INFLUENCES OF LONG-TERM AGING ON MICRO- STRUCTURE EVOLUTION AND LOW CYCLE FATIGUE BEHAVIOR OF GH4169 ALLOY

  • Jinlan AN ,
  • Lei WANG ,
  • Yang LIU ,
  • Guohua XU ,
  • Guangpu ZHAO
Expand
  • 1 Key Lab for Anisotropy and Texture of Materials, Ministry of Education, Northeastern University, Shenyang 110819
    2 High Temperature Material Research Institute, Central Iron and Steel Research Institute, Beijing 100081

Accepted date: 2015-01-20

  Online published: 2015-05-06

Supported by

Supported by High Technology Research and Development Program of China (No.2012AA03-A513) and Ministry of Education Technical Foundation (No.625010337)

Abstract

GH4169 superalloy is one kind of important metallic materials used for manufacturing turbine discs in aero-engine. In order to meet the demand of higher strength, high ratio alloying elements have to be added, resulting in the complex microstructure evolution during the long-term service at elevated temperature. Furthermore, the turbine disc usually bears overloading which will lead to the low cycle fatigue (LCF) damage in real working and result in fatal security problem. Besides, it is meaningful to decide the relationship between the microstructure evolution and performance degradation. In the present work, microstructure evolution and LCF behavior of GH4169 alloy during long-term aging were investigated. The microstructure evolutions of GH4169 alloy during long-term aging at 750 ℃ for 500, 1000, 1500 and 2000 h and the influences of long-term aging on the LCF behavior were investigated. The results show that the size of g″ phases increases and the volume fraction decreases with the increase of aging time, compared with the increase of both size and volume fraction of d phases. Both the fatigue strength and fatigue life of the alloy decrease with the increase of aging time. For the specimen aged for the same time, the cyclic stress firstly contributes to cyclic hardening, then cyclic stability, and finally cyclic softening with the increase of cyclic numbers. It is found that the decrease of cyclic stress contribution is slightly effected by the size of g″ phases increase and volume fraction decrease after long-term aging. Therefore, the LCF life of the alloy decreases since the crack easily propagates along with the long needle-like d phases and the g″ phases precipitate free zones.

Cite this article

Jinlan AN , Lei WANG , Yang LIU , Guohua XU , Guangpu ZHAO . INFLUENCES OF LONG-TERM AGING ON MICRO- STRUCTURE EVOLUTION AND LOW CYCLE FATIGUE BEHAVIOR OF GH4169 ALLOY[J]. Acta Metall Sin, 2015 , 51(7) : 835 -843 . DOI: 10.11900/0412.1961.2014.00626

