SERRATED YIELDING OF 5456 ALUMINIUM MAGNE- SIUM ALLOY BASED ON THREE DIMENSIONAL DIGITAL IMAGE CORRELATION
Revised date: 2014-05-09
Online published: 2014-12-25
Supported by
Supported by National Natural Science Foundation of China (Nos.11332010, 51271174 and 11372300) and Fundamental Research Funds for the Central Universities (No.WK2090050029)
One of the key issues to deeply understand the intrinsic mechanism of Portevin-Le Chatelier (PLC) phenomenon is to analyze the spatial distribution and the evolution of the deformation in PLC bands, associated with serrated yielding. In this work, an investigation was carried out with 5456 aluminium magnesium alloy sheet specimens of different thicknesses at room temperature by using three dimensional digital image correlation (3D-DIC) method, which focused itself on the deformation analysis within serrated yielding under different loading procedures. After statistically analyzing loading curves, it is found that the average amplitude and average period increase with increasing strain. Moreover, there is a positive correlation between the average period and the thickness of specimen, while the average amplitude and the thickness of specimen are independent to some degree. In addition, the experimental result also indicates that the width of the PLC band increases with increasing thickness of the specimen. However, the spatial analysis in PLC bands proves that the angle between the PLC band and the tensile direction is about 60°, which is irrelevant to the specimen thickness and the serration amplitude. Furthermore, it is also found that PLC bands of out-of-plane displacement coincide with bands of strain in the tensile direction by temporal analysis. Most importantly, the experimental result shows that the serration amplitude is proportional to the maximum strain in PLC band when PLC band occurs.
Yulong CAI , Shihua FU , Yuhui WANG , Chenggang TIAN , Yue GAO , Teng CHENG , Qingchuan ZHANG . SERRATED YIELDING OF 5456 ALUMINIUM MAGNE- SIUM ALLOY BASED ON THREE DIMENSIONAL DIGITAL IMAGE CORRELATION[J]. Acta Metall Sin, 2014 , 50(12) : 1491 -1497 . DOI: 10.11900/0412.1961.2014.00251
| [1] | Cottrell A H. Philos Mag, 1953; 44: 829 |
| [2] | Cieslar M, Fressengeas C, Karimi A, Martin J L. Scr Mater, 2003; 48: 1105 |
| [3] | Nagarjuna S, Anozie F N, Evans J T. Mater Sci Technol, 2003; 19: 1661 |
| [4] | Lu J Y, Jiang Z Y, Zhang Q C. Acta Metall Sin, 2006; 42: 139 |
| [4] | (卢俊勇, 蒋震宇, 张青川. 金属学报, 2006; 42: 139) |
| [5] | Sleeswyk A W. Acta Metall, 1958; 6: 598 |
| [6] | Mulford R A, Kocks U F. Acta Metall, 1979; 27: 1125 |
| [7] | McCormick P G. Acta Metall, 1988; 36: 3061 |
| [8] | Springer F, Nortmann A, Schwink C. Phys Status Solidi, 1998; 170A: 63 |
| [9] | Klose F B, Ziegenbein A, Weidenmuller J, Neuhauser H, Hahner P. Comput Mater Sci, 2003; 26: 80 |
| [10] | Wang C, Xu Y B, Han E-H. Acta Metall Sin, 2006; 42: 191 |
| [10] | (王 聪, 徐永波, 韩恩厚. 金属学报, 2006; 42: 191) |
| [11] | Gupta C, Chakravartty J K, Wadekar S L, Dubey J S. Mater Sci Eng, 2000; A292: 49 |
| [12] | Gerland M, Mendez J, Lepinoux J, Violan P. Mater Sci Eng, 1993; A164: 226 |
| [13] | Cui C Y, Gu Y F, Yuan Y, Harada H. Scr Mater, 2011; 64: 502 |
| [14] | Fu S F, Cheng T, Zhang Q C, Hu Q, Cao P T. Acta Mater, 2012; 60: 6650 |
| [15] | Han G M,?Cui C Y,?Gu Y F,?Hu Z Q,?Sun X F. Acta Metall Sin, 2013; 49: 1243 |
| [15] | (韩国明, 崔传勇, 谷月峰, 胡壮麒, 孙晓峰. 金属学报, 2013; 49: 1243) |
| [16] | Chihab K, Estrin Y, Kubin L, Vergnol P J. Scr Mater, 1987; 21: 203 |
| [17] | Ziegenbein A, Hahner P, Neuhauser H. Comput Mater Sci, 2000; 19: 27 |
| [18] | Zhang Q C, Jiang Z Y, Jiang H F, Chen Z J, Wu X P. Int J Plasticity, 2005; 21: 2150 |
| [19] | Jiang H F, Zhang Q C, Jiang Z Y, Chen Z J, Wu X P. Chin Phys Lett, 2005; 22: 99 |
| [20] | Gao Y, Fu S H, Cai Y L, Cheng T, Zhang Q C. Acta Phys Sin, 2014; 63: 066201 |
| [20] | (高 越, 符师桦, 蔡玉龙, 程 腾, 张青川. 物理学报, 2014; 63: 066201) |
| [21] | Ranc N, Wagner D. Mater Sci Eng, 2008; A474: 188 |
| [22] | Ait-Amokhtar H, Fressengeas C, Boudrahema S. Mater Sci Eng, 2008; A488: 540 |
| [23] | Pan B, Li K, Tong W. Experiment Mech, 2013; 53: 1277 |
| [24] | Kang Y L, Zhang Z F, Wang H W, Qin Q H. Mater Sci Eng, 2005; A394: 312 |
| [25] | Guo B Q, Wang H X, Xie H M, Chen P W. Theory Appl Mech Lett, 2014; 4: 021010 |
| [26] | Jiang Z Y, Zhang Q C, Jiang H F, Chen Z J, Wu X P. Mater Sci Eng, 2005; A403: 154 |
| [27] | Xiang G F, Zhang Q C, Liu H W, Jiang H F, Wu X P. Chin Phys Lett, 2006; 15: 2378 |
| [28] | Lebedkina T A, Lebyodkin M A. Acta Mater, 2008; 56: 5567 |
/
| 〈 |
|
〉 |