MAGNETOCALORIC EFFECT OF La0.9Ce0.1Fe11.44Si1.56Hy ALLOY AND POWER BONDED BLOCK

  • Lijuan MU ,
  • Jiaohong HUANG ,
  • Cuilan LIU ,
  • Juan CHENG ,
  • Naikun SUN ,
  • Zengqi ZHAO
Expand
  • 1 School of Materials Science and Engineering, Inner Mongolia University of Technology, Hohhot 010051
    2 School of Mathematics, Physics and Biological Engineering, Inner Mongolia University of Science and Technology, Baotou 014010
    3 Baotou Research Institute of Rare Earth, Baotou 014030
    4 School of Science, Shenyang Ligong University, Shenyang 110159

Received date: 2015-01-15

  Accepted date: 2015-01-15

  Online published: 2015-03-16

Supported by

Supported by National Natural Science Foundation of China (No.51261001) and Liaoning Provincial Natural Science Foundation (No.2013020105)

Abstract

Recently, La(Fe, Si)13-based magnetic refrigeration materials have been widely explored due to the advantages of giant magnetocaloric effect (MCE), tunable Curie temperature (TC), low cost of raw materials and excluding deleterious elements compared to other room-temperature giant MCE materials such as Gd5(Ge1-xSix)4, MnFeP0.45As0.55 and MnAs based compounds. In this work, in order to shift the TC to around room temperature and maintain the large MCE, the method of absorbing hydrogen was employed. La0.9Ce0.1Fe11.44Si1.56 hydride was prepared by saturated hydrogen absorption and then hydrogen contents and TC of the hydrides were controlled by subsequent dehydrogenation at different temperatures (Td=200~250 ℃ for 3 h). The phase structure and magnetocaloric effect were investigated. The results show that the samples possess the cubic NaZn13-type structure with a small amount of a-Fe as impurity phase. TC exhibits an approximately linear decrease with increasing the dehydrogenation temperature. The isothermal magnetic entropy change (ΔSm) of the hydrides decreases compared with the parent compound, which is mainly attributed to the fact that the field-induced itinerant-electron metamagnetic transition has been weakened upon hydrogen absorption. For the sample desorbed hydrogen at temperatures above 230 ℃, ΔSm is remarkably decreased and favorably the magnetic hysteresis loss has been reduced simultaneously. With further increasing the temperature to 250 ℃, ΔSm curve is broadened, weakening the characteristic of the first-order phase transition. Due to the intrinsic brittleness of hydrides, the preparation of a certain shape is of great importance for practical application. For a magnetic field change of 1.5 T, the maximum adiabatic temperature change (ΔTad) and ΔSm for the bonded block of fully hydrogen absorption La0.9Ce0.1Fe11.44Si1.56 hydride are about 2.7 K and 7.5 J/(kgK), respectively, which are larger than those of La(Fe, Co, Si)13 materials in the same magnetic field change range. In conclusion, the bonded La0.9Ce0.1Fe11.44Si1.56 hydrides with good MCE and different TC have been successfully prepared and will be very useful for the practical application of layered magnetic refrigerants at ambient temperature under low field change in magnetic refrigerators.

Cite this article

Lijuan MU , Jiaohong HUANG , Cuilan LIU , Juan CHENG , Naikun SUN , Zengqi ZHAO . MAGNETOCALORIC EFFECT OF La0.9Ce0.1Fe11.44Si1.56Hy ALLOY AND POWER BONDED BLOCK[J]. Acta Metall Sin, 2015 , 51(6) : 762 -768 . DOI: 10.11900/0412.1961.2014.00473

