FORMATION AND MODELING OF VERTICAL OUTSIDE WALL OF COMPOENTS INCLINING INWARD IN LASER SOLID FORMING

  • Menghua SONG ,
  • Xin LIN ,
  • Fenggang LIU ,
  • Haiou YANG ,
  • Weidong HUANG
Expand
  • State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072

Accepted date: 2015-01-12

  Online published: 2015-03-27

Supported by

Supported by National Natural Science Foundation of China (No.51323008), National Basic Research Program of China (No.2011CB610402), High Technology Research and Development Program of China (No.2013AA031103) and Fund of State Key Laboratory of Solidification Processing in NWPU (No.91-QZ-2014)

Abstract

The vertical outside wall is prone to incline inward in laser solid forming, which will deteriorate the dimension precision and processing stability. For solving this problem, samples with different amount of deposited layers were prepared and the variation of boundary single-track clad shape and formation of vertical outside wall inclining inward were investigated. Based on the method of constructing cross-section profile of the single-track clad by height of powders accumulated in molten pool, an analytical model was developed to describe the evolution of vertical outside wall during multilayer superimposition. A series of vertical outside walls under different width/height ratios and critical defocus distance were constructed with this model to investigate their influence. Results indicate that the deposited single-track clad will influence the formation of single-track clad under depositing. Due to the arc-like cross-section profile of single-track clad, the molten pool will shrink inward, which leads the outer edge of boundary single-track clad to shrink inward then the vertical outside wall to incline inward. However, this incline will decrease with the increase of deposited height. For the initial single-track clad with fixed width, decreasing critical defocus distance can decrease the inward incline but increase the offset from the preset dimension. The width/height ratio almost has no effect on outside wall.

Cite this article

Menghua SONG , Xin LIN , Fenggang LIU , Haiou YANG , Weidong HUANG . FORMATION AND MODELING OF VERTICAL OUTSIDE WALL OF COMPOENTS INCLINING INWARD IN LASER SOLID FORMING[J]. Acta Metall Sin, 2015 , 51(6) : 753 -761 . DOI: 10.11900/0412.1961.2014.00631

References

[1] Huang W D,Lin X,Chen J,Liu Z X,Li Y M. Laser Solid Forming—the Rapid and Free Fabricating of High Performance Metal Components. Xi'an: Northwestern Polytechnical University Press, 2007: 1 (黄卫东,林 鑫,陈 静,刘振侠,李延民. 激光立体成形—高性能致密金属零件的快速自由成形. 西安: 西北工业大学出版社, 2007: 1)
[2] Liu F, Lin X, Yang G, Song M, Chen J, Huang W. Opt Laser Technol, 2011; 43: 208
[3] Yang G, Lin X, Liu F, Hu Q, Ma L, Li J, Huang W. Intermetallics, 2012; 22: 110
[4] Cao J, Liu F, Lin X, Huang C, Chen J, Huang W. Opt Laser Technol, 2013; 45: 228
[5] Lin X, Cao Y, Wu X, Yang H, Chen J, Huang W. Mater Sci Eng, 2012; A553: 80
[6] Vrancken B, Thijs L, Kruth J P, Van Humbeeck J. Acta Mater, 2014; 68: 150
[7] Yang H O, Song M H, Yang D H, Lin X, Chen J, Huang W D. Appl Laser, 2011; 31: 384 (杨海欧, 宋梦华, 杨东辉, 林 鑫, 陈 静, 黄卫东. 应用激光, 2011; 31: 384)
[8] Xu Q D, Lin X, Song M H, Yang H O, Huang W D. Acta Metall Sin, 2013; 49: 605 (徐庆东, 林 鑫, 宋梦华, 杨海欧, 黄卫东. 金属学报, 2013; 49: 605)
[9] Huang W D, Lin X. Mater China, 2010; (6): 12 (黄卫东, 林 鑫. 中国材料进展, 2010; (6): 12)
[10] Gu D D, Meiners W, Wissenbach K, Poprawe R. Int Mater Rev, 2012; 57: 133
[11] Li Y, Yang H, Lin X, Huang W, Li J, Zhou Y. Mater Sci Eng, 2003; A360: 18
[12] De Oliveira U, Ocelik V, De Hosson J T M. Surf Coat Technol, 2005; 197: 127
[13] Fallah V, Alimardani M, Corbin S F, Khajepour A. Comp Mater Sci, 2011; 50: 2124
[14] Zhu G X, Zhang A F, Li D C. Chin J Laser, 2010; (1): 296 (朱刚贤, 张安峰, 李涤尘. 中国激光, 2010; (1): 296)
[15] Kaplan A, Groboth G. J Manuf Sci Eng, 2001; 123: 609
[16] Aiyiti W, Zhao W, Lu B, Tang Y. Rapid Prototyping J, 2006; 12: 165
[17] Li Y, Ma J. Surf Coat Technol, 1997; 90: 1
[18] Song M, Lin X, Yang G, Cui X, Yang H, Huang W. J Mater Process Technol, 2014; 214: 701
[19] Bi G, Gasser A, Wissenbach K, Drenker A, Poprawe R. Surf Coat Technol, 2006; 201: 2676
[20] Tan H, Chen J, Zhang F, Lin X, Huang W. Int J Mach Tools Manuf, 2010; 50: 1
[21] Zhu G, Li D, Zhang A, Pi G, Tang Y. Opt Laser Technol, 2012; 44: 349
[22] Liu J, Li L. Opt Laser Technol, 2005; 37: 478
[23] Liu J. Opt Laser Technol, 2007; 39: 1532
[24] Tan H, Chen J, Zhang F, Lin X, Huang W. Opt Laser Technol, 2010; 42: 47
[25] Picasso M, Marsden C F, Wagniere J D, Frenk A, Rappaz M. Metall Mater Trans, 1994; 25B: 281
[26] Lin J, Hwang B C. Opt Laser Technol, 1999; 31: 571
[27] Tan H, Zhang F, Wen R, Chen J, Huang W. Opt Laser Eng, 2012; 50: 391
Outlines

/

〈 〉