DEVELOPMENT OF AN INVERSE HEAT TRANSFER MODEL BETWEEN MELT AND SHOT SLEEVE AND ITS APPLICATION IN HIGH PRESSURE DIE CASTING PROCESS

  • Yongyou CAO ,
  • Shoumei XIONG ,
  • Zhipeng GUO
Expand
  • School of Materials Science and Engineering, Tsinghua University, Beijing 100084

Accepted date: 2015-03-03

  Online published: 2015-03-31

Supported by

Supported by National Natural Science Foundation of China (Nos.51275269 and 51205229) and National Science and Technology Major Project (No.2012ZX04012011)

Abstract

A 2D inverse heat transfer model between molten metal and shot sleeve was based on the nonlinear estimation method. Die casting experiments under both non-shot and shot conditions (via the plunger) were performed using an Al-9%Si-3%Cu alloy. Based on the temperature measurements from thermocouples embedded inside the shot sleeve, the temperature distribution of molten metal and interfacial heat transfer coefficient (IHTC) were successfully determined. Results show that the heat transfer behavior of non-shot condition was different from that in the shot condition, but the IHTC in the middle zone of shot sleeve decreased along the plunger moving direction. Besides, the surface temperature of shot sleeve was higher in both pouring zone and end zone while lower in the middle zone. In accordance to the movement of the plunger, the IHTC profile in the end zone exhibited double peaks.

Cite this article

Yongyou CAO , Shoumei XIONG , Zhipeng GUO . DEVELOPMENT OF AN INVERSE HEAT TRANSFER MODEL BETWEEN MELT AND SHOT SLEEVE AND ITS APPLICATION IN HIGH PRESSURE DIE CASTING PROCESS[J]. Acta Metall Sin, 2015 , 51(6) : 745 -752 . DOI: 10.11900/0412.1961.2014.00604

References

[1] Guo Z P, Xiong S M, Liu B C, Li M, Allison J. Int J Heat Mass Transfer, 2008; 51: 6032
[2] Guo Z P, Xiong S M, Liu B C, Li M, Allison J. Int J Cast Met Res, 2011; 24: 151
[3] Song J, Xiong S M, Li M, Allison J. Mater Sci Eng, 2009; A520: 197
[4] Helenius R, Lohne O, Arnberg L, Laukli H I. Mater Sci Eng, 2005; A413: 52
[5] Jia L R, Xiong S M, Liu B C. J Mater Sci Technol, 2000; 16: 269
[6] Wu M W, Xiong S M. Acta Metall Sin, 2010; 46: 1534 (吴孟武, 熊守美. 金属学报, 2010; 46: 1534)
[7] Hamasaiid A, Dour G, Dargusch M S, Loulou T, Davidson C, Savage G. Metall Mater Trans, 2008; 39A: 853
[8] Long A, Thornhill D, Armstrong C, Watson D. Appl Therm Eng, 2011; 31: 3996
[9] Guo Z P, Xiong S M, Liu B C, Li M, Allison J. Metall Mater Trans, 2008; 39A: 2896
[10] Cao Y Y, Guo Z P, Xiong S M. China Foundry, 2014; 11: 314
[11] Guo Z P, Xiong S M, Cho S H, Choi J K. Acta Metall Sin, 2007; 43: 607 (郭志鹏, 熊守美, 曺尚铉, 崔正吉. 金属学报, 2007; 43: 607)
[12] Guo Z P, Xiong S M, Cho S H, Choi J K. Acta Metall Sin, 2007; 43: 1149 (郭志鹏, 熊守美, 曺尚铉, 崔正吉. 金属学报, 2007; 43: 1149)
[13] Shi Q. PhD Dissertation, Ohio State University, 2002
[14] Beck J V, Blackwell B, Clair C R. Inverse Heat Conduction: Ill-posed Problems. New York: Wiley, 1985: 308
Outlines

/

〈 〉