RESEARCH ON THE INTERFACIAL HEAT TRANSFER COEFFECIENT BETWEEN CASTING AND CERAMIC SHELL IN INVESTMENT CASTING PROCESS OF Ti6Al4V ALLOY

  • Heng SHAO ,
  • Yan LI ,
  • Hai NAN ,
  • Qingyan XU
Expand
  • 1 Key Laboratory for Advanced Materials Processing Technology, Ministry of Education, School of Materials Science and Engineering, Tsinghua University, Beijing 100084
    2 Beijing Institute of Aeronautical Materials, Beijing 100095

Accepted date: 2015-05-02

  Online published: 2015-06-16

Supported by

Supported by China-EU (European Union) Science & Technology Cooperation in Aviation, 7th Framework Programme of EU, National Basic Research Program of China (No.2011CB706801), National Natural Science Foundation of China (Nos.51171089 and 51374137), National Science and Technology Major Project (No.2012ZX04012011) and High Technology Research and Development Program of China (No.2007AA04Z141)

Abstract

Investment casting process is an important way to get complex parts of titanium alloy. However there are few research on the interfacial heat transfer coefficient (h) between casting and shell thus the temperature simulation of investment casting process of titanium alloy is often inaccurate. In order to get a relatively accurate h, a one-dimensional mathematical model for the reverse calculation of h between casting and shell in investment casting process of Ti6Al4V alloy was built and the analytic relationship between temperature and time/heat flux was established. Considering the calculated h is significantly affected by the error of parameters such as the specific heat capacity and thermal diffusivity of shell and position of thermocouples, research on the error of these parameters is essential. The relationship between the error of these parameters and the temperatures in the casting and shell was studied and it was found that the effect of different kind of error on the temperature field was obviously different. An experiment based on the one-dimensional mathematical model was done and temperatures of different positions were measured. Based on the effect of different kind of error and the difference between the calculate temperature field and the measured temperatures, the proportion of effect of each kind of error was assessed. These errors were revised on the basis of the assessment, thus a relatively accurate h between the casting and shell was obtained. The relationships between h and thickness of the solidified layer on the casting/temperature at the surface of casting can be divided into 4 stages: (1) Metal was liquid and h kept about 440 W/(m2K); (2) Solid layer appeared on the surface, and h declined nearly 60%; (3) Solid layer grew up before metal became completely solid and h declined nearly 20% of its maximum; (4) After metal solidified, h declined slowly as temperature on the surface of casting dropped. These relationships were applied in a three-dimensional model for numerical simulation of the temperature field. Temperatures of different positions in casting and shell were calculated and calculated temperatures agreed with measured ones well. Thus the accuracy of h was identified and it can help solve problems in the production in investment casting process of Ti6Al4V alloy.

Cite this article

Heng SHAO , Yan LI , Hai NAN , Qingyan XU . RESEARCH ON THE INTERFACIAL HEAT TRANSFER COEFFECIENT BETWEEN CASTING AND CERAMIC SHELL IN INVESTMENT CASTING PROCESS OF Ti6Al4V ALLOY[J]. Acta Metall Sin, 2015 , 51(8) : 976 -984 . DOI: 10.11900/0412.1961.2015.00037

References

[1] Liu J, Yang Y, Lu D. Foundry, 2008; 57: 1155 (刘 剑, 杨 屹, 卢 东. 铸造, 2008; 57: 1155)
[2] Atwood R C, Lee P D, Curtis R V, Maijer D M. Dent Mater, 2007; 23(1): 60
[3] Liang Z J, Xu Q Y, Li J T, Li S Q, Zhang J, Liu B C, Zhong Z Y. Rare Met Mater Eng, 2003; 32: 164 (梁作俭, 许庆彦, 李俊涛, 李世琼, 张 继, 柳百成, 仲增墉. 稀有金属材料与工程, 2003; 32: 164)
[4] Guo Z P, Xiong S M, Cho S H, Choi J K. Acta Metall Sin, 2007; 43: 1149 (郭志鹏, 熊守美, 曹尚铉, 崔正吉. 金属学报, 2007; 43: 1149)
[5] Guo Z P, Xiong S M, Cho S H, Choi J K. Acta Metall Sin, 2007; 43: 1155 (郭志鹏, 熊守美, 曹尚铉, 崔正吉. 金属学报, 2007; 43: 1155)
[6] Cao Y Y, Guo Z P, Xiong S M. China Foundry, 2014; 11: 314
[7] Guo Z P, Xiong S M, Liu B C, Mei L, Allison J. Int J Heat Mass Transfer, 2008; 51: 6032
[8] Long A, Thornhill D, Armstrong C, Watson D. Appl Therm Eng, 2011; 31: 3996
[9] O'Mahoney D, Browne D J. Exp Therm Fluid Sci, 2000; 22: 111
[10] Yuan S, Bu K, Dong Y W. Foundry Technol, 2012; 33: 177 (袁 帅, 卜 昆, 董一巍. 铸造技术, 2012; 33: 177)
[11] Konrad C H, Brunner M, Kyrgyzbaev K, V?lkl R, Glatzel U. J Mater Process Technol, 2011; 211: 181
[12] Zhang W H, Xie G N, Zhang D. Exp Therm Fluid Sci, 2010; 34: 1068
[13] Dong Y W, Bu K, Dou Y Q, Zhang D H. J Mater Process Technol, 2011; 211: 2123
[14] Rafique M M A, Iqbal J. Int J Heat Mass Transfer, 2009; 52: 2132
[15] Jin H P, Li J R, Yu J, Liu S Z. Rare Met Mater Eng, 2010; 39: 767
[16] Sun Z Z, Hu H, Niu X P. J Mater Process Technol, 2011; 211: 1432
[17] Ilkhchy A F, Jabbari M, Davami P. Int Commun Heat Mass Transfer, 2012; 39: 705
[18] Aweda J O, Adeyemi M B. J Mater Process Technol, 2009; 209: 1477
[19] Xu H, Hou H, Zhao Y H, Chen Z. Chin J Nonferrous Met, 2003; 13: 881 (徐 宏, 侯 华, 赵宇宏, 陈 铮. 中国有色金属学报, 2003; 13: 881)
[20] Palumbo G, Piglionico V, Piccininni A, Guglielmi P, Sorgente D, Tricarico L. Appl Therm Eng, 2015; 78: 682
[21] Chen L P, Wang Y X, Peng L M, Fu P H, Jiang H Y. Exp Therm Fluid Sci, 2014; 54: 196
[22] Wang Z F, Yao M, Wang X D, Zhang X B, Yang L S, Lu H Z, Wang X. J Mater Process Technol, 2014; 214: 44
[23] Watanabe K, Miyakawa O, Takada Y, Okuno O, Okabe T. Biomaterials, 2003; 24: 1737
[24] Liang Z J, Xu Q Y, Li J T, Li S Q, Zhang J, Liu B C, Zhong Z Y. Rare Met Mater Eng, 2002; 31: 353 (梁作俭, 许庆彦, 李俊涛, 李世琼, 张 继, 柳百成, 仲增墉. 稀有金属材料与工程, 2002; 31: 353)
[25] Beck J V, Blackwell B, St Clair C R. Inverse Heat Conduction: Ill-Posed Problems. New York: Wiley, 1985: 145
Outlines

/

〈 〉