ABRASIVE WEAR BEHAVIOR OF LOWER BAINITE DUCTILE IRON IN CORROSION MEDIA
Received date: 2014-06-26
Revised date: 2014-05-05
Online published: 2014-11-25
The corrosion-abrasive wear behavior of lower bainite ductile iron was investigated by corrosion-abrasive wear tests. The main factors of mass loss rate were analyzed. SEM and TEM were used to observe the worn surfaces. The strain-hardening effects beneath the contact surfaces were analyzed by microhardness profiles. The influence of load to corrosion resistance was researched by polarization curves. The results show that the main corrosion wear mechanism was corrosion mass loss and furrow wear. The roughness of worn surface, friction between sample and abrasive, depth of furrow all increased with the test load, which increased the corrosion-abrasive wear rate sharply. Meanwhile, the corrosion micro-cell formed along with the appearance of graphite ribbon and delamination at a higher load, which enhanced the corrosion rate rapidly, and the fracture of delamination resulting from plastic deformation fatigue was another critical factor of the increased mass loss. With the increase of test load, dislocation multiplication and pile-up took place in the retained austenite, which improved the wear resistance of material to some extent. However, the improvement was limited. The average mass loss rate was still increased from 0.16 g/(cm2·h) to 0.42 g/(cm2·h) with the increase of test load; the corrosion current density (icorr) was enhanced from 0.56 mA/cm2 to 5.62 mA/cm2 along with the increase of roughness. In addition, the mass loss curves of lower bainite ductile iron were divided into three stages: point contact wear (initial stage), surface contact wear (transition stage) and fatigue wear (stability stage).
Ting SUN , Renbo SONG , Fuqiang YANG , Yaping LI , Chunjing WU . ABRASIVE WEAR BEHAVIOR OF LOWER BAINITE DUCTILE IRON IN CORROSION MEDIA[J]. Acta Metall Sin, 2014 , 50(11) : 1327 -1334 . DOI: 10.11900/0412.1961.2014.00237
| [1] | Labrecque C, Gagné M. Can Metall Quart, 1998; 37: 343 |
| [2] | Pal S, Daniel W J T, Farjoo M. Int J Fatigue, 2013; 52: 144 |
| [3] | Laino S, Sikora J A, Dommarco R C. Wear, 2008; 265: 1 |
| [4] | Meena A, El Mansori M. Wear, 2011; 271: 2412 |
| [5] | Reed P A S, Thomson R C, James J S, Putman D C, Lee K K, Gunn S R. Mater Sci Eng, 2003; A346: 273 |
| [6] | Chaengkham P, Srichandr P. J Mater Process Technol, 2011; 211: 1372 |
| [7] | Bakhtiari R, Ekrami A. Mater Sci Eng, 2009; A525: 159 |
| [8] | Abbaszadeh K, Saghafian H, Kheirandish S. J Mater Sci Technol, 2012; 28: 336 |
| [9] | Kutsov A, Taran Y, Uzlov K, Krimmel A, Evsyukov M. Mater Sci Eng, 1999; A273-275: 480 |
| [10] | Abedi H R, Fareghi A, Saghafian H, Kheirandish S H. Wear, 2010; 268: 622 |
| [11] | Slatter T, Lewis R, Jones A H. Wear, 2011; 271: 1481 |
| [12] | Zhou Y, Lu Z, Zhan M. Mater Des, 2007; 28: 260 |
| [13] | Efremenko V G, Shimizu K, Noguchi T, Efremenko A V, Chabak Y G. Wear, 2013; 305: 155 |
| [14] | Lv Z L, Deng Y S, Rao Q C. Mater Mech Eng, 2011; 25(5): 32 |
| [14] | (吕振林, 邓月声, 饶启昌. 机械工程材料, 2011; 25(5): 32) |
| [15] | Nie X, Meletis E I, Jiang J C, Leyland A, Yerokhin A L, Matthews A. Surf Coat Technol, 2002; 149: 245 |
| [16] | Cheng X, Hu S, Song W, Xiong X S. Appl Surf Sci, 2013; 286: 334 |
| [17] | Ji Y, Zhao W, Zhou M, Ma H R, Zeng P. Constr Build Mater, 2013; 47: 104 |
| [18] | Mansfeld F. Corros Sci, 2005; 47: 3178 |
| [19] | Dai P Q, He Z R, Mao Z Y. J Iron Steel Res, 2004; 13(6): 47 |
| [19] | (戴品强, 何则荣, 毛志远. 钢铁研究学报, 2004; 13(6): 47) |
| [20] | Stokes B, Gao N, Reed P A S. Mater Sci Eng, 2007; A445-446: 374 |
| [21] | Wu W Q. J Iron Steel Res, 2004; 16(5): 56 |
| [21] | (吴维青. 钢铁研究学报, 2004; 16(5): 56) |
| [22] | Cavallini M, Di Bartolomeo O, Iacoviello F. Eng Fract Mech, 2008; 75: 694 |
| [23] | Abareshi M, Emadoddin E. Mater Des, 2011; 32: 5099 |
| [24] | Wang Y, Zhang K, Guo Z, Chen N L, Rong Y H. Mater Sci Eng, 2012; A552: 288 |
| [25] | Zhang A F, Xing J D, Gao Y M, Su J Y. Acta Metall Sin, 2000; 36: 765 |
| [25] | (张安峰, 邢建东, 高义民, 苏俊义. 金属学报, 2000; 36: 765) |
| [26] | Zhang P, Zhang F C, Yan Z G. Wear, 2011; 271: 697 |
/
| 〈 |
|
〉 |