INFLUENCE OF PRE-DEFORMATION ON THE PRECIP- ITATION BEHAVIORS OF Al-Mg-Si-Cu ALLOY FOR AUTOMOTIVE APPLICATION

  • Li CUI ,
  • Mingxing GUO ,
  • Xiangyang PENG ,
  • Yan ZHANG ,
  • Jishan ZHANG ,
  • Linzhong ZHUANG
Expand
  • State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing,Beijing 100083

Revised date: 2014-07-01

  Online published: 2015-03-25

Supported by

Supported by National High Technology Research and Development Program of China (No.2013AA032403), National Natural Science Foundation of China (No.51301016), Fundamental Research Funds for the Central Universities (No.FRF-TP-14-097A2) and Beijing Higher Education Young Elite Teacher Project in 2013 (No.YETP0409 )

Abstract

To reduce the weight of car body, Al-Mg-Si-Cu alloys have been widely used to produce outer body panels of automobiles due to their favorable high strength-to-weight ratio, corrosion resistance, weldability and good formability. Al-Mg-Si-Cu alloys belong to age-hardenable aluminium alloys, whose strength derives mainly from the matrix precipitation during aging treatments. However, their bake hardening response still need to be further improved to enhance their dent resistance. A novel thermo-mechanical treatment consisting of conventional pre-aging, pre-deformation and re-aging was developed to enhance the tensile properties and bake hardening increment of Al-Mg-Si-Cu alloys. In this work, the effect of pre-deformation on the precipitation behaviors of Al-Mg-Si-Cu alloy was studied by DSC, mechanical property measurement and TEM. The results show that, the GP zone dissolution rate decreases with increasing pre-deformation during the slow heating up process for the pre-aged alloy, the corresponding activation energies of 0, 5% and 15% pre-deformed alloy calculated by Avrami-Johnson-Mehl method are 137.1, 189.5 and 141.3 kJ/mol, respectively. If the pre-deformed alloys are directly bake hardened at 185 ℃ for 20 min, precipitation and bake hardening increment can be greatly improved by pre-deformation (the highest bake hardening increment is 160 MPa), but the bake hardening increment rate gradually decreases if the pre-deformation is above 10%. In addition, the GP zone dissolution rates of pre-deformed alloys after bake hardening treatment are much lower when the heat treatment temperatures are below one certain value, but if the treatment temperatures above it, the corresponding GP zone dissolution rates are higher than that of alloy without pre-deformation, finally, the activation energy changes from high value to low value even can be observed in the ln[(dY/dT)φ/f(Y)]-1/T curve. For the precipitation in the alloys, with increasing pre-deformation, its activation energy gradually decreases, corresponding gradually increase of precipitation rate.

Cite this article

Li CUI , Mingxing GUO , Xiangyang PENG , Yan ZHANG , Jishan ZHANG , Linzhong ZHUANG . INFLUENCE OF PRE-DEFORMATION ON THE PRECIP- ITATION BEHAVIORS OF Al-Mg-Si-Cu ALLOY FOR AUTOMOTIVE APPLICATION[J]. Acta Metall Sin, 2015 , 51(3) : 289 -297 . DOI: 10.11900/0412.1961.2014.00348

References

[1] Birol Y. Mater Sci Eng, 2005; A391: 175
[2] Roven H J, Liu M P, Werenskiold J C. Mater Sci Eng, 2008; A483: 54
[3] Esmaeili S, Wang X, Lloyd D J, Poole W J. Metall Mater Trans, 2003; 34A: 751
[4] Shen C H. J Mater Sci Technol, 2011; 27: 205
[5] Esmaeili S, Lloyd D J, Poole W J. Mater Lett, 2005; 59: 575
[6] Shen C H, Ou B L. J Chin Inst Eng, 2008; 31: 181
[7] Staab T E M, Krause-rehberg R. J Mater Sci, 2006; 41: 1059
[8] Gupta A K, Lloyd D J, Court S A. Mater Sci Eng, 2001; A301: 140
[9] He L Z, Zhang H T, Cui J Z. J Mater Sci Technol, 2010; 26: 141
[10] Han Y, Ma K, Li L, Chen W, Nagaumi H. Mater Des, 2012; 39: 418
[11] Cai M, Field D P, Lorimer G W. Mater Sci Eng, 2004; A373: 65
[12] Gupta A K, Jena A K, Chaturvedi M C. Scr Metall, 1988; 22: 369
[13] Jena A K, Gupta A K, Chaturvedi M C. Acta Metall, 1989; 37: 885
[14] Ghosh K S, Gao N. Trans Nonferrous Met Soc China, 2011; 21: 1199
[15] Ghosh K S, Das K, Chatterjee U K. Mater Sci Technol, 2004; 20: 825
[16] Oguocha I N A, Yannacopoulos S. Mater Sci Eng, 1997; A231: 25
[17] Gupta A K, Marois P H, Lloyd D J. Mater Sci Forum, 1996; 217: 801
[18] Gupta A K, Lloyd D J. Metall Mater Trans, 1999; 30A: 879
[19] Luo A, Lloyd D J, Gupta A, Youdelis W V. Acta Metall Mater, 1993; 41: 769
[20] Zhang Q X, Guo M X, Hu X Q, Cao L Y, Zhuang L Z, Zhang J S.Acta Metall Sin, 2013; 49: 1604
[20] (张巧霞, 郭明星, 胡晓倩, 曹零勇, 庄林忠, 张济山. 金属学报, 2013; 49: 1604)
[21] Edwards G A, Stiller K, Dunlop G L, Couper M J. Acta Mater, 1998; 46: 3893
[22] De Geuser F, Lefebvre W, Blavette D. Philos Mag Lett, 2006; 86: 227
[23] Bryant J D. Metall Mater Trans, 1999; 30A: 1999
[24] Brandes E A, Brook G B. Smithells Metals Reference Book. 7th Ed., Bath: Reed Educational and Professional Publishing Ltd., 1992: 73
[25] Sha G, M?ller H, Stumpf W E, Xia J H, Govender G, Ringer S P. Acta Mater, 2012; 60?: 692
[26] Hirata T, Matsuo S. Trans Nat Res Inst Met, 1973; 15: 271
Outlines

/

〈 〉