EFFECT OF LONG-TERM AGING AT 760 ℃ ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF A Ni-Cr-W-Fe ALLOY

  • Xianchao HAO ,
  • Long ZHANG ,
  • Chao XIONG ,
  • Yingche MA ,
  • Kui LIU
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Accepted date: 2015-03-05

  Online published: 2015-05-18

Abstract

Significant efforts on development of advanced ultra-supercritical (A-USC) fossil fired power plants with steam conditions of 700 ℃ and 30 MPa or higher have been made in recent years. The most important consideration is the development of materials for superheater and reheater tubes with working temperature as high as 760 ℃. During the design and application of these materials, phase stability, creep rupture strength and corrosion performance at 700~760 ℃ should be evaluated. A new type Ni-Cr-W-Fe alloy has been designed for A-USC power plants and the microstructure and mechanical properties of Ni-Cr-W-Fe alloy after long-term aging at 760 ℃ was investigated using OM, SEM, TEM and tensile testing in this work. The fractographs of tensile samples were observed. The results show that the average gain size of specimen after solution-annealing at 1100 ℃ is about 80 μm with twin planes present in the matrix. The major precipitates after aging at 760 ℃ for 16 h are M23C6 and g'. The average particle size and the volume fraction of g' phase are approximately 29 nm and 19%, respectively. The coarsening behavior of g' during long-term aging at 760 ℃ follows Ostwald ripening theory. The solution-annealed Ni-Cr-W-Fe alloy performs excellent ductility at room temperature and the fracture mode of is ductile. The room temperature tensile strengths increase obviously with the decreasing of elongation and reduction of area after aging treatment. The yield strengths at both room and elevated temperatures decrease gradually with the extending aging time at 760 ℃. The tensile ductility at room temperature of Ni-Cr-W-Fe alloy decreases after aging from 1000 to 3000 h, while the elevated temperature ductility varies mildly and keeps at approximately 15%.

Cite this article

Xianchao HAO , Long ZHANG , Chao XIONG , Yingche MA , Kui LIU . EFFECT OF LONG-TERM AGING AT 760 ℃ ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF A Ni-Cr-W-Fe ALLOY[J]. Acta Metall Sin, 2015 , 51(7) : 807 -814 . DOI: 10.11900/0412.1961.2014.00592

References

[1] Lin F S, Xie X S, Zhao S Q, Dong J X. J Chin Soc Power Eng, 2011; 31: 960 (林富生, 谢锡善, 赵双群, 董建新. 动力工程学报, 2011; 31: 960)
[2] Viswanathan R, Purgert R, Goodstine R S, Tanzosh J, Stanko G, Shingledecker J P, Vitalis B. In: Viswanathan R, Gandy D, Coleman K eds., Proc 5th Int Conf on Advances in Materials Technology for Fossil Power Plants, Marco Island, Florida: EPRI, 2007: 1
[3] Nakamura S, Kawashima H, Takei Y, Saito N, Tanaka Y, Nishimoto S. Mitsubishi Heavy Ind Tech Rev, 2011; 48(3): 8
[4] Viswanathan V, Purgert R, Rawls P. Adv Mater Proc, 2008; 8: 47
[5] Knezevic V, Schneider A, Landier C. Procedia Eng, 2013; 55: 240
[6] Van Stone R W. In: Strang A ed., Proc of Parsons 2000 Advanced Materials for 21st Century Turbines and Power Plant, London: IOM Communications Ltd., 2000: 91
[7] Guo J T, Du X K. Acta Metall Sin, 2005; 41: 1221 (郭建亭, 杜秀魁. 金属学报, 2005; 41: 1221)
[8] Allen D, Keustermans J P, Grijbels S, Bicego V. Mater High Temp, 2004; 21: 53
[9] Patel S J, de Barbadillo J J, Baker B A, Gollihue R D. Procedia Eng, 2013; 55: 246
[10] Lin F, Chen S, Xie X. In: Viswanathan R, Gandy D, Coleman K eds., Proc 5th Int Conf on Advances in Materials Technology for Fossil Power Plants, Marco Island, Florida: EPRI, 2007: 46
[11] Tokairin T, Dahl K V, Danielsen H K, Grumsen H B, Sato T, Hald J. Mater Sci Eng, 2013; A565: 285
[12] Wang T T, Wang C S, Guo J T, Zhou L Z. Mater Sci Forum, 2013; 747-748: 647
[13] Viswanathan R, Sarver J, Tanzosh J M. J Mater Eng Perform, 2006; 15: 256
[14] Wu Q, Hyojin S, Swinderman R W, Shingledecker J P, Vasudevan V K. Metall Mater Trans, 2008; 39A: 2569
[15] Zhao S Q, Xie X S, Smith G D, Patel S J. Mater Sci Eng, 2003; A355: 96
[16] Sims C T, Hagel W C. The Superalloys. New York: John Wiley & Sons, 1972: 55
[17] MacKay R A, Nathal M V. Acta Metall Mater, 1990; 38: 993
[18] Kim H T, Chun S S, Yao X X. J Mater Sci, 1997; 32: 4917
[19] Ardell A J. Acta Metall, 1968; 16: 511
[20] Lifscitz I M, Slyozov V V. J Phys Chem Solids, 1961; 19: 35
[21] Footer P K, Richards B P. J Mater Sci, 1982; 17: 2141
[22] Wagner C. Z Elektrochem, 1961; 65: 581
[23] Li X, Saunders N, Miodownik A P. Metall Mater Trans, 2002; 33A: 3367
[24] Patil R V, Kale G B. J Nucl Mater, 1996: 230: 57
[25] Baldan A. J Mater Sci, 2002; 37: 2379
[26] Kong Y H, Chen Q Z. Mater Sci Eng, 2004; A366: 135
[27] Huang Q Y,Li H K. Superalloy. Beijing: Metallurgical Industry Press, 2000: 29 (黄乾尧,李汉康. 高温合金. 北京: 冶金工业出版社, 2000: 29)
Outlines

/