THE CORROSION BEHAVIOUR OF NiCu LOW ALLOY STEEL IN A DEAERATED BICARBONATE SOLUTION CONTAINING Cl- IONS

  • Yunfei LU ,
  • Jingfeng YANG ,
  • Junhua DONG ,
  • Wei KE
Expand
  • Environmental Corrosion Research Center of Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Revised date: 2014-07-01

  Online published: 2015-05-01

Supported by

Supported by National Natural Science Foundation of China (No.51471175)

Abstract

The corrosion behaviour of low alloy steel containing Ni and Cu was studied because it is a promising candidate canister material for the disposal of high-level radioactive waste (HLW) in China. Due to the intensely radioactive nature of HLW, the waste has to be prevented from reaching the biosphere for many tens of thousands of years. Deep geological disposal is now considered to be the most preferable option for isolating HLW and it relies on series of natural and engineered barriers, e.g. a metallic canister. However, as soon as the waste package is settled, groundwater would seep back slowly through the outer barriers and ultimately arrive at the surface of the canister. Accordingly, there comes the groundwater-induced dissolution of the canister and subsequent transport of radionuclides through the barriers. That is to say, the effectiveness of radionuclide retention and isolation depends mostly and finally on the corrosion resistance of metallic canisters in deep groundwater environments. In this work, the test solution is deaerated 0.1 mol/L NaHCO3+0.1 mol/L NaCl, simulating the deep groundwater environment. The evolution of corrosion of NiCu low alloy steel in the test solution was investigated by electrochemical measurements. XRD was used to illustrate the composition of formed corrosion products. SEM was used to observe the electrode surface morphology and the cross section of the rust layer. The electrochemical results showed that low alloy steel has a lower corrosion rate and is less prone to localized corrosion than low carbon steel. In order to understand the mechanism of alloying elements, EDS and EPMA were used to analyse the distribution of alloying elements cross-sectional. XPS and E-pH diagram were used to estimate the possible existence form of alloying elements. By means of EDS and EPMA, it was founded that Ni is concentrated in the inner rust layer while the enrichment of Cu is not so obvious. XRD, XPS and E-pH results indicated that Ni and Cu are existed in the form of NiFe2O4 and CuFeO2 respectively.

Key words: low alloy steel; rust; HCO3-; Cl-

Cite this article

Yunfei LU , Jingfeng YANG , Junhua DONG , Wei KE . THE CORROSION BEHAVIOUR OF NiCu LOW ALLOY STEEL IN A DEAERATED BICARBONATE SOLUTION CONTAINING Cl- IONS[J]. Acta Metall Sin, 2015 , 51(4) : 440 -448 . DOI: 10.11900/0412.1961.2014.00349

References

[1] Wang J, Su R, Chen W M, Guo Y H, Jin Y X, Wen Z J, Liu Y M. Chin J Rock Mech Eng, 2006; 25: 649
[1] (王 驹, 苏 锐, 陈伟明, 郭永海, 金远新, 温志坚, 刘月妙. 岩石力学与工程学报, 2006; 25: 649)
[2] Bennett D G, Gens R. J Nucl Mater, 2008; 379: 1
[3] Nishimura T. J Nucl Mater, 2009; 385: 495
[4] Kursten B, Druyts F, MacDonald D D, Smart N R, Gens R, Wang L, Weetjens E, Govaerts J. Corros Eng Sci Technol, 2011; 46: 91
[5] Taniguchi N, Suzuki H, Kawasaki M, Naito M, Kobayashi M, Takahashi R, Asano H. Corros Eng Sci Technol, 2011; 46: 117
[6] Xia X, Idemitsu K, Arima T, Inagaki Y, Ishidera T, Kurosawa S, Iijima K, Sato H. Appl Clay Sci, 2005; 28: 89
[7] Lu C, Samper J, Fritz B, Clement A, Montenegro L. Phys Chem Earth, 2011; 36: 1661
[8] Neff D, Dillmann P, Bellot-Gurlet L, Beranger G. Corros Sci, 2005; 47: 515
[9] Neff D, Saheb M, Monnier J, Perrin S, Descostes M, L'Hostis V, Crusset D, Millard A, Dillmann P. J Nucl Mater, 2010; 402: 196
[10] Yang J F, Dong J H, Ke W. Acta Metall Sin, 2011; 47: 1321
[10] (阳靖峰, 董俊华, 柯 伟. 金属学报, 2011; 47: 1321)
[11] Taniguchi N, Honda A, Ishikawa H. Mater Res Soc Symp Proc, 1998; 506: 495
[12] Nishimura T, Katayama H, Noda K, Kodama T. Corros Sci, 2000; 42: 1611
[13] Wang Z, Liu J, Wu L, Han R, Sun Y. Corros Sci, 2013; 67: 1
[14] Cao G L, Li G M, Chen S, Chang W S, Chen X Q. Acta Metall Sin, 2011; 47: 145
[14] (曹国良, 李国明, 陈 珊, 常万顺, 陈学群. 金属学报, 2011; 47: 145)
[15] Matsushima I,translated by Jing Y K. Low-Alloy Corrosion Resistant Steels: A History of Development, Application and Research. Beijing: Metallurgic Industry Press, 2004: 100
[15] (松岛 岩 著,靳裕康 译. 低合金耐蚀钢—开发、发展及研究. 北京: 冶金工业出版社, 2004: 100)
[16] Kihira H, Kimura M. Corrosion, 2011; 67: 1
[17] Serdar M, Zulj L V, Bjegovic D. Corros Sci, 2013; 69: 149
[18] Mansfeld F, Lin S, Chen Y C, Shih H. J Electrochem Soc, 1988; 135: 906
[19] Bessone J, Mayer C, Juttner K, Lorenz W J. Electrochim Acta, 1983; 28: 171
[20] Cao C N,Zhang J Q. Introduction of Electrochemical Impedance Spectroscopy. Beijing: Science Press, 2002: 135
[20] (曹楚南,张鉴清. 电化学阻抗谱导论. 北京: 科学出版社, 2002: 135)
[21] Hao L, Zhang S X, Dong J H, Ke W. Corros Sci, 2012; 54: 244
[22] Kimura M, Kihira H, Ohta N, Hashimoto M, Senuma T. Corros Sci, 2005; 47: 2499
[23] Chen X H, Dong J H, Han E H, Ke W. Mater Lett, 2007; 61: 4050
[24] Nishimura T, Kodama T. Corros Sci, 2003; 45: 1073
[25] Hao L, Zhang S X, Dong J H, Ke W. Corros Sci, 2011; 53: 4187
Outlines

/

〈 〉