INFLUENCE OF PULSED MAGNETIC TREATMENT ON MICROSTRUCTURES AND MECHANICAL PROPERTIES OF M42 HIGH SPEED STEEL TOOL

  • Liping MA ,
  • Zhiqiang LIANG ,
  • Xibin WANG ,
  • Wenxiang ZHAO ,
  • Li JIAO ,
  • Zhibing LIU
Expand
  • Key Laboratory of Fundamental Science for Advanced Machining, Beijing Institute of Technology, Beijing 100081

Revised date: 2014-06-02

  Online published: 2015-03-25

Supported by

Supported by National Natural Science Foundation of China (Nos.50935001 and 51205024)

Abstract

Magnetic treatment of tools is a novel method to increase tool life in which the tool is magnetized before cutting or the cutting is performed in a magnetic field. The method has many attractive features, such as short treatment time and no pollution. However, this approach has not been widely applied yet, since the mechanism of magnetic treatment of tools is not clear and treatment results are affected by many factors. Therefore, it is important to study the mechanism of magnetic treatment of tools. This work aims to study the influence of pulsed magnetic treatment on microstructures and mechanical properties of M42 (W2Mo9Cr4VCo8) high speed steel, which is a typical tool material which contains high amounts of cobalt. So it can show a stronger magnetism in the process of pulsed magnetic treatment. Changes of dislocation configuration, carbide distribution and microstructure before and after magnetic treatment were characterized by TEM and laser scanning confocal microscope. Moreover, Rockwell hardness and micro-hardness were measured to quantitatively investigate the influence of magnetic treatment on the mechanical properties. Results showed that after pulsed magnetic treatment the lattice of material was distorted, the carbide was precipitated, and the microstructure and crystalline grain were refined. The changes of microstructure led to changes of mechanical properties, of which the Rockwell hardness and micro-hardness were significantly increased. The maximum increase of Rockwell hardness was 2.9 HRC. Ultimately, the strengthening mechanisms of high speed steel were analyzed based on dislocation theory. It was shown that the subjected force of dislocations due to the magnetic treatment could overcome the centripetal restoring force and the Peierls stress of dislocations. Therefore, dislocations proliferated by the Orowan dislocation strengthening mechanism, and dislocation density increased. The dislocation configuration determined from TEM micrographs was in good agreement with the discussion of dislocation mechanisms.

Cite this article

Liping MA , Zhiqiang LIANG , Xibin WANG , Wenxiang ZHAO , Li JIAO , Zhibing LIU . INFLUENCE OF PULSED MAGNETIC TREATMENT ON MICROSTRUCTURES AND MECHANICAL PROPERTIES OF M42 HIGH SPEED STEEL TOOL[J]. Acta Metall Sin, 2015 , 51(3) : 307 -314 . DOI: 10.11900/0412.1961.2014.00295

References

[1] Li G R, Zhao Y T, Dai Q X, Zhang H J, Wang H M. J Univ Sci Technol Beijing, 2007; 14: 460
[2] Miller P C. Tool Prod, 1990; 55: 100
[3] Batainech O, Klamecki B, Koepke B G. J Mater Process Technol, 2003; 134: 190
[4] E1 Mansori M, Pierron F, Paulmier D. Surf Coat Technol, 2003; 163: 472
[5] E1 Mansori M, Lordache V, Seitier P, Paulmier D. Surf Coat Technol, 2004; 188: 566
[6] Mkaddem A, Benabou A, E1 Mansori M, Clenet S. Int J Solids Struct, 2013; 50: 2078
[7] E1 Mansori M, Schmitt M, Paulmier D. Surf Coat Technol, 1998; 108-109: 479
[8] E1 Mansori M, Paulmier D. Appl Surf Sci, 1999; 144-145: 233
[9] Chin K J, Zaidi H, Nguyen M T, Renault P O. Wear, 2001; 250: 470
[10] Chin K J, Zaidi H, Mathia T. Wear, 2005; 259: 477
[11] Singh S, Shan H S, Kumar P. J Mater Process Technol, 2002; 128: 155
[12] Klamecki B E. J Mater Process Technol, 2003; 141: 385
[13] Tang F, Lu A L, Fang H Z, Mei J F. Mater Sci Eng, 1998; A248: 98
[14] Cai Z P, Huang X Q. Mater Sci Eng, 2011; A528: 6287
[15] Zaidi H, Pan L, Paulmier D, Robert F. Wear, 1995; 181: 799
[16] Jiang J L, Tian Y, Meng Y G. Wear, 2011; 271: 2991
[17] Fahmy Y, Hare T, Tooke R, Conrad H. Scr Mater, 1998; 38: 1355
[18] Bose M S C. Phys Status Solidi, 1984; 86A: 649
[19] Zhong W D. Ferromagnetics. Beijing: Science Press, 1987: 7
[19] (钟文定.铁磁学. 北京: 科学出版社, 1987: 7)
[20] Li G R, Wang H M, Yuan X T, Cai Y. Chin J Mater Res, 2013; 27: 397
[20] (李桂荣, 王宏明, 袁雪婷, 蔡 云. 材料研究学报, 2013; 27: 397)
[21] Lei T Q,Yao Z K,Yang D Z. Thermomechanical Treatment of Steel. Beijing: China Machine Press, 1979: 135
[21] (雷廷权,姚忠开,杨德庄. 钢的形变热处理. 北京: 机械工业出版社, 1979: 135)
[22] Xu B J, Gu N J, Yan D R, Yin F X. Acta Metall Sin, 1989; 25: 352
[22] (徐伯钧, 谷南驹, 阎殿然, 殷福星. 金属学报, 1989; 25: 352)
[23] Sun Z J. Heat Treat, 2002; 17(1): 37
[23] (孙忠继. 热处理, 2002; 17(1): 37 )
[24] Ferreira P J, Vander S J B. Scr Mater, 1999; 41: 117
[25] Wang Y N,Chen S J,Dong X C. Dislocation Theory and its Applications. Beijing: Metallurgical Industry Press, 2007: 35
[25] (王亚男,陈树江,董希淳. 位错理论及其应用. 北京: 冶金工业出版社, 2007: 35)
[26] Li H Q, Chen Q Z, Wang Y B, Chu W Y. Chin Sci Bull, 1997; 42: 2282
[26] (李红旗, 陈奇志, 王燕斌, 褚武扬. 科学通报, 1997; 42: 2282)
Outlines

/

〈 〉