EFFECTS OF (W+Mo)/Cr RATIO ON MICROSTRUC-TURAL EVOLUTIONS AND MECHANICAL PROPER-TIES OF CAST Ni-BASED SUPERALLOYS DURING LONG-TERM THERMAL EXPOSURE

  • Wen SUN ,
  • Xuezhi QIN ,
  • Jianting GUO ,
  • Langhong LOU ,
  • Lanzhang ZHOU
Expand
  • 1 University of Science and Technology of China, Hefei 230022
    2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Revised date: 2014-05-26

  Online published: 2015-01-25

Supported by

Supported by National Natural Science Foundation of China (No.51001101) and High Technology Research and Development Program of China (No.2012AA03A501)

Abstract

The Ni-based superalloys are widely used as microstructural components of modern turbine engines due to its good high temperature strength, good fatigue and creep property and excellent hot-corrosion resistance. In order to increase their high temperature strength, more and more refractory elements, such as W and Mo, are added into these alloys while Cr content gradually decreases. During long-term aging, these alloys generally experience various microstructural changes, including coarsening of g' phase coarsening, formation of a continuous grain boundary (GB) carbide network, precipitation topologically close-packed (TCP) phase, and degeneration of MC carbide. However, there is limited available data about the effect of (W+Mo)/Cr ratios on the microstructural evolution of Ni-based superalloys. In this work, the cast Ni-based superalloys with different (W+Mo)/Cr ratios (mass ratios) are fabricated by vacuum induction furnace. After standard heat treated (1110 ℃, 4.5 h, air cooling+750 ℃, 10.5 h, air cooling), they are thermally exposed at 850 ℃ for different times. The stress-rupture tests are operated under the condition of 800 ℃, 294 MPa. Effects of (W+Mo)/Cr ratios on the microstructure evolutions and mechanical properties are investigated by the combination of OM, SEM, TEM and stress-rupture tests. The experiment results show that the (W+Mo)/Cr ratio has no obvious influence on the standard heat treated microstructure, which is mainly composed of g matrix, g' phase, MC carbide and secondary carbides distributing at grain boundaries. During long-term thermal exposure, the microstructure evolutions occur by g' phase coarsening, TCP phases formation, MC degeneration and grain boundary coarsening. The g' phase coarsening behavior is not affected obviously by the (W+Mo)/Cr ratio. However, the amount of TCP phases decreases significantly with decreasing of (W+Mo)/Cr ratio and the type of TCP phases transforms from m phase to coexist of m and s phases when (W+Mo)/Cr ratio decreases from 0.55 to 0.37. There are no TCP phases observed in the sample with (W+Mo)/Cr ratio of 0.22. The thermal stability of MC carbide is reduced obviously and the grain boundaries coarsen more severely by the decrease of (W+Mo)/Cr ratio. The degradation of stress-rupture property is attributed to the coarsening of g' phase and grain boundaries and the formation of TCP phases. Combined with the effect of (W+Mo)/Cr ratio on the solid solution strengthening, microstructure evolution and stress-rupture property, it can be concluded that the optimum stress-rupture property can be obtained when the (W+Mo)/Cr ratio is about 0.37.

Cite this article

Wen SUN , Xuezhi QIN , Jianting GUO , Langhong LOU , Lanzhang ZHOU . EFFECTS OF (W+Mo)/Cr RATIO ON MICROSTRUC-TURAL EVOLUTIONS AND MECHANICAL PROPER-TIES OF CAST Ni-BASED SUPERALLOYS DURING LONG-TERM THERMAL EXPOSURE[J]. Acta Metall Sin, 2015 , 51(1) : 67 -76 . DOI: 10.11900/0412.1961.2014.00281

References

[1] Guo J T. Materials Science and Engineering for Superalloys. Vol.1Beijing,: Science Press, 2008: 39
[1] (郭建亭.高温合金材料学(上册). 北京: 科学出版社, 2008: 39)
[2] Cai Y L, Zheng Y R. Acta Metall Sin, 1982; 18: 30
[2] (蔡榆林, 郑运荣. 金属学报, 1982; 18: 30)
[3] Ross E W, Sims C T. In: Sims C T, Stoloff N S, Hagel W C eds., Superalloys II, New York: Wiley, 1987: 97
[4] Pollock T M. Mater Sci Eng, 1999; B32: 255
[5] Giamei A F, Anton D L. Metall Trans, 1985; 16A: 1997
[6] Rae C M F, Karunaratne M S A, Small C J, Broomfiels C N, Jones C N, Reed R C. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, Mclean M, Olson S, Schirra J J eds., Superalloys 2000, Warrendale: TMS, 2000: 767
[7] Koul A K, Castillo R. Metall Trans, 1988; 19A: 2049
[8] Qin X Z, Guo J T, Yuan C, Chen C L, Ye H Q. Metall Mater Trans, 2007; 38A: 3014
[9] Qin X Z, Guo J T, Yuan C, Hou J S, Ye H Q. Mater Lett, 2008; 62: 258
[10] Qin X Z, Guo J T, Yuan C, Hou J S, Ye H Q. Mater Lett, 2008; 62: 2275
[11] Qin X Z, Guo J T, Yuan C, Yang G X, Zhou L Z, Ye H Q. J Mater Sci, 2009; 44: 4840
[12] Stevens R A, Flewitt P E J. Mater Sci Eng, 1979; A37: 237
[13] Lifshitz I M, Slyozov V V. J Phys Chem Solids, 1961; 19: 35
[14] Wanger C Z. Elektrochem, 1961; 65: 581
[15] Swalin R A, Martin A. J Met, 1956; 206: 567
[16] Van Der Molten F H, Oblak J M, Kriege O H. Metall Trans, 1971; 2: 1627
[17] Lvov G, Levit V I, Kaufman M J. Metall Mater Trans, 2004; 35A: 1669
[18] Wang J, Zhou L Z, Qin X Z, Sheng L Y, Hou J S, Guo J T. Mater Sci Eng, 2012; A533: 14
[19] Qin X Z, Guo J T, Yuan C, Yang G X, Zhou L Z, Ye H Q. Mater Sci Eng, 2008; A485: 74
[20] Sun W, Qin X Z, Guo Y A, Guo J T, Zhou L Z, Lou L H. Acta Metall Sin, 2014; 50: 744
[20] (孙 文, 秦学智, 郭永安, 郭建亭, 周兰章, 楼琅洪.金属学报, 2014; 50: 744)
[21] Liu L R, Jin T, Zhao N R, Sun X F, Guan H R, Hu Z Q. Mater Sci Eng, 2003; A361:191
[22] Chen Q Z, Knowles D M. Metall Trans, 2002; 33A: 1319
[23] Pessah M, Caron P, Khan T. In: Antolovich S D, Stusrud R W, MacKay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds., Superalloys 1992, Warrendale: TMS, 1992,567
[24] Pessah-Simonetti M, Caron P, Khan T. Mater Sci Eng, 1998; A254: 1
Outlines

/