI , Jiwen LI , Hao LI , Junpin LIN . STUDY ON THE PREPARATION PROCESS OF T2 ALLOY IN THE Mo-Si-B SYSTEM[J]. Acta Metall Sin, 2015 , 51(11) : 1377 -1383 . DOI: 10.11900/0412.1961.2015.00053

References

[1] Depka T, Somsen C, Eggeler G, Mukherji D, R?sler J, Krüger M, Saage H, Heilmaier M. Mater Sci Eng, 2009; A510-511: 337
[2] Sakidja R, Perepezko J H, Kim S. Acta Mater, 2008; 56: 5223
[3] Zhang F, Zhang L, Shan A, Wu J. Intermetallics, 2006; 14: 406
[4] Mandal P, Thom A J, Kramer M J. Mater Sci Eng, 2004; A371: 335
[5] Meyer M K, Kramer M J, Akinca M. Intermetallics, 1996; 4: 273
[6] Nunes C A, Sakidja R, Dong Z. Intermetallics, 2000; 8: 327
[7] Pan K M, Liu W, Zhang L Q, Wei S Z, You L, Lin J P, Li J W, Xu L J, Zhou S Z, Han M R. Mater Sci Eng, 2015; A623: 124
[8] Zhang L Q, Pan K M, Du W, Wang M, Lin J P, Ni X D, Shang H K, Sun J H. Intermetallics, 2014; 50: 79
[9] Pan K M, Zhang L Q, Wang J, Du W, Lin J P. Acta Metall Sin, 2013; 49: 1392 (潘昆明, 张来启, 王 珏, 杜 伟, 林均品. 金属学报, 2013; 49: 1392
[10] Zhang L Q, Pan K M, Lin J P. Intermetallics, 2013; 38: 49
[11] Rawn C J, Schneibel J H, Hoffmann C M. Intermetallics, 2001; 9: 209
[12] Yamauchi A, Yoshimi K, Kurokawa K. J Alloys Compd, 2007; 434-435: 420
[13] Abbasi A R, Shamanian M. Mater Sci Eng, 2011; A528: 3295
[14] Urquhart A W. Mater Sci Eng, 1991; A144: 75
[15] Wan D T, Zhou Y C, Bao Y W. Ceram Int, 2006; 32: 883
[16] Pan K M, Zhang L Q, Wang J, Lin J P, Chen G L. Surf Interface Anal, 2013; 45: 955
[17] Nesmeianov A N. Vapor Pressure of the Chemical Elements. Amsterdam: Elsevier Pub. Co., 1963: 85
[18] Mandal P, Thom A J, Kramer M J. Mater Sci Eng, 2004; A371: 335
[19] Deevi S C, Thadhani N N. Mater Sci Eng, 1995; A192-193: 604
[20] Shen Z, Johnsson M, Zhao Z. J Am Ceram Soc, 2002; 85: 1921
[21] Ls D, Gurry R W. Physical Chemistry of Metals. Tokyo: McGraw-Hill Book Company and Kogakusha Company Ltd., 1993: 126
[22] Zhang L Q, Huang L. J Univ Sci Technol Beijing, 2008; 30: 281 (张来启, 黄 蕾, 北京科技大学学报, 2008; 30: 281)
[23] Yoon J, Lee J, Lee K. Intermetallics, 2003; 11: 687
[24] Rosales I, Schneibel J H. Intermetallics, 2000; 8: 885
[25] Str?m E. Mater Charact, 2005; 55: 402
[26] Huebsch J. Intermetallics, 2000; 8: 143
[27] Hayashi T, Ito K, Numakura H. Intermetallics, 2005; 13: 93
[28] Wang S W, Chen L D, Hirai T. J Mater Res, 2000; 15: 982
Outlines

/

〈 〉