EFFECTS OF TEMPERING ON THE MICROSTRUC-TURE AND MECHANICAL PROPERTY OF ELECTRON BEAM WELDING JOINT OF 9Cr2WVTa STEEL

  • Heng GAO ,
  • Yuanyuan SONG ,
  • Mingjiu ZHAO ,
  • Xiaofeng HU ,
  • Lijian RONG
Expand
  • Key Laborotary of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Revised date: 2014-06-23

  Online published: 2014-12-25

Supported by

Supported by National Natural Science Foundation of China (No.91226204) and Strategic Priority Program of the Chinese Academy of Sciences (No.XDA03010304)

Abstract

9Cr2WVTa steel is one kind of reduced activation ferritic/martensitic (RAFM) steels which exhibit lower thermal expansion coefficient, higher thermal conductivity and less irradiation swelling compared with austenitic steel. It has been considered as the candidate structural material for the accelerator driven subcritical system (ADS). Due to the narrow heat affected zone and large depth to width ratio, electron beam (EB) welding is expected as a potential technique to connect components of ADS. However, few previous studies have focused on the weldability of 9Cr2WVTa steel by EB welding. In this work, EB welding was applied to join the 9Cr2WVTa steel and tempering was used to modify the microstructure and mechanical properties of the weld joint. Microstructure analysis shows that the weld metal consists of coarse lath martensite and d-ferrite. After high temperature tempering, large amounts of M23C6 type carbides precipitate in the matrix. Tempering lowers the hardness of the weld metal. Tensile tests show that the strength of the weld joint decreases, but the total elongation increases after tempering. It was found that the accurate impact energy of the weld metal was not able to be measured with standard Charpy impact specimen due to the crack deviation from the weld metal to the base metal. In order to estimate the impact property of the weld metal accurately, Charpy V-notch specimens with side-grooves were used. The result shows that tempering induces a significant improvement of the impact energy to the weld metal compared with the as-welded condition. Furthermore, the weld metal demonstrates better impact property than the base metal, which results from the existence of low fraction of d-ferrite in the weld metal.

Cite this article

Heng GAO , Yuanyuan SONG , Mingjiu ZHAO , Xiaofeng HU , Lijian RONG . EFFECTS OF TEMPERING ON THE MICROSTRUC-TURE AND MECHANICAL PROPERTY OF ELECTRON BEAM WELDING JOINT OF 9Cr2WVTa STEEL[J]. Acta Metall Sin, 2014 , 50(12) : 1429 -1436 . DOI: 10.11900/0412.1961.2014.00333

References

[1] Shiba K, Enoeda M, Jitsukawa S. J Nucl Mater, 2004; 329-333: 243
[2] Yang C G, Yan W, Wang W, Shan Y Y, Yang K. Acta Metall Sin, 2011; 47: 917
[2] (杨春光, 严 伟, 王 威, 单以银, 杨 柯. 金属学报, 2011; 47: 917)
[3] Yvon P, Carre F. J Nucl Mater, 2009; 385: 217
[4] Klimiankou M, Lindau R, Moslang A. Micron, 2005; 36: 1
[5] Klueh R L. Int Mater Rev, 2005; 50: 287
[6] Kohyama A. Mater Trans, 2005; 46: 384
[7] Kurtz R J, Abe K, Chernov V M, Hoelzer D T, Matsui H. J Nucl Mater, 2004; 329-333: 47
[8] Pilloni L, Attura F, Calza-Bini A, De Santis G, Filacchioni G, Carosi A, Amato S. J Nucl Mater, 1998; 258-263: 1329
[9] Jiang Z Z, Huang J H, Chen S H, Ju X. Trans Chin Weld Inst, 2011; 32(3): 45
[9] (姜志忠, 黄继华, 陈树海, 巨 新. 焊接学报, 2011; 32(3): 45)
[10] Cho S, Kim D H, Ahn M Y. J Nucl Mater, 2009; 386-388: 491
[11] Rensman J,van Osch E V, Horsten M G, d'Hulst D S. J Nucl Mater, 2000; 283-287: 1201
[12] Schaeffler A L. Metall Prog, 1974; 106: 227
[13] Hu X Q, Xiao N M, Luo X H, Li D Z. Acta Metall Sin, 2009; 45: 553
[13] (胡小强, 肖纳敏, 罗兴宏, 李殿中. 金属学报, 2009; 45: 553)
[14] Wang P, Lu S P, Xiao N M, Li Y Y. Mater Sci Eng, 2010; A527: 3210
[15] Onoro J. Int J Pressure Vessels Piping, 2006; 83: 540
[16] Lippold J C. J Nucl Mater, 1981; 103-104: 1127
[17] Fenn R, Jordan M F. Met Technol, 1982; 9: 327
[18] Elmer J W, Allen S M, Eagar T W. Metall Trans, 1989; 20A: 2117
[19] Kokawa H, Kuwana T, Yamamoto A. Weld J, 1989; 68: 92
[20] Wen T, Hu X F, Song Y Y, Yan D S, Rong L J. Acta Metall Sin, 2014; 50: 447
[20] (温 涛, 胡小锋, 宋元元, 闫德胜, 戎利建. 金属学报, 2014; 50: 447)
[21] Atamert S, King J E. Acta Mater, 1991; 39: 273
[22] Jayaram R, Klueh R L. Metall Mater Trans, 1998; 29A: 1551
[23] Kim S H, Moon H K, Kang T, Lee C S. Mater Sci Eng, 2003; A356: 390
[24] Pesicka J, Kuzel R, Dronhofer A, Eggeler G. Acta Mater, 2003; 51: 4847
[25] Pesicka J, Dronhofer A, Eggeller G. Mater Sci Eng, 2004; A387-389: 176
[26] Ohashi M. J Mater Sci, 2007; 42: 9877
[27] Green G, Knott J F. Met Technol, 1975; 2: 422
[28] Anderko K, Schafer L, Matterna-Morros E. J Nucl Mater, 1991; 179-181: 492