CORROSION MECHANISM DISCUSSION OF X65 STEEL IN NaCl SOLUTION SATURATED WITH SUPERCRITICAL CO2

  • Liang WEI ,
  • Xiaolu PANG ,
  • Kewei GAO
Expand
  • Department of Materials Physics and Chemistry, University of Science and Technology Beijing, Beijing 100083

Accepted date: 2015-03-16

  Online published: 2015-03-25

Supported by

Supported by National Natural Science Foundation of China (No.51271024) and Beijing Natural Science Foundation Major Project (No.2131004)

Abstract

In recent years, the corrosion problem of steels under supercritical CO2/H2O system in oil/gas production has got more and more attention. The temperature and pressure of some oil wells in China usually exceed 120 ℃ and 100 MPa, where CO2 is in supercritical state. To transportation easier and cost reduction, the oil/gas in pipelines is usually pressured to a high pressure, normally causes CO2 in supercritical state. The supercritical CO2 corrosion environment includes CO2-saturated water and H2O-saturated CO2 phases. Moreover, corrosive ions such as Cl- usually exists in CO2 corrosion environment, however the influence of Cl- on corrosion of carbon steel in supercritical CO2-saturated NaCl solution and NaCl solution-saturated supercritical CO2 are investigated limited. The corrosion behaviors and corrosion rates of X65 carbon steel exposed in supercritical CO2-saturated 3.5%NaCl solution, supercritical CO2-saturated deionized water and NaCl solution-saturated supercritical CO2 systems were investigated. SEM, EDS and XRD were used to analyze the morphology and characteristic of corrosion product scale on the steel surface. The results show that the addition of Cl- in supercritical CO2-satureated water significantly increased the corrosion rate of X65 steel, and modified the FeCO3 grain morphology. The average corrosion rate of X65 steel in NaCl solution-saturated supercritical CO2 was much lower than in supercritical CO2-saturated NaCl solution, but in supercritical CO2 phase X65 steel suffered serious localized corrosion. The corrosion process of X65 steel in supercritical CO2-saturated NaCl solution could be divided into three stages: the first was the active dissolution stage, the surface of X65 steel was corroded inhomogeneous due to the competitive adsorption between Cl- and H2CO3, HCO3-, and Fe3C as well as some lumpish matrix were residued on steel surface; the second was the initiation stage of FeCO3 precipitation, Cl- postponed the precipitation of FeCO3, the FeCO3 scale formed in this period was incomplete, and increased the area of cathodic reaction subsequently the corrosion rate; the last was the protective stage of FeCO3 corrosion scale, the corrosion product scale formed in this period was denser and provided better protectiveness to X65 steel matrix, however Cl- could pass this scale and reach the scale/matrix interface, resulted in the corrosion rate of X65 steel keeping at a higher value than in deionized water environment. The corrosion model of normal pipelines was developed to better understand the corrosion mechanism in supercritical CO2-saturated Cl--containing solution.

Cite this article

Liang WEI , Xiaolu PANG , Kewei GAO . CORROSION MECHANISM DISCUSSION OF X65 STEEL IN NaCl SOLUTION SATURATED WITH SUPERCRITICAL CO2[J]. Acta Metall Sin, 2015 , 51(6) : 701 -712 . DOI: 10.11900/0412.1961.2014.00491

References

[1] Gray L G S, Anderson B G, Danysh M J, Tremaine P G. Corrosion 1989, Houston: NACE, 1989: paper No.464
[2] Kermani M B, Morshed A. Corrosion, 2003; 59: 659
[3] Nesic S. Corros Sci, 2007; 49: 4308
[4] Nesic S, Postlethwaite J, Olsen S. Corrosion, 1996; 52: 280
[5] Choi Y S, Nesic S. Int J Greenhouse Gas Control, 2011; 5: 788
[6] Cui Z D, Wu S L, Zhu S L, Yang X J. Appl Surf Sci, 2006; 252: 2368
[7] Zhang Y C, Qu S P, Pang X L, Gao K W. Corros Prot, 2011; 32: 854 (张玉成, 屈少鹏, 庞晓露, 高克玮. 腐蚀与防护, 2011; 32: 854)
[8] Yevtushenko O, B?βler R. Corrosion 2014, Houston: NACE, 2014: paper No.3838
[9] Zhang Y C, Pang X L, Qu S P, Li X, Gao K W. Corros Sci, 2012; 59: 186
[10] Choi Y S, Magalhaes A A O, Farelas F, Andrade C D A, Nesic S. Corrosion 2013, Houston: NACE, 2013: paper No.2380
[11] Cui Z D, Wu S L, Li C F, Zhu S L, Yang X J. Mater Lett, 2004; 58: 1035
[12] Zhang Y C, Gao K W, Schmitt G. Corrosion 2011, Houston: NACE, 2011: paper No.11378
[13] Schremp F W, Roberson G R. Soc Pet Eng J, 1975; 15: 227
[14] Zhang Y C, Gao K W, Schmitt G. Mater Perform, 2011; 50: 62
[15] Yevtushenko O, Bettge F, Bohraus S, Baesslera R, Pfennig A, Kranzmann A. Process Saf Environ Prot, 2014; 92: 108
[16] Liu Q Y, Mao L J, Zhou S W. Corros Sci, 2014; 84: 165
[17] Chen C F, Lu M X, Zhao G X, Bai Z Q, Yan M L, Yang Y Q. Acta Metall Sin, 2003; 39: 848 (陈长风, 路民旭, 赵国仙, 白真权, 严密林, 杨延清. 金属学报, 2003; 39: 848)
[18] Schmitt G. Corrosion 1984, Houston: NACE, 1984: paper No.1
[19] Ikeda A, Mukai S, Uede M. Corrosion 1984, Houston: NACE, 1984; 1: 39
[20] Sun J B, Liu W, Yang L Y, Yang J W, Lu M X. Acta Metall Sin, 2008; 44: 991 (孙建波, 柳 伟, 杨丽颖, 杨建炜, 路民旭. 金属学报, 2008; 44: 991)
[21] Dugstad A. Corrosion 2006, Houston: NACE, 2006: paper No.06111
[22] Tanupabrungsun T, Brown B, Nesic S. Corrosion 2013: Houston: NACE, 2013: paper No.2348
[23] Dugstad A. Corrosion 1998, Houston: NACE, 1998: paper No.31
[24] Nesic S, Nordsveen M, Nyborg R, Stangeland A. Corrosion, 2003; 59: 489
[25] Sun W, Nesic S, Woollam R C. Corros Sci, 2009; 51: 1273
[26] Johnson M L, Tomson M B. Corrosion 1991, Houston: NACE, 1991: paper No.268
[27] Van Hunnik E W J, Pots B F M, Hendriksen E L J A. Corrosion 1996, Houston: NACE, 1996: paper No.6
[28] Hedayat A, Yannacopoulos S, Postlethwaite J. Corrosion, 1992; 48: 953
[29] Chen C F, Lu M X, Zhao G X, Bai Z Q, Yan M L, Yang Y Q. Acta Metall Sin, 2002; 38: 411 (陈长风, 路民旭, 赵国仙, 白真权, 严密林, 杨延清. 金属学报, 2002; 38: 411)
[30] Ramachandran S, Campbell S, Ward M B. Corrosion 2000, Houston: NACE, 2000: paper No.25
Outlines

/

〈 〉