EFFECT OF Mn PRE-PARTITIONING ON C PARTITIONING AND RETAINED AUSTENITE OF Q&P STEELS
Received date: 2014-08-18
Online published: 2015-07-23
Supported by
National Natural Science Foundation of China (Nos.51254004 and 51304186), Natural Science Foundation of Hebei Province (No.E2014209191) and Science Foundation of Department of Education of Hebei Province (No.YQ2013003)
The chemical compositions of C and Mn have a strong influence on the stability of the metastable retained austenite at room temperature. In the intercritical annealing process, Mn element improves the stability of the austenite by partitioning from ferrite to austenite and the enrichment of Mn in austenite can also impact on the diffusion of C element from martensite to retained austenite in partitioning process. Based on C partitioning, Mn partitioning can further improve the product of strength and elongation, and has no negative effect on weldability of the low carbon high strength steel. Thus, it can effectively solve the contradiction between mechanical property and weldability of low carbon high strength steel in traditional quenching-partitioning (Q&P) process. In this case, it is of great significance to study the Mn pre-partitioning mechanism and its influence on C partitioning and retained austenite of the low carbon high strength steel. Therefore, one low alloy C-Si-Mn steel was studied in the present work. The Mn pre-partitioning behavior and its effect on C partitioning and the stability of the retained austenite were investigated by means of intercritical heating-quenching (IQ) process, Q&P and intercritical heatingaustenitizing-quenching-partitioning (I&Q&P) process. The results showed that during the process of phase transformation in the intercritical reheating, C and Mn elements constantly diffused from ferrite to austenite. When this process ended, C and Mn elements enriched in austenite. While Mn element in microstructure at room temperature was still enrichment and C element enriched regularly between the martensite laths in the I&Q&P treated steel. With the increase of C partitioning time in both Q&P and I&Q&P process, the tensile strength of steel was decreased constantly, while the elongation showed an increasing fristly and then decreasing trend. The product of strength and elongation of the steel treated by I&Q&P process reached 23478 MPa·% with the C partitioning time of 90 s. The more austenite in martensite phase would be obtained after the first quenching with the Mn pre-partitioning. It was important to prompt more C diffusing into austenite during C partitioning process to stabilize more retained austenite at room temperature of the steel after the second quenching. With the same experimental conditions, the retained austenite of the combined effects of C and Mn partitioning during I&Q&P process would be increased 2.4% than the effect of C partitioning during Q&P process.
Liansheng CHEN , Jianyang ZHANG , Yaqiang TIAN , Jinying SONG , Yong XU , Shihong ZHANG . EFFECT OF Mn PRE-PARTITIONING ON C PARTITIONING AND RETAINED AUSTENITE OF Q&P STEELS[J]. Acta Metall Sin, 2015 , 51(5) : 527 -536 . DOI: 10.11900/0412.1961.2014.00462
| [1] | Speer J G, Assun??o F C R, Matlock D K, Edmonds D V. Mater Res, 2005; 8: 417 |
