TEXTURE OF Ti60 ALLOY PRECISION BARS AND ITS EFFECT ON TENSILE PROPERTIES

  • Zibo ZHAO ,
  • Qingjiang WANG ,
  • Jianrong LIU ,
  • Zhiyong CHEN ,
  • Shaoxiang ZHU ,
  • Bingbing YU
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2014-08-12

  Online published: 2014-12-12

Abstract

Microstructure and texture of titanium alloy are determined by thermomechanical and heat treatments and can significantly affect the mechanical properties of the final products. In this work, the microstructure and texture evolution during the heat treatment in α/β and β phase field in Ti60 precision forging bars were investigated. The results implied that the actual deformation temperature gradually decreased during precision forging processes. The microstructure and texture of Ti60 bar were determined by the finish forging temperature and the diameter, and strong microtexture macrozones existed in the forged Ti60 bar. For the bar with diameter of 45 mm (D45), the finish forging temperature fell in the lower temperature region of the α/β phase field, and the main α textures in these bars were <0001> and < 10 1 ? 0 > fiber texture components in initial Ti60 bar. The similarity of the microstructure and texture were found after heat treatment at 950 ℃. The intensity of < 10 1 ? 0 > fiber texture gradually decreased while that of <0001> fiber texture increased with the increase of the heat treatment temperature. Heat treatments have little influence on the strength of forged Ti60 bars of D45, while their ductility was reduced after β heat treatment. For the bar with diameter of 30 mm (D30), the finish forging temperature was below the α/β phase field, and the main α texture in those bars was < 10 1 ? 0 > fiber texture component. The intensity of <0001> fiber texture in those bars increased while that of < 10 1 ? 0 > fiber texture gradually decreased with the increase of the heat treatment temperature. Their room temperature strength significantly increased with the increase of the heat treatment temperature, and yield strength and tensile strength reached to 1086 and 1144 MPa, respectively, but the elongation only 3.3% after β heat treatment.

Cite this article

Zibo ZHAO , Qingjiang WANG , Jianrong LIU , Zhiyong CHEN , Shaoxiang ZHU , Bingbing YU . TEXTURE OF Ti60 ALLOY PRECISION BARS AND ITS EFFECT ON TENSILE PROPERTIES[J]. Acta Metall Sin, 2015 , 51(5) : 561 -568 . DOI: 10.11900/0412.1961.2014.00451

References

[1] Zhang S Z. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2004 (张尚州. 中国科学院金属研究所博士学位论文, 沈阳, 2004)
[2] Leyens C,Peters M,translated by Chen Z H. Titanium and Titanium Alloy. Beijing: Chemical Industry Press, 2005: 88 (Leyens C, Peters M著, 陈振华 译. 钛与钛合金. 北京: 化学工业出版社, 2005: 88)
[3] Shi Z, Guo H, Qin C, Liang H, Yao Z. Mater Sci Eng, 2014; A611: 136
[4] Tian X J, Zhang S Q, Wang H M. Int J Electr Power Energy Syst, 2014; 608: 95
[5] Seal J R, Crimp M A, Bieler T R, Boehlert C J. Mater Sci Eng, 2012; A552: 61
[6] Birosca S, Buffiere J Y, Karadge M, Preuss M. Acta Mater, 2011; 59: 1510
[7] Leary R K, Merson E, Birmingham K, Harvey D, Brydson R. Mater Sci Eng, 2010; A527: 7694
[8] Mironov S, Murzinova M, Zherebtsov S, Salishchev G A, Semiatin S L. Acta Mater, 2009; 57: 2470
[9] Wanjara P, Jahazi M, Monajati H, Yue S, Immarigeon J P. Mater Sci Eng, 2005; A396: 50
[10] Warwick J L W, Jones N G, Bantounas I, Preuss M, Dye D. Acta Mater, 2013; 61: 1603
[11] Jia W J, Zeng W D, Han Y T, Liu J R, Zhou Y, Wang Q J. Mater Des, 2011; 32: 4676
[12] Tang Z L, Wang F H, Wu W T, Wang Q J, Li D. Mater Sci Eng, 1998; A255: 133
[13] Xiong Y M, Zhu S L, Wang F H. Surf Coat Technol, 2005; 190: 195
[14] Glavicic M G, Kobryn P A, Bieler T R, Semiatin S L. Mater Sci Eng, 2003; A346: 50
[15] Obasi G C, Birosca S, Leo Prakash D G, Quinta da Fonseca J, Preuss M. Acta Mater, 2012; 60: 6013
[16] Obasi G C, da Fonseca J Q, Rugg D, Preuss M. Mater Sci Eng, 2013; A576: 272
[17] Germain L, Gey N, Humbert M, Vo P, Jahazi M, Bocher P. Acta Mater, 2008; 56: 4298
[18] Stanford N, Bate P S. Acta Mater, 2004; 52: 5215
[19] Van Bohemen S M C, Kamp A, Petrov R H, Kestens L A I, Sietsma J. Acta Mater, 2008; 56: 5907
[20] Shi R, Dixit V, Fraser H L, Wang Y. Acta Mater, 2014; 75: 156
[21] Wang Y N, Huang J C. Mater Chem Phys, 2003; 81: 11
[22] Glavicic M G, Bartha B B, Jha S K, Szczepanski C J. Mater Sci Eng, 2009; A513: 325
[23] Gey N, Bocher P, Uta E, Germain L, Humbert M. Acta Mater, 2012; 60: 2647
[24] Glavicic M G, Kobryn P A, Bieler T R, Semiatin S L. Mater Sci Eng, 2003; A346: 50
[25] Uta E, Gey N, Bocher P, Humbert M, Gilgert J. J Microscopy, 2009; 233: 451
[26] Roy S, Suwas S, Tamirisakandala S, Miracle D B, Srinivasan R. Acta Mater, 2011; 59: 5494
[27] Peck J F, Thomas D A. Trans Met Soc AIME, 1962; 221: 1240
[28] Zhang Z B. Master Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2011 (张振波. 中国科学院金属研究所硕士学位论文, 沈阳, 2011)
Outlines

/

〈 〉