EFFECT OF NOTCH ORIENTATION AND LOCAL RECRYSTALLIZATION ON THERMAL FATIGUE PROPERTIES OF A DIREC- TIONALLY SOLIDIFIED Co-BASED SUPERALLOY

  • Sheng PU ,
  • Li WANG ,
  • Guang XIE ,
  • Xianfei DING ,
  • Langhong LOU ,
  • Qiang FENG
Expand
  • 1 State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083
    2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
    3 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
    4 National Center for Materials Service Safety, University of Science and Technology Beijing, Beijing 100083

Revised date: 2014-08-01

  Online published: 2015-05-01

Supported by

Supported by National Basic Research Program of China (No.2010CB631201), High Technology Research and Development Program of China (No.2012AA03A513), National Natural Science Foundation of China (No.50901079) and Supporting Technology Program of Chinese Ministry of Education (No.625010337)

Abstract

The directionally solidificated (DS) Co-based superalloys are widely used in aircraft turbine vanes due to the good stress-rupture parameters and excellent hot corrosion resistance. The cyclic change of temperatures and complex stress state thermal fatigue (TF) cracks happen frequently in vanes during service. However, most of the work are conducted in Ni-based superalloys and there is rare report concerning the TF behavior of DS Co-based superalloys. Furthermore, due to the residual strain accumulated during processing, shot peening, grinding and recrystallization (RX) frequently occur when the DS components are exposed to high temperatures. It is believed that RX may change the microstructure, especially adding more grain boundaries to DS alloys, and result in the reduction of the mechanical properties of DS superalloys. Therefore, in this work, V-notch plate specimens with notch direction perpendicular and parallel to the DS orientation are machined from the DS plate. Local RX grains are prepared (local indented and then heat treated) in the notch areas of some samples. TF test is conducted between 1000 ℃ to room temperature. The effect of DS orientation and RX on TF properties of a DS Co-based superalloy is investigated. The results indicate that the cracks propagate along the interdendritic regions in the samples with notches parallel to the DS direction, which exhibites lower TF properties than samples with notches vertical to the DS direction. TF cracks initiate and propagate along RX boundaries in samples containing RX grains. Precipitation of M23C6 carbides is found along the RX boundaries during TF tests. Due to the oxidation at the tip of crack, M23C6 desquamates and leads to the formation of micro voids, which accelerates the crack propagation and decreases TF properties of tested alloy. In samples with notches parallel to the DS direction, cracks preferentially propagate along the RX grain boundaries.

Cite this article

Sheng PU , Li WANG , Guang XIE , Xianfei DING , Langhong LOU , Qiang FENG . EFFECT OF NOTCH ORIENTATION AND LOCAL RECRYSTALLIZATION ON THERMAL FATIGUE PROPERTIES OF A DIREC- TIONALLY SOLIDIFIED Co-BASED SUPERALLOY[J]. Acta Metall Sin, 2015 , 51(4) : 449 -457 . DOI: 10.11900/0412.1961.2014.00425

References

[1] Badger F S. J Met, 1958; 10: 512
[2] Ratna V, Sarma D S. Scr Metall, 1993; 29: 467
[3] Glover N E, Davis C L. Scr Metall, 1996; 34: 675
[4] Li Y L, Yuan C, Guo J T. Acta Metall Sin, 2006; 42: 1056
[4] (李友林, 袁 超, 郭建亭. 金属学报, 2006; 42: 1056)
[5] Beck C G, Santhanam A T. Scr Metall, 1978; 12: 255
[6] Bhattachar V S. Int J Fatigue, 1995; 17: 407
[7] Woodford D A, Mowbray D F. Mater Sci Eng, 1974; A16: 5
[8] Xia P C, Yu J J, Sun X F, Guan H R, Hu Z Q. Rare Met Mater Eng, 2008; 37: 50
[8] (夏鹏成, 于金江, 孙晓峰, 管恒荣, 胡壮麒. 稀有金属材料与工程, 2008; 37: 50)
[9] Reuchet J, Remy L. Mater Sci Eng, 1983; A58:19
[10] Miao J S, Pollock T M, Jones J W. Acta Mater, 2009; 57: 5964
[11] Pedron J P, Pineau A. Mater Sci Eng, 1982; 56: 143
[12] Xiao X, Xu H, Qing X Z, Guo Y A, Guo J T, Zhou L Z. Acta Metall Sin, 2011; 47: 129
[12] (肖 旋, 许 辉, 秦学智, 郭永安, 郭建亭, 周兰章. 金属学报, 2011; 47: 129)
[13] Xia P C, Yu J J, Sun X F, Guan H R, Hu Z Q. Rare Met Mater Eng, 2011; 40: 152
[13] (夏鹏成, 于金江, 孙晓峰, 管恒荣, 胡壮麒. 稀有金属材料与工程, 2011; 40: 152)
[14] Panwisawas C, Mathur H, Gebelin J, Putman D, Rae C M F, Reed R C. Acta Mater, 2013; 61: 51
[15] Wang L, Pyczak F, Zhang J, Lou L H, Singer R F. Mater Sci Eng, 2012; A532: 487
[16] Xie G, Wang L, Zhang J, Lou L H. Metall Mater Trans, 2008; 39A: 206
[17] Khan T, Caron P, Nakagawa Y G. J Met, 1986; 38: 16
[18] Pu S, Zhang J, Shen Y F, Lou L H. Mater Sci Eng, 2008; A480: 428
[19] Guo X F, Wang H Q. Aeronaut Mater, 1984; (6): 1
[19] (郭秀芬, 王海清. 航空材料, 1984; (6): 1)
[20] Robert A K, Richard W N. Int J Fatigue, 2010; 32: 1330
[21] Xia P C, Yang L, Yu J J, Sun X F, Guan H R, Hu Z Q. Rare Met, 2011; 30(special issue): 472
[22] Liu P S, Chen G F, Liang K M. J Chin Soc Corros Prot, 1999; 19: 339
[22] (刘培生, 陈国锋, 梁开明. 中国腐蚀与防护学报, 1999; 19: 339)
[23] Reuchet J, Remy L. Mater Sci Eng, 1983; A58: 19
[24] Kang B, Liu X B, Cisloiu C, Chang K M. Mater Sci Eng, 2003; A347: 205
[25] Brandes E A,Brook G B. Smithells Metals Reference Book. 7th Ed., London: Butterworths Press, 1992: 11
[26] Chen K Y, Zhao L R. J Phys Chem Sol, 2007; 68: 1805
[27] Zheng Y R, Ruan Z C, Wang S C. Acta Metall Sin, 1995; 31(suppl): 325
[27] (郑运荣, 阮忠慈, 王顺才. 金属学报, 1995; 31(增刊): 325)
[28] Lu Z, Lu L, Xu Y B, Hu Z Q. Fatigue Fract Eng Mater Struct, 1998; 21: 1589
[29] Jiang W H, Yao X D, Guan H R. Mater Sci Eng, 1999; A271: 101
[30] He L Z, Zheng Q, Sun X F. Mater Sci Eng, 2005; A397: 297
[31] Mishin Y, Herzig C. Mater Sci Eng, 1999; A260: 55
[32] Parthasarathy T A, Shewmon P G. Scr Metall, 1983; 17: 943
Outlines

/

〈 〉