| [2] | Edmonds D, He K, Rizzo F, De Cooman B, Matlock D, Speer J. Mater Sci Eng, 2006; A438: 25 |
| [3] | Clarke A J, Speer J G, Matlock D K, Rizzo F, Edmonds D V, Santofimia M J. Scr Mater, 2009; 61: 149 |
| [4] | Li Y, Lu Y P, Wang C, Li S T, Chen L B. J Iron Steel Res Int, 2011; 18(2): 70 |
| [5] | Jiang H T, Zhuang B T, Duan X G, Wu Y X, Cai Z X. Int J Miner Metall Mater, 2013; 20: 105 |
| [6] | Paravicini B E, Santofimia M, Zhao L, Sietsma J, Anelli E. Mater Sci Eng, 2013; A559: 486 |
| [7] | Wu R, Wang L, Jin X. Phys Procedia, 2013; 50: 8 |
| [8] | Zhong N. PhD Dissertation, Shanghai Jiao Tong University, 2009 (钟 宁. 上海交通大学博士学位论文, 2009) |
| [9] | Wang Y. PhD Dissertation, Shanghai Jiao Tong University, 2013 (王 颖. 上海交通大学博士学位论文, 2013) |
| [10] | Oi S W, Hill P, Rawson M, Bhadeshia H. Mater Sci Eng, 2013; A564: 485 |
| [11] | Wu Q, Shanthraj P, Zikry M A. Int J Fracture, 2013; 184: 241 |
| [12] | Paravicini B E, Santofimia M, Zhao L, Sietsma J, Anelli E. Mater Sci Eng, 2013; A559: 486 |
| [13] | Li D Z, Wei Y H, Liu C Y, Hou L F, Liu D F, Ya T X, Hu Y T. J Iron Steel Res, 2009; 21(2): 1 (李大赵, 卫英慧, 刘春月, 侯利锋, 刘东风, 崖天燮, 胡玉亭. 钢铁研究学报, 2009; 21(2): 1) |
| [14] | Zhang M. PhD Dissertation, Shanghai University, 2007 (张 梅. 上海大学博士学位论文, 2007) |
| [15] | Yu S F, Qian B N, Guo X M. Acta Metall Sin, 2005; 41: 402 (于少飞, 钱百年, 国旭明. 金属学报, 2005; 41: 402) |
| [16] | Lee S, Lee S J, De Cooman B C. Scr Mater, 2011; 65: 225 |
| [17] | Toji Y, Yamashita T, Nakajima K, Okuda K, Matsuda H, Hasegawa K, Seto K. ISIJ Int, 2011; 51: 818 |
| [18] | De Moor E, Matlock D K, Speer J G, Merwin M J. Scr Mater, 2011; 64: 185 |
| [19] | Garcia C I, De Ardo A J. Metall Trans, 1981; 12A: 521 |
| [20] | Speich G R, Demarest V A, Miller R L. Metall Trans, 1981; 12(8): 1419 |
| [21] | Lee S J, Lee S, De Cooman B C. Scr Mater, 2011; 64: 649 |
| [22] | Tian Y Q, Zhang H J, Chen L S, Song J Y, Xu Y, Zhang S H. Acta Metall Sin, 2014; 50: 531 (田亚强, 张宏军, 陈连生, 宋进英, 徐 勇, 张士宏. 金属学报, 2014, 50: 531) |
| [23] | Chen L S, Zhao Y, Tian Y Q, Song J Y, Wei Y L, Yang D. J Mater Eng, 2014; (6): 5 (陈连生, 赵 远, 田亚强, 宋进英, 魏英立, 杨 栋. 材料工程, 2014; (6): 5) |
| [24] | Chen L S, Zhang J Y, Tian Y Q, Song J Y, Wei Y L, Zhao Y. J Iron Steel Res, 2014; 26(5): 72 (陈连生, 张健杨, 田亚强, 宋进英, 魏英立, 赵 远. 钢铁研究学报, 2014; 26(5): 72) |
| [25] | Maruyama H. J Jpn Soc Heat Treat, 1977; 17: 198 |
| [26] | Nishiyama Z. Martensitic Transformations. New York: Academic Press, 1978: 60 |
| [27] | Li N, Liu G Q, Kang R M, Yang Y, Yu H. Trans Mater Heat Treat, 2013; 34(3): 118 (李 娜, 刘国权, 康人木, 杨 云, 余 慧. 材料热处理学报, 2013; 34(3): 118) |
| [28] | Yang H F, Wang L, Feng W J, Lu F G. Hot Work Technol, 2011; 40(18): 148 (杨海峰, 王 利, 冯伟骏, 芦凤桂. 热加工工艺, 2011; 40(18): 148) |
| [29] | Long C X. PhD Dissertation, Hunan University, Changsha, 2012 (龙彩霞. 湖南大学博士学位论文, 长沙, 2012) |
| [30] | Wang M J, Ma Q, Li J L, Zhang Y, Wang Y, Chen L. J Yanshan Univ, 2013; 37: 385 (王明家, 马 千, 李景丽, 张 勇, 王 艳, 陈 雷. 燕山大学学报, 2013; 37: 385) |
| [31] | Xu Z Y. Trans Mater Heat Treat, 2009; (6): 1 (徐祖耀. 金属热处理, 2009; (6): 1) |
| [32] | Mahieu J, Maki J, De Cooman B C, Claessens S. Metall Mater Trans, 2002; 33A: 2573 |
| [33] | H?mberg D. J Appl Math, 1995; 54(1): 31 |
/
| 〈 |
|
〉 |