MICROSTRUCTURE EVOLUTION AND MECHANICAL PROPERTIES OF TC1 ALLOY FABRICATED BY PLASMA ARC COLD HEARTH MELTING DURING ROLLING PROCESS

  • Mengying LIU ,
  • Hai CHANG ,
  • Feng XU ,
  • Zhengfang XU ,
  • Zhao YANG ,
  • Ning WANG ,
  • Weimin GAN ,
  • Qiang FENG
Expand
  • 1 National Center for Materials Service Safety, University of Science and Technology Beijing, Beijing 100083
    2 Baosteel Special Metals Co., Ltd., Shanghai 200940
    3 Helmholtz-Zentrum Geesthacht, Out Station at FRM2, Garching, Germany, 85747
    4 State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083

Revised date: 2014-10-23

  Online published: 2015-03-25

Supported by

Supported by National Natural Science Foundation of China (No.51201006) and Programme of Introducing Talents of Discipline to Universities (No.B12012)

Abstract

Plasma arc cold hearth melting (PAM) is an effective technology to produce high purity titanium alloy ingots which are widely used in aeronautic and astronautic industries. To date, the development of PAM in our country is still at initial stage. It is necessary to investigate the melting parameters of PAM and the following thermal mechanical processing of the ingots fabricated by PAM. In this study, the TC1 alloy ingots casted by PAM were cogged at b transus temperature and then rolled by unidirectional rolling and cross rolling in the a+b phase field. The typical widmanstatten structure of cast-ingots turned to transformed b morphology after cogging at b transus temperature in which the a phases forms in smaller colonies of laths. After the unidirectinal rolling in the a+b phase field, the a colonies were distorted and the a laths re-arranged along the rolling direction, while they had weaker directivity after cross rolling. The sheets rolled by both unidirectional and cross rolling showed typical prismatic texture. After annealing treatment below the b transus temperature, the a phases turned to equiaxial morphology. The ambient yield strength of the sheet in transverse direction was significantly higher than in rolling direction, which could be attributed to the strong prismatic texture introduced by hot rolling process.

Cite this article

Mengying LIU , Hai CHANG , Feng XU , Zhengfang XU , Zhao YANG , Ning WANG , Weimin GAN , Qiang FENG . MICROSTRUCTURE EVOLUTION AND MECHANICAL PROPERTIES OF TC1 ALLOY FABRICATED BY PLASMA ARC COLD HEARTH MELTING DURING ROLLING PROCESS[J]. Acta Metall Sin, 2015 , 51(3) : 341 -348 . DOI: 10.11900/0412.1961.2014.00575

References

[1] Mo W. Titanium. Beijing: Metallugical Industry Press, 2008: 330
[1] (莫 畏. 钛. 北京: 冶金工业出版社, 2008: 330 )
[2] Ma J M,He J Y,Pang K C. Ingot and Forging of Titanium. Beijing: Metallugical Industry Press, 2012: 82
[2] (马济民,贺金宇,庞克昌. 钛铸锭和锻造. 北京: 冶金工业出版社, 2012: 82)
[3] Chinnis W R. Titanium 1990: Products and Application, 1990; 2: 830
[4] Tian Y X, Li S J, Hao Y L, Yang R. Acta Metall Sin, 2012; 48: 837
[4] (田宇兴, 李述军, 郝玉琳, 杨 锐. 金属学报, 2012; 48: 837)
[5] Zhang Z Q, Dong L M, Yang Y, Guan S X, Liu Y Y, Yang R. Acta Metall Sin, 2011; 47: 1257
[5] (张志强, 董利民, 杨 洋, 关少轩, 刘羽寅, 杨 锐. 金属学报, 2011; 47: 1257)
[6] Wang T, Guo H, Wang Y, Yao Z. Mater Sci Eng, 2010; A528: 736
[7] Ding R, Guo Z X, Wilson A. Mater Sci Eng, 2002; A327: 233
[8] Lütjering G. Mater Sci Eng, 1998; A243: 32
[9] Roy S, Karanth S, Suwas S. Metall Mater Trans, 2013; 44A: 3322
[10] Gurao N P, Ali A A, Suwas S. Mater Sci Eng, 2009; A504: 24
[11] You L, Song X P. Acta Metall Sin, 2008; 44: 1310
[11] (尤 力, 宋西平. 金属学报, 2008; 44: 1310)
[12] Qin G H, Wang W B, Ji B, Wu Y Y. Chin J Nonferrous Met, 2010; 20: 877
[12] (秦桂红, 王万波, 计 波, 吴英彦. 中国有色金属学报, 2010; 20: 877)
[13] Song J H, Hong K J, Ha T K, Jeong H T. Mater Sci Eng, 2007; A449-451: 144
[14] Zheng J M, Lei R Q. Titanium Industry Progress, 2008; 25(4): 27
[14] (郑建民, 雷让歧. 钛工业进展, 2008; 25(4): 27)
[15] Boehlert C J. Mater Sci Eng, 2000; A279: 118
[16] Mao W M,Yang P,Chen L. Analysis Principle of Texture and Testing Technique . Beijing: Metallugical Industry Press, 2008: 15
[16] (毛卫民,杨 平,陈 冷.材料织构分析原理与检测技术. 北京: 冶金工业出版社, 2008: 15)
[17] Philippe M J, Esling C, Hocheid B. Textures Microstruct, 1988; 7: 265
[18] Salem A A, Glavicic M G, Semiatin S L. Mater Sci Eng, 2008; A496: 169
[19] Warwick J L W, Jones N G, Bantounas I, Preuss M, Dye D. Acta Mater, 2013; 61: 1603
[20] Singh A K, Schwarzer R A. Mater Sci Eng, 2001; A307: 151
[21] Gey N, Humbert M, Philippe M J, Combres Y. Mater Sci Eng, 1996; A219: 80
[22] Russell A M, Chumbley L S, Ellis T W, Laabs F C, Norris B, Donizetti G E. J Mater Sci, 1995; 30: 4249
[23] Zhu Z S, Gu J L, Chen N P. Chin J Nonferrous Met, 1995; 5: 83
[23] (朱知寿, 顾家琳, 陈南平. 中国有色金属学报, 1995; 5: 83)
[24] Zhu Z S, Gu J L, Chen N P, Yang Z S. Mater Mech Eng, 1994; 18(6): 23
[24] (朱知寿, 顾家琳, 陈南平, 杨照苏. 机械工程材料, 1994; 18(6): 23)
[25] Lin P, Feng A, Yuan S, Li G, Shen J. Mater Sci Eng, 2013; A563: 16
Outlines

/

〈 〉