MICRO-CHARACTERIZATION OF DISSIMILAR METAL WELD JOINT FOR CONNECTING PIPE- NOZZLE TO SAFE-END IN GENERATION III NUCLEAR POWER PLANT
Revised date: 2014-06-06
Online published: 2015-05-01
The dissimilar metal weld joint (DMWJ) in primary water system of pressurized water reactors (PWRs) has been proven to be a vulnerable component owing to its proneness to different type of flaws. Thus, maintaining integrity of such joint in case of defect presence is of great importance to the design and safe management of nuclear power plants (NPPs). For a reliable integrity analysis of DMWJ, it is essential to understand the microscopic characteristics in all regions of the joint. In this work, OM, TEM, SEM, durometer, AFM, MFM and SKPFM were utilized to investigate the microstructure, micro-hardness and the distribution of main elements, grain boundary characteristic and residual strain in the A508/52M/316L DMWJ that used for connecting the pipe safe-end and the nozzle of reactor pressure vessel in PWRs, and a comparative analysis about the microstructure and property along the radical direction of the DMWJ was obtained. The results showed that there was no region that differed from the other part of the weldment in terms of the microstructure and micro-hardness dramatically. A layer of fine grain resulting from unmelted filler metal was found in the backing weld part of the joint. The residual strain in the heat affected zone (HAZ) of 316L was higher than that in other regions. Meanwhile, drastic variations in the microstructure, chemical composition distribution and grain boundary character distribution (GBCD) in both the 316L/52Mw and the 52Mb/A508 interface regions were observed. The analyses using TEM and MFM test showed that a large number of chromium and molybdenum-rich precipitates particles distributed both along the grain boundaries and inside grains in the 316L base metal, which were identified to be precipitates with complex elementary composition rather than the normal string delta ferrite in 316L austenitic stainless steel. The SKPFM test result indicated that these precipitates were more prone to be corroded than the base metal. Therefore, further investigation about the cause of deformation and the impacts to the corrosion resistance, particularly the stress corrosion cracking (SCC) sensitivity of the precipitates needs to be carried out.
Jie DING , Zhiming ZHANG , Jianqiu WANG , En-Hou HAN , Weibao TANG , Maolong ZHANG , Zhiyuan SUN . MICRO-CHARACTERIZATION OF DISSIMILAR METAL WELD JOINT FOR CONNECTING PIPE- NOZZLE TO SAFE-END IN GENERATION III NUCLEAR POWER PLANT[J]. Acta Metall Sin, 2015 , 51(4) : 425 -439 . DOI: 10.11900/0412.1961.2014.00299
| [1] | Han E H, Wang J Q, Wu X Q, Ke W. Acta Metall Sin, 2010; 46: 1379 |
| [1] | (韩恩厚, 王俭秋, 吴欣强, 柯 伟. 金属学报, 2010; 46: 1379) |
| [2] | Joseph A,Rai S K,Jayakumar T,Murugan N. Int J Pressure Vessels Piping, 2006; 82: 700 |
| [3] | Seifert H P, Ritter S, Shoji T. J Nucl Mater, 2008; 378: 197 |
| [4] | Wang H T, Wang G Z, Xuan F Z, Tu S T. Eng Failure Analysis, 2013; 28: 134 |
| [5] | Peng Q J, Xue H, Hou J, Sakaguchi K, Takeda Y, Kuniya J, Shoji T. Corros Sci, 2011; 53: 4309 |
| [6] | Hou J, Peng Q J, Kuniya J, Shoji T, Wang J Q, Han E H, Ke W. J Mater Sci, 2010; 397: 109 |
