EFFECT OF Zr ADDITION ON MICROSTRUCTURE AND OXIDATION RESISTANCE OF Nb-Ti-Si BASE ULTRAHIGH-TEMPERATURE ALLOYS
Online published: 2015-07-06
Supported by
Supported by National Natural Science Foundation of China (Nos.51371145, 51431003, U1435201 and 51401166)
Nb-Ti-Si base in situ composites which consist of Nb solid solution (Nbss) and silicides (a-Nb5Si3, b-Nb5Si3, g-Nb5Si3 and/or Nb3Si) phases, have shown great potential as alternative materials to Ni-based superalloys due to their high melting points (beyond 1700 ℃), good formability, low density (6.6~7.2 g/cm3) and high strength. However, a major hindrance to the applications of these alloys at elevated temperatures is their poor oxidation resistance. Alloying is an effective method to improve the integrated properties of the alloys, especially for the oxidation resistance. Up to now, many beneficial elements such as Ti, Al, Cr and Sn have been employed to ameliorate their oxidation resistance. Nevertheless, there is no systematic and comprehensive investigation on the effect of Zr contents on the microstructure and oxidation behavior of the alloys based on Nb-Ti-Si system. The aim of this work is to clarify the effects of Zr contents on phase selection, microstructure and high temperature oxidation resistance of Nb-Ti-Si based alloys in detail. The constituent phases, microstructure and composition of the alloys under as-cast state and after oxidation were investigated by OM, XRD, SEM and EDS. Thus, six Nb-Ti-Si base ultrahigh-temperature alloys with compositions of Nb-22Ti-15Si-5Cr-3Hf-3Al-xZr (x=0, 0.5, 1, 2, 4, 8, atomic fraction, %) were prepared by vacuum non-consumable arc-melting. The results show that the alloys with different Zr contents are mainly composed of Nbss and g-(Nb, X)5Si3 (X represents Ti, Hf, Cr and Zr). However, the addition of Zr has an obvious affect on the microstructure of Nb-Ti-Si base alloys. Both the sizes and amounts of primary g-(Nb, X)5Si3 increase with increase in Zr contents. Alloys with different Zr contents were oxidized at 1250 ℃ for 1~50 h, respectively. It is found that both adhesion and compactness of the scales are improved effectively by increase in Zr contents. The scales of alloys with higher Zr contents (x=4 and 8) after oxidation for 50 h show an obvious layered structure: the outmost layer is only composed of TiO2, the middle layer mainly consists of ZrO2, TiNb2O7 and TiO2, and the inner layer is mainly comprised of Si-rich oxides. The mass gain per unit area and the thickness of the scale after oxidation decrease with increase in Zr contents in the alloys, indicating that the addition of Zr can improve the oxidation resistance of the alloys significantly.
Yuxiang ZENG , Xiping GUO , Yanqiang QIAO , Zhongyi NIE . EFFECT OF Zr ADDITION ON MICROSTRUCTURE AND OXIDATION RESISTANCE OF Nb-Ti-Si BASE ULTRAHIGH-TEMPERATURE ALLOYS[J]. Acta Metall Sin, 2015 , 51(9) : 1049 -1058 . DOI: 10.11900/0412.1961.2015.00092
| [1] | Bewlay B P, Jackson M R, Lipsitt H A. Metall Mater Trans, 1996; 27A: 3801 |
| [2] | Grammenos I, Tsakiropoulos P. Intermetallics, 2010; 18: 242 |
| [3] | Bewlay B P, Jackson M R, Zhao J C, Subramanian P R. Metall Mater Trans, 2003; 34A: 2043 |
| [4] | Wu C L, Zhou L Z, Guo J T. Acta Metall Sin, 2006; 42: 1061 (伍春兰, 周兰章, 郭建亭. 金属学报, 2006; 42: 1061) |
| [5] | Kang Y W, Qu S Y, Song J X, Han Y F. Acta Metall Sin, 2008; 44: 593 (康永旺, 曲士昱, 宋尽霞, 韩雅芳. 金属学报, 2008; 44: 593) |
| [6] | Jia L N, Gao M, Ge J R, Zheng L J, Sha J B, Zhang H. Acta Metall Sin, 2011; 47: 88 (贾丽娜, 高 明, 盖京茹, 郑立静, 沙江波, 张 虎. 金属学报, 2011; 47: 88) |
| [7] | Wang J, Guo X P, Guo J M. Chin J Aeronaut, 2009; 22: 544 |
| [8] | Zhang S, Guo X P. Intermetallics, 2015; 57: 83 |
| [9] | Xiong B W, Cai C C, Wan H, Zheng Y H. J Alloys Compd, 2009; 486: 330 |
| [10] | Guo J M, Guo X P, Song S G. Acta Metall Sin, 2008; 44: 574 (郭金明, 郭喜平, 宋曙光. 金属学报, 2008; 44: 574) |
| [11] | Zelenitsas K, Tsakiropoulos P. Mater Sci Eng, 2006; A416: 269 |
| [12] | Geng J, Tsakiropoulos P, Shao G S. Mater Sci Eng, 2006; A441: 26 |
| [13] | Li Z F, Tsakiropoulos P. Intermetallics, 2012; 26: 18 |
| [14] | Wang L G, Jia L N, Cui R J, Zheng L J, Zhang H. Chin J Aeronaut, 2012; 25: 292 |
| [15] | Grammenos I, Tsakiropoulos P. Intermetallics, 2011; 19: 1612 |
| [16] | Geng J, Tsakiropoulos P. Intermetallics, 2007; 15: 382 |
| [17] | Behrani V, Thom A J, Kramer M J, Akinc M. Intermetallics, 2006; 14: 24 |
| [18] | Vellios N, Tsakiropoulos P. Intermetallics, 2010; 18: 1729 |
| [19] | Vellios N, Tsakiropoulos P. Intermetallics, 2007; 15: 1518 |
| [20] | Yuan W H, Liang Z Y. Mater Des, 2011; 32: 4195 |
| [21] | Mousa M, Wanderka N, Timpel M, Singh S, Krüger M, Heilmaier M, Banhart J. Ultramicroscopy, 2011; 111: 706 |
| [22] | Gorr B, Wang L, Burk S, Azim M, Majumdar S, Christ H J, Mukherji D, R?sler J, Schliephake D, Heilmaier M. Intermetallics, 2014; 48: 34 |
| [23] | Yu Q H, Zhou C G, Zhang H Y, Zhao F. J Eur Ceram Soc, 2010; 30: 889 |
| [24] | Li X, Guo X P, Qiao Y Q. Oxid Met, 2015; 83: 253 |
| [25] | Li X, Guo X P. Acta Metall Sin, 2012; 48: 1394 (李 轩, 郭喜平. 金属学报, 2012; 48: 1394) |
| [26] | Tian Y X, Guo J T, Sheng L Y, Cheng G M, Zhou L Z, He L L, Ye H Q. Intermetallics, 2008; 16: 807 |
| [27] | Li X F, Guo X P. Acta Metall Sin, 2013; 49: 853 (李小飞, 郭喜平. 金属学报, 2013; 49: 853) |
| [28] | Liu A Q, Sun L, Li S S, Han Y F. J Rare Earth, 2007; 25: 474 |
| [29] | Lee D B, Woo S W. Intermetallics, 2005; 13: 169 |
/
| 〈 |
|
〉 |