References

[1] Pecharsky V K, Gschneidner Jr K A. Phys Rev Lett, 1997; 78: 4494
[2] Hu F X, Shen B G, Sun J R, Cheng Z H, Rao G H, Zhang X X. Appl Phys Lett, 2001; 78: 3675
[3] Fujieda S, Fujita A, Fukamichi K. Appl Phys Lett, 2002; 81: 1276
[4] Tegus O, Brück E, Buschow K H J, de Boer F R. Nature, 2002; 415: 150
[5] Zhang M, Liu D M, Liu C X, Huang Q Z, Wang S B, Zhang H, Yue M. Acta Metall Sin, 2013; 49: 783 (张孟, 刘丹敏, 刘翠秀, 黄清镇, 王少博, 张虎, 岳明. 金属学报, 2013; 49: 783)
[6] Dung N H, Ou Z Q, Caron L, Zhang L, Cam Thanh D T, de Wijs G A, de Groot R A, Buschow K H J, Brück E. Adv Energy Mater, 2011; 1: 1215
[7] Krenke T, Duman E, Acet M, Wassermann E F, Moya X, Manosa L, Planes A. Nat Mater, 2005; 4: 450
[8] Shen J, Li Y X, Sun J R, Shen B G. Chin Phys, 2009; 18B: 2058
[9] Balli M, Fruchart D, Gignoux D. J Phys: Condens Matter, 2007; 19: 236230
[10] Cheng J, Liu G D, Huang J H, Liu C L, Jin P Y, Yan H W. J Rare Earths, 2013; 31: 1163
[11] Li F A, Song L, Bao L H, Hasi C L, Tegus O, Huang J H. Acta Metall Sin, 2008; 44: 371 (李福安, 松 林, 包黎红, 哈斯朝鲁, 特古斯, 黄焦宏. 金属学报, 2008; 44: 371)
[12] Chen Y F, Wang F, Shen B G, Hu F X, Cheng Z H, Wang G J, Sun J R. Chin Phys, 2002; 11: 741
[13] Fujita A, Fujieda S, Fukamichi K, Yamazaki Y, Iijima Y. Mater Trans, 2002; 43: 1202
[14] Fujita A, Fukamichi K. J Alloys Compd, 2005; 404: 554
[15] Barcza A, Katter M, Zellmann V, Russek S, Jacobs S, Zimm C. IEEE Trans Magn, 2011; 47: 3391
[16] Krautz M, Moore J D, Skokov K P, Liu J, Teixeira C S, Schafer R, Schultz L, Gutfleisch O. J Appl Phys, 2012; 112: 083918
[17] Zimm C, Jacobs S. J Appl Phys, 2013; 113: 17A908
[18] Legait U, Guillou F, Kedous-Lebouc A, Hardy V, Almanza M. Int J Refrigeration, 2014; 37: 147
[19] Balli M, Sari O, Mahmed C, Besson C, Bonhote P, Duc D, Forchelet J. In: Egolf P W, ed., 4th IIF-IIR Int Conf on Magnetic Refrigeration at Room Temperature, Paris: Institute of Refrigeraton and Institut International du Froid of France, 2010: 313
[20] Tusek J, Kitanovski A, Tomc U, Favero C, Poredos A. Int J Refrigeration, 2014; 37: 117
[21] Zhang H, Shen B G, Xu Z Y, Zheng X Q, Shen J, Hu F X, Sun J R, Long Y. J Appl Phys, 2012; 111: 07A909
[22] Chen Y F, Wang F, Shen B G, Wang G J, Sun J R. J Appl Phys, 2003; 93: 1323
[23] Yamada H. Phys Rev, 1993; 47B: 11211
[24] Huang J H, Sun N K, Liu C L, Ge Y M, Zhang T, Liu F, Si P Z. Acta Metall Sin (Engl Lett), 2014; 27: 27
[25] Chen X, Chen Y G, Tang Y B. J Alloys Compd, 2011; 509: 2864
[26] Pathak A K, Basnyat P, Dubenko I, Stadler S, Ali N. J Appl Phys, 2009; 106: 063917
[27] Balli M, Fruchart D, Sari O, Gignoux D, Huang J H, Hu J, Egolf P W. J Appl Phys, 2009; 106: 023902
Outlines

/

〈 〉