FINITE ELEMENT SIMULATION OF HOT ROLLING PROCESS FOR SiCp/Al COMPOSITES
Accepted date: 2015-05-11
Online published: 2015-05-15
Supported by
Supported by National Basic Research Program of China (No.2012CB619600)
In this work, the hot rolling process of SiCp/2009Al composites is simulated using the fully coupled thermal-stress analysis in Abaqus/Explicit. By the investigation of formation process for rolling along with different fields of temperature, strain rate, strain and stress and their evolutionary history, the hot rolling mechanisms under complicated stress states is achieved. The results show that the maximum principal stress changes from compressive stress to tensile stress at the stage of rolling entrance and a reverse trend replaces it at the exit, and that the compressive stress is dominant in the deformation zone at the steady rolling stage. The temperature drop effect due to heat transfer is far greater than the temperature rise effect due to friction on the plate surface while the temperature rise is embodied in the center due to plastic deformation. Besides, the effect of strain rate on flow stress plays a leading role at the entrance and exit stage, and the flow stress on the plate surface in the deformation region is mainly determined by strain and temperature except the stick zone which is controlled by strain rate, however, the center flow stress in deformation is mainly affected by temperature.
Key words: rolling; rheological behavior; composites; finite element
Li ZHOU , Changzhou WANG , Xingxing ZHANG , Bolü XIAO , Zongyi MA . FINITE ELEMENT SIMULATION OF HOT ROLLING PROCESS FOR SiCp/Al COMPOSITES[J]. Acta Metall Sin, 2015 , 51(7) : 889 -896 . DOI: 10.11900/0412.1961.2015.00210
| [1] | Selvam J D R, Smart D S R, Dinaharan I. Mater Des, 2013; 49: 28 |
| [2] | Mortensen A, Llorca J. Annu Rev Mater Res, 2010; 40: 243 |
| [3] | Wang S S, Mao C H, Yang J, Liang Q S, Sun B. Chin J Rare Met, 2012; 36: 167 (汪山山, 毛昌辉, 杨 剑, 梁秋实, 孙 波. 稀有金属, 2012; 36: 167) |
| [4] | Hassani A, Bagherpour E, Qods F. J Alloys Compd, 2014; 591: 132 |
| [5] | Balasubramanian I, Maheswaran R. Mater Des, 2015; 65: 511 |
| [6] | Liu J W, Zheng Z X, Wang J M, Wu Y C, Tang W M, Lu J. J Alloys Compd, 2008; 465: 239 |
| [7] | El-Sabbagh A, Solimam M, Taha M, Palkowski H. J Mater Process Technol, 2012; 212: 497 |
| [8] | Goswami R K, Sikand R, Dhar A, Grover O P, Jindal U C, Gupta A K. Mater Sci Technol, 1999; 15: 443 |
| [9] | El-Sabbagh A,?Soliman M,?Taha?M,?Palkowski H. J Mater Process Technol, 2013; 213: 1669 |
| [10] | Euh K, Kang S B. Mater Sci Eng, 2005; A395: 47 |
| [11] | Liu X H. Acta Metall Sin, 2010; 46: 1025 (刘相华. 金属学报, 2010; 46: 1025) |
| [12] | Shahani A R, Setayeshi S, Nodamaie S A, Asadi M A, Rezaie S. J Mater Process Technol, 2009; 209: 1920 |
| [13] | Duan X J, Sheppard T. J Mater Process Technol, 2004; 150: 100 |
| [14] | Yu H L, Jiao Z J, Liu X H, Zhao X M. J Mater Metall, 2005; 4(1): 70 (喻海良, 矫志杰, 刘相华, 赵宪明. 材料与冶金学报, 2005; 4(1): 70) |
| [15] | Arif A F M, Khan O, Sheikh A K. J Mater Process Technol, 2004; 147: 255 |
| [16] | Kan Y, Liu Z G, Zhang S H, Zhang L W, Cheng M, Song H W. Chin J Rare Met, 2015; 39(4): 289 (阚 盈, 刘振刚, 张士宏, 张立文, 程 明, 宋鸿武. 稀有金属, 2015; 39(4): 289) |
| [17] | Shao J C, Xiao B L, Wang Q Z, Ma Z Y, Liu Y, Yang K. Mater Sci Eng, 2010; A527: 7865 |
| [18] | Xu H, Zhang X, Li H W, Li S, Wang C S, Wang Y L, Zhang B D. J Wuhan Univ Technol—Mater Sci Ed, 2012; 27: 443 |
| [19] | Serajzadeh S, Karimi T A, Nejati M, Izadi J, Fattahi M. J Mater Process Technol, 2002; 128: 88 |
| [20] | Yaakoubi M, Kchaou M, Dammak F. Comp Mater Sci, 2013; 68: 297 |
| [21] | Chen J, Chandrashekhara K, Mahimkar C, Lekakh S N, Richards V L. J Mater Process Technol, 2011; 211: 245 |
| [22] | Zhu Y, Kishawy H A. Int J Mach Tools Manuf, 2005; 45: 389 |
| [23] | Tan Y Q, Yang D M, Sheng Y. J Eur Ceram Soc, 2009; 29: 1029 |
| [24] | Ducobu F, Rivière-Lorphèvre E, Filippi E. Simul Modell Pract Theory, 2015; 53: 1 |
| [25] | Cocchetti G, Pagani M, Perego U. Comp Struct, 2013; 127: 39 |
/
| 〈 |
|
〉 |