STRENGTH AND TOUGHNESS OF T250 MARAGING STEEL JOINT HYBRID-TREATED WITH LASER WELDING AND AGING

  • Kun LI ,
  • Jiguo SHAN ,
  • Chunxu WANG ,
  • Zhiling TIAN
Expand
  • 1 Laser Processing Research Center, Department of Mechanical Engineering, Tsinghua University, Beijing 100084
    2 Key Laboratory for Advanced Materials Processing Technology, Ministry of Education, Tsinghua University, Beijing 100084
    3 Institute for Special Steel, Central Iron & Steel Research Institute, Beijing 100081

Accepted date: 2015-02-11

  Online published: 2015-05-22

Abstract

Maraging steels are leading members of the ultra-high strength steel family due to a combination of two solid state reactions: martensitic transformation and subsequent ageing. These steels can be hardened by the precipitation of refined Ni3(Ti, Mo) intermetallic particles. They have been widely used in the military and aerospace applications such as solid rocket motor cases and submarine shells due to their high strength and toughness. The T250 maraging steel has used Ti as one of the primary strengthening elements to replace Co, which decreases the cost of maraging steels. Its properties are comparable to the standard Co-bearing grades in the 1.4~2.1 GPa strength levels. It possesses good weldability without porosity in the weld and other weld defects. However, the combination of strength and toughness of welded joints is the main problem which has not been solved well via different welding methods so far. In this work, T250 maraging steel plate with 2 mm thickness was hybrid-treated with laser welding and aging treatment. The strength and toughness of welded joints aged before and after welding were investigated. The microstructures of parent metals and welded joints were observed with OM and SEM. Chemical compositions in parent metals and weld zones were analyzed with EPMA. The tensile strength and static toughness were acquired with the auxiliary device of Gleeble machine and could represent strength and toughness of the welded joints. The results show that the tensile strength and static toughness of the welded joint aged before welding are 62% and 28% that of the aged parent metal, respectively. However, the tensile strength and static toughness of the welded joint aged after welding reach 98% and 71% that of the aged parent metal, respectively. The weld metal is the key zone to influence the strength and toughness of the welded joints. Ni3(Ti, Mo) precipitates in the weld metal are the intrinsic reason resulting in that the strength and toughness of the welded joint aged after welding are superior to that of the welded joint aged before welding. Ni3(Ti, Mo) precipitates are beneficial to the strength and static toughness in the elastic deformation stage, and it has a dual effect on the static toughness in the plastic deformation stage of the welded joints. The reverted austenite has a negligible effect on the strength and static toughness in the elastic deformation stage, while it is detrimental to the static toughness in the plastic deformation stage of the welded joints.

Cite this article

Kun LI , Jiguo SHAN , Chunxu WANG , Zhiling TIAN . STRENGTH AND TOUGHNESS OF T250 MARAGING STEEL JOINT HYBRID-TREATED WITH LASER WELDING AND AGING[J]. Acta Metall Sin, 2015 , 51(8) : 904 -912 . DOI: 10.11900/0412.1961.2014.00635

References

[1] Decker R F, Floreens S. In: Wilson R K ed., Maraging Steels: Recent Developments and Applications, Huntington, West Virginia: The Minerals, Metals & Materials Society, 1988: 1
[2] Liang D M, Zhu Y Z, Liu G H. Heat Treat Met, 2010; 35(12): 34 (梁冬梅, 朱远志, 刘光辉. 金属热处理, 2010; 35(12): 34)
[3] Jiang Y, Yin Z D. Mater Sci Technol, 2004; 12(1): 108 (姜 越, 尹钟大. 材料科学与工艺, 2004; 12(1): 108)
[4] He Y, Yang K, Kong F Y, Qu W S, Su G Y. Acta Metall Sin, 2002; 38: 278 (何 毅, 杨 柯, 孔凡亚, 曲文生, 苏国跃. 金属学报, 2002; 38: 278)
[5] Vasudevan V K, Kim S J, Wayman C M. Metall Mater Trans, 1995; 21A: 2655
[6] Fan Z B, Han D, Duan S C. Aerosp Technol, 2010; 10(5): 41 (范赵斌, 韩 冬, 段述苍. 航空航天技术, 2010; 10(5): 41)
[7] Tsay L W, Huang W B, Chen C. J Mater Eng Perform, 1997; 6(2): 182
[8] Sundaresan S, Manirajan M, Nageswara R B. Mater Des, 2010; 31: 4921
[9] Subhananda R A, Venkata R G, Nageswara R B. Eng Failure Anal, 2005; 12: 325
[10] Floreen D S, Bayer A M. In: Wilson R K ed., Maraging Steels: Recent Developments and Applications, Huntington, West Virginia: The Minerals, Metals & Materials Society, 1988: 39
[11] Shamantha C R, Narayanan R, Iyer K J L, Radhakrishnan V M, Seshadri S K, Sundararajan S, Sundaresan S. Sci Technol Weld Joining, 2000; 5: 329
[12] Gupta R, Reddy R, Mukherjee M K. Weld World, 2012; 56(9): 69
[13] Mo D F, He G Q, Hu Z F, Shi Y L, Zhang W H. Trans China Weld Inst, 2008; 29(4): 29 (莫德锋, 何国求, 胡正飞, 施延龄, 张卫华. 焊接学报, 2008; 29(4): 29)
[14] Lee Y J, Lee I K, Wu S C, Kung M C, Chou C P. Sci Technol Weld Joining, 2007; 12: 266
[15] Reddy G M, Rao V V, Raju A V S. J Mater, 2013; 223(4): 149
[16] Tsay L W, Chen C, Chan S L I. Int J Mater Prod Technol, 1995; 10(1-2): 132
[17] Fanton B L, Abdalla A J, Fernandes M S. Weld J, 2014; 93: 362
[18] Zhao Z Y. The Design of Alloy Steels. Beijing: National Defense Industry Press, 1999: 64 (赵振业. 合金钢设计. 北京: 国防工业出版社, 1999: 64)
[19] Zhang L Y, Yang G, Huang C X, Chen W L, Wang L M. Acta Metall Sin, 2008; 44: 409 (张凌义, 杨 钢, 黄崇湘, 陈为亮, 王立明. 金属学报, 2008; 44: 409)
[20] Zhang Z M, Zhang X, Wang Q, Li B C. J Mech Eng, 2012; 48(18): 67 (张治民, 张 星, 王 强, 李保成. 机械工程学报, 2012; 48(18): 67)
[21] Lu L, Li Z B, Bi Z Y, Xue L H, Ma X. J Iron Steel Res, 2014; 26(6): 67 (芦 琳, 李周波, 毕宗岳, 薛磊红, 马 璇. 钢铁研究学报, 2014; 26(6): 67)
[22] Yin Z D, Li X D, Li H B, Lai Z H. Acta Metall Sin, 1995; 43: 7 (尹钟大, 李晓东, 李海滨, 来忠红. 金属学报, 1995; 43: 7)
[23] Tsay L W, Lee W C, Luu W C, Wu J K. Corros Sci, 2002; 44: 1311
[24] Ye H Q, Zou B S. Acta Metall Sin, 1979; 15: 69 (叶恒强, 邹本三. 金属学报, 1979; 15: 69)
[25] Kenyon N. Weld J, 1968; 47(5): 193
[26] Narayanan P R, Sreekumar K, Natarajan A, Sinha P P. J Mater Sci, 1990; 25: 4587
Outlines

/

〈 〉