RELATIONSHIP BETWEEN THE EVOLUTION OF PHASE PARAMETERS OF GRAIN BOUNDARY M23C6 AND EMBRITTLEMENT OF HR3C SUPER-HEATER TUBES IN SERVICE

  • Zhifang PENG ,
  • Wen REN ,
  • Chao YANG ,
  • Fangyu CHEN ,
  • Hongguo LIU ,
  • Fangfang PENG ,
  • Qingsong MEI
Expand
  • 1 School of Power and Mechanical Engineering, Wuhan University, Wuhan 430072
    2 Jiangsu Frontier Electric Technology Co. Ltd., Nanjing 211102
    3 Research Institute of Wuhan Iron and Steel (Group) Corp., Wuhan 430080
    4 Shenhua (Fujian) Energy Co. Ltd., Fuzhou 350004
    5 Dongfang Boiler Group Co. Ltd., Zigong 643000

Online published: 2015-06-23

Abstract

The relationship of the evolution of the phase parameters (area fraction ? M 23 C 6 and equivalent width W ) of grain boundary M23C6 plates with the embrittlement of HR3C super-heater tube samples in service was studied. Based on the ASTM E112 standard charts, the total length of two dimensional austenite grain boundaries (Lgb) corresponding to each grain size number (GL) was determined in the observed area of the metallographic images and expressed as Lgb (GL). Making use of the SEM-SE images of the samples, the ? M 23 C 6 and W were determined. The relationships of W with GL and ? M 23 C 6 were established as W(GL, ? M 23 C 6 ). Combined with the result from a Charpy impact test, the function of the impact value (aKV) as the W was obtained. In addition, the grain boundary elastic modulus (Er) was measured by a nano-hardness test. The result shows that intergranular fracture occurred on all the room temperature impact test specimens taken from the super-heater tubes exposed under the operating conditions. The W was increased with the decrease of GL and the increase of Er at a constant ? M 23 C 6 , causing a corresponding decrease of aKV, and hence promoting the embrittlement of the HR3C super-heater tubes. The related mechanism for the intergranular fracture caused by the increase of the equivalent width W of grain boundary carbides (carbide coarsening) can be explained through the application of the proposed method.

Cite this article

Zhifang PENG , Wen REN , Chao YANG , Fangyu CHEN , Hongguo LIU , Fangfang PENG , Qingsong MEI . RELATIONSHIP BETWEEN THE EVOLUTION OF PHASE PARAMETERS OF GRAIN BOUNDARY M23C6 AND EMBRITTLEMENT OF HR3C SUPER-HEATER TUBES IN SERVICE[J]. Acta Metall Sin, 2015 , 51(11) : 1325 -1332 . DOI: 10.11900/0412.1961.2015.00077

References

[1] Yang F,Zhang Y L,Ren Y N,Li W M. New Heat-Resistant Steels Welding. Beijing: China Electric Power Press, 2006: 143 (杨 富,章应霖,任永宁,李为民. 新型耐热钢焊接. 北京: 中国电力出版社, 2006: 143)
[2] Iseda A, Okada H, Semba H, Igarashi M. Energy Mater, 2007; 2(4): 199
[3] Fang Y Y, Zhao J, Li X N. Acta Metall Sin, 2010; 46: 844 (方园园, 赵 杰, 李晓娜. 金属学报, 2010; 46: 844)
[4] Komai N,Igarashi M,Minami Y,Mimura H,Masuyama F,Prager M,Boyles P R. In: American Society of Mechanical Engineers ed.,2007 Proc ASME Pressure Vessels and Piping Conference-8th Int Conf on Creep and Fatigue at Elevated Temperatures-CREEP, New York: ASME, 2007: 203
[5] Hu P. Electr Power Constr, 2005; 26(6): 26 (胡 平. 电力建设, 2005; 26(6): 26)
[6] Jiang Z S, Dong W G, Mao G G. Electr Power Constr, 2007; 28(8): 7 (江哲生, 董卫国, 毛国光. 电力建设, 2007; 28(8): 7)
[7] Sun Y Z. Electr Power Constr, 2003; 24(9): 11 (孙叶柱. 电力建设, 2003; 24(9): 11)
[8] Yin Z, Cai H, Liu H G. Proc Chin Soc Elec Eng, 2011; 31: 103 (殷 尊, 蔡 晖, 刘鸿国. 中国电机工程学报, 2011; 31: 103 )
[9] Du B S, Wei Y Z, Zhang Z W, Li X M, Liu R. Trans Mater Heat Treatment, 2014; 35(12): 84 (杜宝帅, 魏玉忠, 张忠文, 李新梅, 刘 睿. 材料热处理学报, 2014; 35(12): 84 )
[10] Okada H,Igarashi M,Yamamoto S,Miyahara O,Iseda A,Komai N,Masuyama F. In: American Society of Mechanical Engineers ed., 2007 Proc ASME Pressure Vessels and Piping Conference-8th Int Conf on Creep and Fatigue at Elevated Temperatures-CREEP, New York: ASME, 2007: 181
[11] Li T J, Liu F G, Fan C X, Yao B Y. Hot Working Technol, 2010; 39(14): 43 (李太江, 刘福广, 范长信, 姚兵印. 热加工工艺, 2010; 39(14): 43 )
[12] Bai X, Pan J, Chen G, Liu J, Wang J, Zhang T, Tang W. Mater Sci Technol, 2014; 30(2): 205
[13] Zhen Z J. Boiler Technol, 2011; 42(4): 46 (郑子杰. 锅炉技术, 2011; 42(4): 46 )
[14] Gao J Q, Hong J, Zhou Y D, Toda Y, Wang Q J, Liu J L. Metall Anal (Suppl.: Phys), 2012; 32: 172 (高加强, 洪 杰, 周冶东, 户田佳明, 王起江, 刘俊亮. 冶金分析(增刊: 物理分册), 2012; 32: 172)
[15] Peng B C, Zhang H X, Hong J, Gao J Q, Wang Q J, Zhang H Q. Mater Sci Eng, 2010; A527:1957
[16] Peng Z F, Peng F F, Chen F Y. In: Gandy D, Shingledecker J eds., Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference (EPRI 2013), Waikoloa, Hawaii, USA: ASM International, 2013: 1151
[17] Shen Q, Liu H G, Tang L Y. Electr Power Constr, 2009; 30(9): 62 (沈 琦, 刘鸿国, 唐丽英. 电力建设, 2009; 30(9): 62)
Outlines

/

〈 〉