MODEL OF THE EFFECT OF GRAIN SIZE ON PLASTI-CITY IN ULTRA-FINE GRAIN SIZE STEELS

  • Jin LIU ,
  • Guohui ZHU
Expand
  • 1 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
    2 School of Metallurgical Engineering, Anhui University of Technology, Maanshan 243000

Online published: 2015-05-11

Supported by

Supported by National Natural Science Foundation of China (No.51071026) and Scientific Research Foundation for the Returned Overseas Chinese Scholars, Ministry of Education

Abstract

Based on our earlier preliminary work, a model was developed for prediction of the critical grain size where the plasticity would be decreased as the grain refined. In the model the effect of grain size on the fracture strength was combined. The prediction of the model exhibited that in the range of grain size of 10 mm to 0.2 mm as an example, the total elongation of the steels would be firstly increased. But when the grain size was refined to 2.5 mm and below, the total elongation of the steels was not increased but decreased sharply, which was good agreement with the experimental results published recently. Present work illustrated that the dominant mechanism of the elongation decreased in the ultra-fine grain size materials is due to increase in resistance force of grain boundaries on the dislocation sources resulting in the difficulty of activation of dislocation movements. Its expression would be the decrease of the plastic strain in macro-level.

Cite this article

Jin LIU , Guohui ZHU . MODEL OF THE EFFECT OF GRAIN SIZE ON PLASTI-CITY IN ULTRA-FINE GRAIN SIZE STEELS[J]. Acta Metall Sin, 2015 , 51(7) : 777 -783 . DOI: 10.11900/0412.1961.2014.00678

References

[1] Kim Y M, Kim S K, Lim Y J, Kim N J. ISIJ Int, 2002; 42: 1571
[2] Zhao M C, Shan Y Y, Xiao F R, Yang K, Li Y H. Mater Lett, 2002; 57: 141
[3] Okatsu M, Shikanai N, Kondo J. JFE Tech Rep, 2008; 12: 8
[4] Ishikawa N, Shikanai N, Kondo J. JFE Tech Rep, 2008; 12: 15
[5] Park K T, KimY S, Lee J G, Shin D H. Mater Sci Eng, 2000; A293: 165
[6] Tsuji N, Ito Y, Saito Y, Minamino Y. Scr Mater, 2002; 47: 893
[7] Kumar B R, Sharma S, Kashyap B P, Prabhu N. Mater Des, 2015; 68: 63
[8] Song R, Ponge D, Raabe D. Scr Mater, 2005; 52: 1075
[9] Lee T, Koyama M, Tsuzaki K, Lee Y H, Lee C S. Mater Lett, 2012; 75: 169
[10] Lee T, Park C H, Lee D, Lee C S. Mater Sci Eng, 2011; A528: 6558
[11] Hu T, Ma K, Topping T D, Saller B, Yousefiani A, Schoenung J M, Lavernia E J. Scr Mater, 2014; 78-79: 25
[12] Song R, Ponge D, Raabe D, Speer J G, Matlock D K. Mater Sci Eng, 2006; A441: 1
[13] Xue P, Xiao B L, Ma Z Y. Mater Sci Eng, 2012; A532: 106
[14] Zhuang Z, Cui Y N, Gao Y, Liu Z L. Adv Mech, 2011; 41: 647 (庄 茁, 崔一南, 高 原, 柳占立. 力学进展, 2011; 41: 647)
[15] Rao S I, Dimiduk D M, Parthasarathy T A, Uchic M D, Tang M, Woodward C. Acta Mater, 2008; 56: 3245
[16] Liu J, Zhu G H, Mao W M, Subramanian S V. Mater Sci Eng, 2014; A607: 302
[17] Stroh A N. Adv Phys, 1957; 6: 418
[18] Smith E. Acta Metall, 1966; 14: 985
[19] McMahon C J, Cohen M. Acta Metall, 1965; 13: 591
[20] Knott J F. Fundamentals of Fracture Mechanics. New York: John Wiley-Halsted Press, 1973: 98
[21] Lin T, Evans A G, Ritchie R O. Metall Trans, 1987; 18A: 641
[22] Curry D A, King J E. Met Sci, 1978; 12: 247
[23] Yu Y N,Yang P,Qiang W J,Chen L. Fundament of Materials Science. Beijing: Higher Education Press, 2006: 537 (余永宁,杨 平,强文江,陈 冷. 材料科学基础. 北京: 高等教育出版社, 2006: 537)
[24] Wu S J, Davis C L. Mater Sci Eng, 2004; A387-389: 456
[25] Sato S, Wagatsuma K, Suzuki S, Kumagai M, Imafuku M, Tashiro H, Kajiwara K, Shobu T. Mater Charact, 2013; 83: 152
[26] Veistinen M K, Lindroos V K. Scr Metall, 1984; 18: 185
[27] Deng W, Gao X M, Qin X M, Zhao D W, Du L X, Wang G D. Acta Metall Sin, 2010; 46: 533 (邓 伟, 高秀梅, 秦小梅, 赵德文, 杜林秀, 王国栋. 金属学报, 2010; 46: 533)
[28] Yang P. Electron Back Scattering Diffraction Technique and its Application. Beijing: Metallurgical Industry Press, 2007: 157 (杨 平. 电子背散射衍射技术及其应用. 北京: 冶金工业出版社, 2007: 157)
[29] Zhu G, Mao W, Yu Y. Scr Mater, 2000; 42: 37
[30] Mao W M, Chen L, Yu Y N. Chin Sci Bull, 2002; 47: 1540 (毛卫民, 陈 冷, 余永宁. 科学通报, 2002; 47: 1540)
[31] Chin G Y. Metall Trans, 1972; 3: 2213
[32] Franciosi P. Acta Metall, 1983; 31: 1331
[33] Eshelby J D, Frank F C, Nabarro F R N. Philos Mag, 1951; 742: 351
[34] Gao H L. Pipeline Steel and Pipeline Pipe. Beijing: China Petrochemical Press, 2012: 8 (高惠临. 管线钢与管线钢管. 北京: 中国石化出版社, 2012: 8)
[35] Ohashi T, Kawamukai M, Zbib H. Int J Plast, 2007; 23: 897
[36] Cheng C, Jie M, Chan L, Chow C L. Int J Mech Sci, 2009; 49: 217
[37] Zhao M, Yin F, Hanamura T, Nagai K, Atrens A. Scr Mater, 2007; 57: 857
[38] Hanamura T, Yin F, Nagai K. ISIJ Int, 2004; 44: 610
[39] Park K T, Han S Y, ShinD H, LeeY K, Lee K J, Lee K S. ISIJ Int, 2004; 44: 1057
[40] Song R, Pong D, Raabe D. Acta Mater, 2005; 53: 4881
[41] Dini G, Najafizadeh A, Ueji R, Monir-Vaghefi S M. Mater Lett, 2010; 64: 15
[42] Ueji R, Tsuchida N, Terada D, Tsuji N, Tanaka Y, Takemura A, Kunishige K. Scr Mater, 2008; 59: 963
Outlines

/

〈 〉