EFFECT OF INTERLAYERS ON THE MICROSTRUC-TURE AND SHEAR STRENGTH OF ALUMINA CERAMIC AND 1Cr18Ni9Ti STAINLESS STEEL BRAZED BONDING
Received date: 2014-06-27
Revised date: 2014-11-03
Online published: 2015-07-23
Supported by
Supported by Applied Basic Research Project of Yunnan Province (No.2010ZC56)
In recent years, there have been great efforts focused on joining ceramics to metals to establish processes for a wide range of industrial uses. Several important problems, however, still remain unsolved. Among them, how to produce atomic bonds at ceramic/metal interfaces and how to minimize the residual stress due to large thermal expansion mismatch between two constituents are the most critical. The thermal expansion mismatch effect is a serious problem because, even if a strong interface could be achieved, joints with large residual stress are easily broken. Therefore, it is desirable to reduce the magnitude of the residual stress. Some researchers have succeeded in achieving a strong joint between alumina and stainless steel by using a soft metallic interlayer. In this study, the effects of interlayers of nickel, copper and copper coated with nickel on the microstructure and shear strength of alumina ceramic and 1Cr18Ni9Ti stainless steel bonding with Ag-Cu-Ti filler metal were investigated. The results indicated that, when using copper as an interlayer, sufficient interfacial reaction between the ceramic and the filler metal could obtain. However, when using nickel as an interlayer, resulting in an insufficient reaction between the ceramic and the filler metal and the formation of large amount Ni3Ti intermetallic compounds, and thus, the strength of the joint decreased heavily. It is very interesting that when using copper coated with Ni, the existence of the small amount of nickel didn't affect the activity of titanium in the filler metal, meanwhile, it decreased the effect of the filler metal on the solubility of copper. Compared with copper and Ni interlayer, this interlayer could reduce interfacial residual stress more effectively. And the shear strength of 109 MPa was obtained when the thickness of Cu was 0.2 mm coated with 30 μm thick nickel。
Yi LIU , Guofeng JIANG , Kun XU , Ximing LUO , Dengquan CHEN , Wei LI . EFFECT OF INTERLAYERS ON THE MICROSTRUC-TURE AND SHEAR STRENGTH OF ALUMINA CERAMIC AND 1Cr18Ni9Ti STAINLESS STEEL BRAZED BONDING[J]. Acta Metall Sin, 2015 , 51(2) : 209 -215 . DOI: 10.11900/0412.1961.2014.00343
| [1] | Nicholas M G. Joining of Ceramics. London: Chapman and Hall Ltd, 1990: 1 |
| [2] | Schwartz M M. Ceramic Joining. Material park, Ohio: ASM International, 1990: 1 |
| [3] | Park J W, Mendez P F, Eagar T W. Acta Mater, 2002; 50: 883 |
| [4] | Zhang J X, Chandel R S, Chen Y Z, Seow H P. J Mater Process Technol, 2002; 122: 220 |
| [5] | Li Z R, Fan J X, Feng J C. Aerosp Mater Technol, 2008; (4): 6 |
| [5] | (李卓然, 樊建新, 冯吉才. 宇航材料工艺, 2008; (4): 6) |
| [6] | Xian A P, Si C Y. J Mater Sci, 1992; 27: 1560 |
| [7] | Huang X L, Lin S, Xiao J M. Trans China Weld Inst, 1998; 19: 216 |
| [7] | (黄小丽, 林 实, 肖纪美. 焊接学报, 1998; 19: 216) |
| [8] | Huang X L, Lin S, Xiao J M, Chu J X. Mater Sci Eng, 1996; 14(3): 58 |
| [8] | (黄小丽, 林 实, 肖纪美, 楚建新. 材料科学与工程, 1996; 14(3): 58) |
| [9] | Zou G S, Ren J L, Wu A P, Peng Z S, Zeng W J. Mater Rev, 1999; 13(2): 16 |
| [9] | (邹贵生, 任家烈, 吴爱萍, 彭真山, 曾文军. 材料导报, 1999; 13(2): 16) |
| [10] | Xian A P, Si C Y. Acta Metall Sin, 1991; 27: 421 |
| [10] | (冼爱平, 斯重遥. 金属学报, 1991; 27: 421) |
| [11] | Zhou Y, Bao F H, Ren J L, North T H. Mater Sci Technol, 1991; 7: 863 |
| [12] | Wang Y, He P, Feng J C, Zhang L X, Gu X L, Wang D Y. Trans Chin Weld Inst, 2007; 28(4): 13 |
| [12] | (王 颖, 何 鹏, 冯吉才,?张丽霞, ?顾小龙,?王大勇. 焊接学报, 2007; 28(4): 13) |
| [13] | Suganuma K, Okamoto T, Koizumi M, Kamachi K. J Mater Sci,1987; 22: 3561 |
| [14] | Suganuma K. J Mater Sci, 1991; 26: 6144 |
| [15] | Zhu M U, Chung D D L. J Mater Sci, 1997; 32: 5321 |
| [16] | Shirzadi A A, Zhu Y, Bhadeshia H K D H. Mater Sci Eng, 2008; A496: 501 |
| [17] | Tang Q, Chu J X, Zhang X Y. Electros Proc Technol, 2001; 22: 166 |
| [17] | (唐 群, 楚建新, 张晓勇. 电子工艺技术, 2001; 22: 166) |
| [18] | Hao H Q, Wang Y L, Jin Z H, Wang X T. J Mater Sci, 1995; 30: 4107 |
| [19] | Zou X. Brazing. Beijing: China Machine Press, 1997: 392 |
| [19] | (邹 僖. 钎焊. 北京: 机械工业出版社, 1997: 392) |
| [20] | Valette C, Devismes M F, Voytovych R, Eustathopoulos N. Scr Mater, 2005; 52: 1 |
| [21] | Arróyave R, Eagar T W. Acta Mater, 2003; 51: 4871 |
| [22] | Jocelyn L W. Master Thesis, Massachusetts Institute of Technology, Cambridge, USA, 2001 |
| [23] | Torvund T, Grong ?, Akselsen O M, Ulvens?en J H. J Mater Sci, 1997; 32: 4437 |
| [24] | Zhu D Y, Wang Y L, Jin Z H. Ordnance Mater Sci Eng, 1998; 21(20): 22 |
| [24] | (朱定一, 王永兰, 金志浩. 兵器材料科学与工程, 1998; 21(20): 22) |
| [25] | Wang X Y, Li Y, Wei S Z, Xu L J, Ma X D. New Technol New Proc, 2010; (5): 85 |
| [25] | (王新阳, 李 炎, 魏世忠, 徐流杰, 马向东. 新技术新工艺, 2010; (5): 85) |
| [26] | Li Z R, Fan J X, Feng J C. J Mater Eng, 2008; (9): 1 |
| [26] | (李卓然, 樊建新, 冯吉才. 材料工程, 2008; (9): 1) |
/
| 〈 |
|
〉 |