Abstract

Over the past decades, traditional hard transition metal nitride films, such as TiN, have been widely used as machining and metal-forming tools coating materials due to their high hardness and chemical stability. With the rapid development of modern industrial technology, TiN has been unable to meet the requirements of modern industry, nanocomposite films because of its excellent comprehensive performance have attracted more and more scholars' attention. TiWN film as one of the TiN-based films has become a better substitute material. However the room temperature tribological property of TiWN film is not ideal, which limits its use of performance. According to the published experimental studies, C can well improve the room temperature tribological property because of its self-lubricating performance. However the effects of C content on the hardness of TiWN film is still not clear. The effects of C on mechanical property and the friction and wear property of TiWN film remain to be investigated. A series of TiWCN composite films with various C contents have been synthesized by magnetron sputtering technique. The microstructures, mechanical properties and the friction and wear property were investigated by XRD, SEM, nano-indentation, high temperature ball-on-disc tribo-meter, respectively. The results show that TiWCN composite films consist of fcc structure TiWCN phase and hcp structure Ti2N phase. With the increase of C content, the hardness of TiWCN films increases first and then decreases, the wear rate decreases first and then increases, while the friction coefficient gradually decreases. The maximum hardness of 35.97 GPa and the minimum wear rate value of 1.26×10-5 mm3·N-1·m-1 are obtained when C content is 11.25%. The minimum friction coefficient of 0.32 is obtained when C content is 13.68%. The friction coefficient and wear rate of TiWCN composite films are lower than that of TiWN films when the temperature is below 370 ℃; while the values are higher than that of TiWN films when the temperature exceeds 370 ℃. C added to the TiWN films improves mechanical properties and the room temperature friction and wear properties of the films though does not enhance the high temperature friction and wear properties of the films.

Cite this article

Lihua YU , Hongzhi DONG , Junhua XU . INFLUENCE OF C CONTENT ON MICROSTRUCTURE, MECHANICAL PROPERTIES AND FRICTION AND WEAR PROPERTIES OF TiWCN COMPOSITE FILMS[J]. Acta Metall Sin, 2014 , 50(11) : 1350 -1356 . DOI: 10.11900/0412.1961.2014.00183

References

[1] Gustavsson L E, Baránková H, Bárdos L. Surf Coat Technol, 2006; 201: 1464
[2] Veprek S, Veprek-Heijman M J G. Surf Coat Technol, 2008; 202: 5063
[3] Pan L, Bai Y Z, Zhang D, Wang J. Rare Met, 2012; 31: 183
[4] Neidhardt J, Czigány Z, Sartory B, Tessadri R, Mitterer C. Int J Refract Met Hard Mater, 2010; 28: 23
[5] Yu L H, Xue A J, Dong S T, Xu J H. Trans Mater Heat Treat, 2010; 31: 140
[5] (喻利花, 薛安俊, 董松涛, 许俊华. 材料热处理学报, 2010; 31: 140)
[6] Ezura H, Ichijo K, Hasegawa H, Yamamoto K, Hotta A, Suzuki T. Vacuum, 2008; 82: 476
[7] Caicedo J C, Yate L, Montes J. Surf Coat Technol, 2011; 205: 2947
[8] Manory R R, Mollica S, Ward L, Purushotham K P, Evans P, Noorman J, Perry A J. Surf Coat Technol, 2002; 155: 136
[9] Tian B, Yue W, Fu Z Q, Gu Y H, Wang C B, Liu J J. Vacuum, 2014; 99: 68
[10] Gassner G, Mayrhofer P H, Kutschej K, Mitterer C, Kathrein M. Surf Coat Technol, 2006; 201: 3335
[11] Chang C L, Hsieh T J. J Mater Process Technol, 2009; 209: 5521
[12] Yu L H, Ma B Y, Xu J H. Acta Metall Sin, 2012; 48: 469
[12] (喻利花, 马冰洋, 许俊华. 金属学报, 2012; 48: 469)
[13] Zhang X H, Jiang J Q, Zeng Y Q, Lin J L,Wang F L, Moore J J. Surf Coat Technol, 2008; 203: 594
[14] Xu J H, Cao J, Yu L H. Acta Metall Sin, 2012; 48: 555
[14] (许俊华, 曹 峻, 喻利花. 金属学报, 2012; 48: 555)
[15] Cheng G A, Han D Y, Liang C L,Wu X L, Zheng R T. Surf Coat Technol, 2013; 228: S328
[16] Li C Y, Chen L. Iron Steel Res, 1991; (2): 41
[16] (李长一, 陈 亮. 钢铁研究, 1991; (2): 41)
[17] Chen R, Tu J P, Liu D G, Mai Y J, Gu C D. Surf Coat Technol, 2011; 205: 5228
[18] Xue Q J,Wang L P. Diamond-Like Carbon Film Materials. Beijing: Science Press, 2012: 18
[18] (薛群基,王立平. 类金刚石碳基薄膜材料. 北京: 科学出版社, 2012: 18)
[19] Martínez-Martínez D, Sánchez-López J C, Rojas T C, Fernández A, Eaton P, Belin M. Thin Solid Films, 2005; 472: 64
[20] Ertürk E, Knotek O, Burgmer W, Prengel H G, Heuvel H J, Dederichs H G, St?ssel C. Surf Coat Technol, 1991; 46: 39
[21] Aliofkhazraei M, Sabour Rouhaghdam A. Surf Coat Technol, 2010; 205: S51
[22] Yamamoto T, Kawate M, Hasegawa H, Suzuki T. Surf Coat Technol, 2005; 193: 372
[23] Wu W Y, Wu C H, Xiao B H, Yang T X, Lin S Y, Chen P H, Chang C L. Vacuum, 2013; 87: 209
[24] Zhang L Q, Yang H S, Pang X L, Gao K W, Volinsky A A. Surf Coat Technol, 2013; 224: 120
[25] Lin J L, Moore J J, Mishra B, Pinkas M, Sproul W D. Acta Mater, 2010; 58: 1554
[26] Ziegele H, Rebholz C, Voevodin A A, Leyland A, Rohde S L, Matthews A. Tribology Int, 1997; 30: 845
[27] Chen X Y, Wang Z H, Ma S L, Ji V. Diamond Relat Mater, 2010; 19: 1336
[28] Aizawa T, Mitsuo A, Yamamoto S, Sumitomo T, Muraishi S. Wear, 2005; 259: 708
[29] Zeman P, Musil J. Appl Surf Sci, 2006; 252: 8319
[30] Aubert A, Danroc J, Gaucher A. Thin Solid Films, 1985; 126 : 61
[31] Aizawa T, Mitsuo A, Yamamoto S, Sumitomo T, Muraishi S. Wear, 2005; 259: 708
Outlines

/