ANALYSIS OF SURFACE OXIDE FILM FORMED ON ELETROPOLISHED ALLOY 690TT IN HIGH TEMPERATURE AND HIGH PRESSURE WATER WITH SEQUENTIALLY DISSOLVED HYDROGEN AND OXYGEN

  • Zhiming ZHANG ,
  • Jianqiu WANG ,
  • En-Hou HAN ,
  • Wei KE
Expand
  • 1 Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
    2 Liaoning Key Laboratory for Safety and Assessment Technique of Nuclear Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Revised date: 2014-07-01

  Online published: 2015-01-25

Supported by

Supported by National Basic Research Program of China (No.2011CB610502), National Science and Technology Major Project (No.2011ZX06004-009) and National Natural Science Foundation of China (No.51025104)

Abstract

The electropolished (EP) alloy 690TT samples were first oxidized in the simulated B and Li containing primary water with 2.5 mg/L H2 at 325 ℃ and 15.6 MPa for 720 h, and then half of the samples were continuously immersed in this solution with 2.0 mg/L O2 for another 720 h. The microstructures and chemical composition of the oxide films formed under the above two conditions were analyzed. The results show that the dual layered oxide film formed under the single hydrogen water chemistry is mainly composed of spinel oxides. The outer layer is composed of big oxide particles rich in Ni and Fe and the underlying loose needle-like oxides rich in Ni. The inner layer is continuous Cr-rich oxides. The oxide film formed on EP alloy 690TT under the hydrogen/oxygen water chemistry also shows a dual layered structure. The surface morphology and chemical composition of the outer layer are similar to the oxide film formed under the hydrogen water chemistry. However, the inner layer is changed to the nano-sized NiO. The stable phase region in the potential-pH diagram for the Ni oxides is enlarged by the later dissolved oxygen. As a result, the oxygen promotes the fast growth of the outer needle-like oxides rich in Ni. Further, the oxygen promotes the dissolution of the inner Cr-rich oxides formed under the hydrogen water chemistry and increases the corrosion rate of the EP alloy 690TT. Electropolishing treatment can not reduce the corrosion rate of alloy 690TT in the simulated primary water with sequentially dissolved hydrogen and oxygen.

Cite this article

Zhiming ZHANG , Jianqiu WANG , En-Hou HAN , Wei KE . ANALYSIS OF SURFACE OXIDE FILM FORMED ON ELETROPOLISHED ALLOY 690TT IN HIGH TEMPERATURE AND HIGH PRESSURE WATER WITH SEQUENTIALLY DISSOLVED HYDROGEN AND OXYGEN[J]. Acta Metall Sin, 2015 , 51(1) : 85 -92 . DOI: 10.11900/0412.1961.2014.00351

References

[1] Dutaa R S. J Nucl Mater, 2009; 393: 343
[2] Li Y C,Zhu Z P,Yang D W,Li J Y,et al.Control of Water Chemistry in Nuclear Power Plants. Beijing: Chemical Industry Press, 2008: 66
[2] (李宇春,朱志平,杨道武,李敬业等. 核电站水化学控制工况. 北京: 化学工业出版社, 2008: 66)
[3] Yu G P, Yao H C. Corrosion, 1990; 46: 391
[4] Ziemniak S E, Hanson M, Sander P C. Corros Sci, 2008; 50: 2465
[5] Zhang Z M, Wang J Q, Han E H, Ke W. Acta Metall Sin, 2011; 47: 831
[5] (张志明, 王俭秋, 韩恩厚, 柯 伟. 金属学报, 2011; 47: 831)
[6] Zhang Z M, Wang J Q, Han E H, Ke W. Acta Metall Sin, 2011; 47: 823
[6] (张志明, 王俭秋, 韩恩厚, 柯 伟. 金属学报, 2011; 47: 823)
[7] Zhang Z M, Wang J Q, Han E H, Ke W. J Mater Sci Technol, 2012; 28: 353
[8] Yun G C,Cheng X Z. Water Chemistry of Pressured Water Reactors. Harbin: Harbin Engineering University Press, 2009: 52
[8] (云桂春,成徐州. 压水反应堆水化学. 哈尔滨: 哈尔滨工程大学出版社, 2009: 52)
[9] Dan T C, Shoji T, Lu Z P, Sakaguchi K, Wang J Q, Han E H, Ke W. Corros Sci, 2010; 52: 1228
[10] Zhang Z M, Wang J Q, Han E H, Ke W. Corros Sci, 2011; 53: 3623
[11] Zhang Z M, Wang J Q, Han E H, Ke W. In: Peng Q J ed., Proc 3rd Int Symp on Materials and Reliability in Nuclear Power Plants, Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2013: 25
[12] Zhang Z M, Wang J Q, Han E H, Ke W. J Mater Sci Technol, 2014; DOI: 10.1016/j.jmst.2014.09.002
[13] Sennour M, Marchetti L, Martin F, Perrin S, Molins R, Pijolat M. J Nucl Mater, 2010; 402: 147
[14] Marchetti L, Perrin S, Raquet O, Pijolat M. Mater Sci Forum, 2008; 595-598: 529
[15] Lefaix-Jeuland H, Marchetti L, Perrin S, Pijolat M, Sennour M, Molins R. Corros Sci, 2011; 53: 3914
[16] Ziemniak S E, Hanson M. Corros Sci, 2006; 48: 498
[17] Terachi T, Totsuka N, Yamada T, Nakagawa T, Deguchi H, Horiuchi M, Oshitani M. J Nucl Sci Technol, 2003; 40: 509
[18] Staehle R W, Gorman J A. Corrosion, 2003; 59: 931
[19] Liu X H, Wu X Q, Han E H. Corros Sci, 2011; 53: 3337
[20] Kim Y J. Corrosion, 2000; 56: 389
[21] Li M S. High Temperature Corrosion of Metals. Beijing: Metallurgical Industry Press, 2001: 162
[21] (李美栓. 金属的高温腐蚀. 北京: 机械工业出版社, 2001: 162)
[22] Rebak R B, Smialowska Z S. Corros Sci, 1996; 38: 971
Outlines

/

〈 〉