References

[1] Huang Q Y,Li H K. Superalloy. Beijing: Metallurgy Industry Press, 2000: 1 (黄乾尧,李汉康. 高温合金. 北京: 冶金工业出版社, 2000: 1)
[2] Leo P D G, Walsh M J, Maclachlan D, Korsunsky A M. Int Fatigue, 2009; 31: 1966
[3] Wang Y, Lin L, Shao W Z, Zhen L, Zhang X M. Trans Mater Heat Treat, 2007; 28(suppl): 176
[4] Medeiros S C, Prasad Y V R K, Frazier W G, Srinivasan R. Mater Sci Eng, 2003; A193: 198
[5] Tian S G, Wang X, Xie J, Liu C, Guo Z G, Liu J, Sun W R. Acta Metall Sin, 2013; 49: 845 (田素贵, 王 欣, 谢 君, 刘 臣, 郭忠革, 刘 姣, 孙文儒. 金属学报, 2013; 49: 845)
[6] Zhang H Y, Zhang S H, Zhang W H, Cheng M, Wang Z T. J Plast Eng, 2007; 14(4): 69 (张海燕, 张士宏, 张伟红, 程 明, 王忠堂. 塑性工程学报, 2007; 14(4): 69)
[7] Yang Y R, Liang X F, Cai B C, Huang F X. J Aeronaut Mater, 1996; 16(2): 38 (杨玉荣, 梁学锋, 蔡伯成, 黄福祥. 航空材料学报, 1996; 16(2): 38)
[8] Jiang H P. Gas Turbine Experiment Res, 2002; 15(4): 1 (江和甫. 燃气涡轮试验与研究, 2002;15(4): 1)
[9] Liu F, Sun W R,Yang S L, Li Z, Guo S R, Yang H C, Hu Z Q. Acta Metall Sin, 2008; 44: 791 (刘 芳, 孙文儒, 杨树林, 李 站, 郭守仁, 杨洪才, 胡壮麒. 金属学报, 2008; 44: 791)
[10] Dong J X, Bai Y Q, Xu Z C, Xie X S, Zhang S H. J Univ Sci Technol Beijing, 1993; 15: 567 (董建新, 白元强, 徐志超, 谢锡善, 章守华. 北京科技大学学报, 1993; 15: 567)
[11] Azadian S, Wei L Y, Warren R. Mater Charact, 2004; 53: 7
[12] Tang J X, Lu S. J Aerospace Power, 2006; 21: 706 (唐俊星, 陆 山. 航空动力学报, 2006; 21: 706)
[13] Miller H E, Chamber W L. In: Sims C T, Ctoloff N S, Hagel W C eds., Superalloy II, New York: John-Wiley & Sons, 1987: 18
[14] Coffin L F. In: Carden A E, McEvily A J, Wells C H eds., Fatigue at Elevated Temperatures, Baltimore: ASTM, 1973: 112
[15] Gell M, Leverant G R. In: Carden A E, McEvily A J, Wells C H eds., Fatigue at Elevated Temperatures, Baltimore: ASTM, 1973: 37
[16] Coffin L F Jr. Soc Mater Sci, Japan, 1971; 21: 30
[17] Merrick H K. Metall Trans, 1974; 5A: 891
[18] Fournier D, Pineau A. Metall Trans, 1977; 8A: 109
[19] Day M F, Thyomas G B. Met Sci, 1979; 13: 25
[20] Antolovich S D, Liu S, Baur R. Metall Trans, 1981; 12A: 473
[21] Yao J, Guo J T, Yuan C, Li Z J. Acta Metall Sin, 2005; 41: 357 (姚 俊, 郭建亭, 袁 超, 李志军. 金属学报, 2005; 41: 357)
[22] Xie X S, Dong J X, Fu S H, Zhang M C. Acta Metall Sin, 2010; 46: 1289 (谢锡善, 董建新, 付书红, 张麦仓. 金属学报, 2010; 46: 1289 )
[23] Wang K, Li M Q, Luo J, Li C. Mater Sci Eng, 2011; A528: 4723
[24] Xiao L, Chen D L. Scr Mater, 2004; 52: 603
[25] Deng Q, Zhuang J Y, Du J H. J Iron Steel Res, 1998; 10(2): 33 (邓 群, 庄景云, 杜金辉. 钢铁研究学报, 1998; 10(2): 33)
[26] Miller M K, Babu S S, Burke M G. Mater Sci Eng, 1999; A270: 14
[27] Miller M K. Micron, 2001; 32: 757
[28] Du J H, Lv X D, Den Q. Rare Met Mater Eng, 2014; 43: 1830
[29] Li S Q, Zhuang J Y, Yang J Y, Deng Q, Du J H, Xie X S, Li B, Xu Z C, Cao Z, SuZ Q, Jiang C Z. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Pittsburgh, PA: TMS, 1994: 545
[30] Collier J P, Wong S H. Metall Trans, 1988; 19A: 1657
[31] Dong J X, Xie X S, Xu Z C, Zhang S H, Chen M Z, Radavich J F. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Pittsburgh, PA: TMS, 1994: 649
[32] Wang L, Liu Y, Jin J C, Feng F, Lv X D, Zhang B J. J Iron Steel Res, 2011; 23(suppl 2): 213 (王 磊, 刘 杨, 晋俊超, 冯 飞, 吕旭东, 张北江. 钢铁研究学报, 2011; 23(增刊2): 213)
[33] Wang Y W, Yang L Y, You W, Bai B Z. Mater Sci Forum, 2005; 475-479: 3003
[34] Liu Y, Wang L, He S S, Feng F, Lv X D, Zhang B J. Acta Metall Sin, 2012; 48: 49 (刘 杨, 王 磊, 何思斯, 冯 飞, 吕旭东, 张北江. 金属学报, 2012; 48: 49)
[35] Wang L. Mechanical Properties of Materials. Shenyang: Northeastern University Press, 2014: 94 (王 磊. 材料的力学性能. 沈阳: 东北大学出版社, 2014: 94)
[36] An J L. Master Thesis, Northeastern University, Shenyang, 2014 (安金岚. 东北大学硕士学位论文, 沈阳, 2014)
Outlines

/