EFFECT OF SOLUTION TEMPERATURE ON MICRO- STRUCTURE AND PITTING CORROSION RESISTANCE OF S32760 DUPLEX STAINLESS STEEL

  • Yulai CHEN ,
  • Zhaoyin LUO ,
  • Jingyuan LI
Expand
  • 1 Metallurgical Engineering Research Institute, University of Science and Technology Beijing, Beijing 100083
    2 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083

Online published: 2015-07-06

Supported by

Supported by National Natural Science Foundation of China (No.51174026), National Science and Technology Pillar Program of the Twelfth Five-Year Plan (No.2012BAE04-B02)

Abstract

In order to obtain the optimal corrosion resistance, the characteristics of microstructure and alloy elements distribution of S32760 duplex stainless steel were studied after solid solution treatment at various temperatures from 1000 ℃ to 1300 ℃ by means of OM, EPMA, SEM, EDS and TEM. In addition, the pitting corrosion resistance was measured by the electrochemical workstation. The results show that the N atoms diffused into d phase from g phase during solution treatment when the temperature was higher than 1080 ℃. N atoms migrated back into g phase when the subsequent cooling was slow enough. However, Cr2N phase in situ precipitated during quenching because there was not enough time for the N atoms to diffuse back into g phase. Cr2N particles increased with the solution temperature increasing. Furthermore, s phase precipitated when the tested sheet was heat treated at or below 1040 ℃ due to the high content of N. Thus it is obvious that the solution temperature range of the S32750 duplex stainless steel is quite narrow, which is between 1040 ℃ and 1080 ℃, and it is confirmed that the optimal temperature is 1060 ℃. After treated at 1060 ℃ for 60 min, the Brinell hardness of S32760 steel is 249 HBW, pitting potential is up to 1068 mV and the passive current density is as low as 1.48×10-4 A/cm2.

Cite this article

Yulai CHEN , Zhaoyin LUO , Jingyuan LI . EFFECT OF SOLUTION TEMPERATURE ON MICRO- STRUCTURE AND PITTING CORROSION RESISTANCE OF S32760 DUPLEX STAINLESS STEEL[J]. Acta Metall Sin, 2015 , 51(9) : 1085 -1091 . DOI: 10.11900/0412.1961.2015.00044

References

[1] Gurrappa I, Krishna Reddy C V. J Mater Process Technol, 2007; 182: 195
[2] Huang C S, Shih C C. Mater Sci Eng, 2005; A402: 66
[3] Migiakis K, Daniolos N, Papadimitriou G D. Mater Manuf Processes, 2010; 25: 598
[4] Sun X G. Shanxi Metall, 2013; (3): 6 (孙晓刚. 山西冶金, 2013; (3): 6)
[5] Wu J. Duplex Stainless Steel. Beijing: Metallurgy Industry Press, 1999: 8 (吴 玖. 双相不锈钢. 北京: 冶金工业出版社, 1999: 8)
[6] Yang S M, Chen Y C, Chen C H, Huang W P, Lin D Y. J Alloys Compd, 2015; 633: 48
[7] Fargas G, Anglada M, Mateo A. J Mater Process Technol, 2009; 209: 1770
[8] Bettini E, Kivis?kk U, Leygraf C, Pan J. Electrochim Acta, 2013; 113: 280
[9] Du J, Wang C, Wang K, Chen K. Intermetallics, 2014; 45: 80
[10] Chen X H, Ren X P, Xu H, Tong J G, Zhang H Y. Int J Min Met Mater, 2012; 19: 518
[11] Zanotto F, Grassi V, Merlin M, Balbo A, Zucchi F. Corros Sci, 2015; 94: 38
[12] Lacerda J C, Candido L C, Godefroid L B. Int J Fatigue, 2015; 74: 81
[13] Migiakis K, Papadimitriou G D. J Mater Sci, 2009; 44: 6372
[14] Elsabbagh F M, Hamouda R M, Taha M A. J Mater Eng Perform, 2014; 23: 275
[15] Xiang H L, He F S, Liu D. Acta Metall Sin, 2009; 45: 1456 (向红亮, 何福善, 刘 东. 金属学报, 2009; 45: 1456)
[16] Udayakumar T, Raja K, Afsal Husain T M, Sathiya P. Mater Des, 2014; 53: 226
[17] de Messano L V R, Sathler L, Reznik L Y, Coutinho R. Int Biodeter Biodegr, 2009; 63: 607
[18] Chen W, Wang X Y, Wang D Y, Zhang H G. Heat Treat, 2013; (3): 45 (陈 炜, 王晓燕, 王冬颖, 张会国. 热处理, 2013; (3): 45)
[19] Yan K R. Metall Collections, 1994; (1): 28 (颜宽然. 冶金丛刊, 1994; (1): 28)
[20] Li R S, Wang Z Y. Acta Metall Sin, 1994; 30: 477 (李仁顺, 王佐义. 金属学报, 1994; 30: 477)
[21] Xiang H L, Huang W L, Liu D, He F S. Acta Metall Sin, 2010; 46: 304 (向红亮, 黄伟林, 刘 东, 何福善. 金属学报, 2010; 46: 304)
[22] Garfias-Mesias L F, Sykes J M, Tuck C D S. Corros Sci, 1996; 38: 1319
[23] Yong Q L. Secondary Phases in Steels. Beijing: Metallurgy Industry Press, 2006: 7 (雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 7)
[24] Zhao J L, Xiao X S, Xu M H, Fang J X, Li J, Li M. Shanghai Steel Iron Res, 2006; (3): 33 (赵钧良, 肖学山, 徐明华, 方静贤, 李 钧, 李 明. 上海钢研, 2006; (3): 33)
[25] Comer A, Looney L. Int J Fatigue, 2006; 28: 826
Outlines

/

〈 〉