EFFECT OF Hf, Sn, Ta, Zr, Dy AND Ho ON MICRO- STRUCTURE AND MECHANICAL PROPERTIES OF Nb-Nb5Si3 ALLOY

  • Jianting GUO ,
  • Lanzhang ZHOU ,
  • Yuxin TIAN ,
  • Jieshan HOU ,
  • Gusong LI
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Accepted date: 2015-01-29

  Online published: 2015-03-25

Abstract

This paper reviews the research works of effects of elements on the microstructure and mechanical properties of Nb-Si alloys conducted by the authors in recent years, including effect of Hf on Ni-16Si, Hf and Sn on Ni-20Ti-5Cr-3Al-18Si, Zr on Ni-22Ti-16Si, Ta on Nb-22Ti-16Si-7Cr-3Al, and rare earth elements Dy and Ho on Ni-23Ti-10Ta-2Cr-18Si and Ni-22Ti-16Si-7Cr-3Al-3Ta-2Hf, respectively. The addition of elements Hf, Zr, Sn+Hf, Ta, Dy and Ho in Nb-Si binary system and multi-component system enhances room and high temperature strength, plasticity and fracture toughness obviously. The enhancement of strength is related with the solution strengthening of elements, and the improvement of plasticity and ductility is related with the fining of microstructure and the increase of particles which exceed the critical size of (Nb, Ti)ss.

Cite this article

Jianting GUO , Lanzhang ZHOU , Yuxin TIAN , Jieshan HOU , Gusong LI . EFFECT OF Hf, Sn, Ta, Zr, Dy AND Ho ON MICRO- STRUCTURE AND MECHANICAL PROPERTIES OF Nb-Nb5Si3 ALLOY[J]. Acta Metall Sin, 2015 , 51(7) : 815 -827 . DOI: 10.11900/0412.1961.2014.00477

References

[1] Guo J T, Tian Y X, Sheng L Y, Zhou L Z, Ye H Q. Int J Mater Res, 2008; 99: 1
[2] Zelenitsas K, Tsakiropoulos P. Intermetallies, 2006; 14: 639
[3] Geng J, Tsakiropoulos P, Shao G. Intermetallics, 2006; 14: 227
[4] Ma C L, Li J G, Tan Y, Tanaka R, Hanada S. Mater Sci Eng, 2004; A386: 375
[5] Kim W Y, Yeo I D, Ra T Y, Cho G S, Kim M S. J Alloys Compd, 2004; 364: 186
[6] Jin-Hak K, Tatsuo T, Michiru S, Shuji H. Mater Sci Eng, 2004; A372: 137
[7] Kim W Y, Yeo I D, Kim M S, Hanada S. Mater Trans, 2002; 43: 3254
[8] Chan K S. Mater Sci Eng, 2002; A329-331: 531
[9] Bewlay B P, Lewandowski J J. J Mater, 1977; 60: 44
[10] Tian Y X, Guo J T, Zhou L Z, Cheng G M, Ye H Q. Mater Lett, 2008; 62: 2657
[11] Tian Y X, Guo J T, Sheng L Y, Cheng G M, Zhou L Z, He L L, Ye H Q. Intermetallics, 2008; 16: 807
[12] Tian Y X,Zhou L Z,Guo J T. In: High-Temperature Material Branch of The Chinese Society for Metals eds., The Power and The Energy Use High Temperature Structural Materials—11th Session of China High Temperature Alloy Annual Meeting Collection, Beijing: Metallurgical Industry Press, 2007: 602 (田玉新,周兰章,郭建亭. 见: 中国金属学会高温材料分会主编, 动力与能源用高温结构材料—第11届中国高温合金年会论文集, 北京: 冶金工业出版社, 2007: 602)
[13] Wu C L, Zhou L Z, Guo J T. Acta Metall Sin, 2006; 42: 1061 (伍春兰, 周兰章, 郭建亭. 金属学报, 2006; 42: 1061)
[14] Tian Y X, Guo J T, Zhou L Z, Li G S, Ye H Q. Acta Metall Sin, 2008; 44: 580 (田玉新, 郭建亭, 周兰章, 李谷松, 叶恒强. 金属学报, 2008; 44: 580)
[15] Tian Y X, Guo J T, Liang Y C, Wu C L, Zhou L Z, Ye H Q. Int J Mater Res, 2007; 98: 511
[16] Tian Y X, Guo J T, Cheng G M, Sheng L Y, Zhou L Z, He L L, Ye H Q. Int J Mater Res, 2008; 99: 2
[17] Tian Y X, Cheng G M, Guo J T, Zhou L Z, He L L, Ye H Q. Adv Eng Mater, 2007; 9: 936
[18] Tian Y X, Guo J T, Cheng G M, Sheng L Y, Zhou L Z, He L L, Ye H Q. Mater Des, 2009; 30: 2274
[19] Guo J T, Tian Y X, Cheng G M, Zhou L Z, He L L, Ye H Q. J Alloys Compd, 2009; 470: 606
[20] Cheng G M, Tian Y X, He L L, Guo J T. Philos Mag, 2009; 89: 2801
[21] Kim W Y, Tanaka H, Kasama A, Hanada S. Intemetallics, 2001; 9: 827
[22] Chan K S. Metall Mater Trans, 2001; 32A: 2475
[23] Kumar K S, Manna S K. Mater Res Symp Proc, 1989; 133: 415
[24] Massalski T B. Binary Alloy Phase Diagram. 2nd Ed., Materials Park, Ohio: The Materials Information Society, 1996: 2764, 2772
[25] Miura S, Aoki M, Saeki Y, Ohkubo K, Mishima Y, Mohri T. Metall Mater Trans, 2005; 36A: 489
Outlines

/

〈 〉