| [7] | Li G F, Congleton J. Corros Sci, 2000; 42: 1005 |
| [8] | Meng F J, Wang J Q, Han E H, Shoji T, Ke W. Acta Metall Sin, 2011; 47: 839 |
| [8] | (孟凡江, 王俭秋, 韩恩厚, 庄子哲雄, 柯 伟. 金属学报, 2011; 47: 839) |
| [9] | Bowerman B S, Czajkowski C J, Roberts T C, Neal C. Mater Charact, 1999; 43: 347 |
| [10] | Li G F, Li G J, Fang K W, Peng J, Yang W. Acta Metall Sin, 2011; 47: 797 |
| [10] | (李光福, 李冠军, 方可伟, 彭 君, 杨 武. 金属学报, 2011; 47: 797) |
| [11] | Wang H T, Wang G Z, Xuan F Z, Liu F Z, Tu S T. Mater Sci Eng, 2013; A568: 108 |
| [12] | Choi K J, Kim J J, Lee B H, Bahn C B, Kim J H. J Nucl Mater, 2013; 441: 493 |
| [13] | Hou J, Peng Q J, Lu Z P, Shoji T, Wang J Q, Han E H, Ke W. Corros Sci, 2010; 52: 3949 |
| [14] | Hanninen H, Brederholm A, Toivonen A. 15th Int Conf on Environmental Degradation of Materials in Nuclear Power Systems-Water Reactors, Colorado Springs: TMS, 2011: 197 |
| [15] | Sathirathinda N, Gubner R, Pan J, Kivisakk U. Electrochem Solid-State Lett, 2008; 11: C41 |
| [16] | Kasper J S. Acta Metall, 1954; 2: 456 |
| [17] | Michalska J, Sozanska M. Mater Charact, 2006; 56: 355 |
| [18] | Popov A A, Bannikova A S, Belikov S V. Phys Met Metall, 2009; 108: 586 |
| [19] | Chun E J, Baba H, Nishimoto K, Saida K. Mater Charact, 2013; 86: 152 |
| [20] | Escriba D M, Materna-Morris E, Plaut R L, Padilha A F. Mater Charact, 2009; 60: 1214 |
| [21] | Martin D S,Rivera Diaz del Castillo P E J, Peekstok E van del Zwaag S. Mater Charact, 2007; 58: 455 |
| [22] | Lai J K L, Meshukat M. Met Sci, 1978; 9: 416 |
| [23] | Falata L, Svoboda M, Vyrostkova A, Petryshynets I, Sopko M. Mater Charact, 2012; 72: 15 |
| [24] | Naffakh H, Shamanian M, Ashrafizadeh F. J Mater Process Technol, 2009; 209: 3628 |
| [25] | Nelson T W, Lippold J C, Mills M J. Sci Technol Weld Joining, 1998; 77: 249 |
| [26] | Rowe M D, Nelson T W, Lippold J C. Sci Technol Weld Joining, 1999; 78: 31 |
| [27] | Srinivasan P B, Muthupandi V, Dietzel W, Sivan V. Mater Des, 2006; 27: 182 |
| [28] | Hou J, Peng Q J, Shoji T, Wang J Q, Ke W, Han E H. Acta Metall Sin, 2010; 46: 1258 |
| [28] | (侯 娟, 彭群家, 庄子哲雄, 王俭秋, 柯 伟, 韩恩厚. 金属学报, 2010; 46: 1258) |
| [29] | Asami K, Sakai T. Trans Iron Steel Inst Jpn, 1981; 21: B269 |
| [30] | Nelson T W, Lippold J C, Mills M J. Sci Technol Weld Joining, 1999; 78: 329 |
| [31] | Nelson T W, Lippold J C, Mills M J. Sci Technol Weld Joining, 2000; 79: 267 |
| [32] | Hou J, Peng Q J, Takeda Y, Kuniya J, Shoji T, Wang J Q, Han E H, Ke W. J Mater Sci, 2010; 45: 5332 |
| [33] | Wang H T. PhD Dissertation, East China University of Science and Technology, Shanghai, 2013 |
| [33] | (王海涛. 华东理工大学博士学位论文, 上海, 2013) |
| [34] | Naffakh H, Shamanian M, Ashrafizadeh F. J Mater Process Technol, 2009; 209: 3628 |
| [35] | Gertsman V Y, Tangri K, Valiev R Z. Acta Metall Mater, 1994; 42: 1785 |
| [36] | Gertsman V Y, Bruemmer S M. Acta Mater, 2001; 49: 1589 |
| [37] | Lehockey E M, Brennenstuhl A M, Thompson I. Corros Sci, 2004; 46: 2383 |
| [38] | Pan Y, Adams B L, Olson T, Panayotou N. Acta Mater, 1996; 44: 4685 |
| [39] | Lee H T, Wu J L. Corros Sci, 2009; 51: 733 |
| [40] | Qiao D, Zhang W, Pan T Y, Crooker P, David S, Feng Z. Sci Technol Weld Joining, 2013; 92: 624 |
/
| 〈 |
|
〉 |