Received date: 2014-08-09
Revised date: 2014-04-17
Online published: 2014-11-25
Supported by
National Natural Science Foundation of China (No.51271024)
As a candidate package material for high level radiation waste disposal, the crevice corrosion behavior of Q235 low carbon steel weld joint was investigated in a solution simulated to the groundwater in the northwest part of China. The influences of temperature and oxygen content were evaluated. The microstructure of the weld joint was observed by OM, and SEM and surface profile were employed to analyze the crevice corrosion behavior of the weld joint. Open circuit potential of different regions of the weld joint was measured by electrochemical method. Experimental results indicated that the increases of temperature and oxygen content could promote the occurrence of crevice corrosion, and facilitate the corrosion processes both inside and outside the crevice. Fusion zone with a microstructure of clustered ferrite was the most severe corroded area in the weld joint, followed by weld metal, which was characterized by a coarse widmanstaetten structure. The microstructures of base metal and heat affected zone were fine and homogeneous, so these two regions underwent slighter corrosion.
Key words: Q235 weld joint; crevice corrosion; temperature; oxygen; microstructure
Qiaohong YU , Chao LIU , Xiaolu PANG , Quanlin LIU , Kewei GAO . CREVICE CORROSION BEHAVIORS OF Q235 WELD JOINT[J]. Acta Metall Sin, 2014 , 50(11) : 1319 -1326 . DOI: 10.11900/0412.1961.2014.00188
| [1] | Yin K J, Li C, Qiu S Y, Luo Q. Nucl Power Eng, 2007; 28(2 suppl): 76 |
| [1] | (尹开锯, 李 聪, 邱邵宇, 罗 强. 核动力工程, 2007; 28(2 增刊): 76) |
| [2] | Guo Y X. Phys Chem Inspection (Phys Vol), 1999; 35: 471 |
| [2] | (郭演星. 理化检验(物理分册), 1999; 35: 471) |
| [3] | Du Z Y. Material Connection Principle. Beijing: Mechanical Industry Press, 2011: 103 |
| [3] | (杜则裕. 材料连接原理. 北京: 机械工业出版社, 2011: 103) |
| [4] | Gong M. Theory of Metal Corrosion and Corrosion Control. Beijing: Chemical Industry Press, 2009: 160 |
| [4] | (龚 敏. 金属腐蚀理论及腐蚀控制. 北京: 化学工业出版社, 2009: 160) |
| [5] | Cai B P, Liu Y H, Tian X J, Wang F, Li H, Ji R J. Corros Sci, 2010; 52: 3235 |
| [6] | Abdulsalam M I. Corros Sci, 2005; 47: 1336 |
| [7] | Kennell G F, Evitts R W. Electrochim Acta, 2009; 54: 4696 |
| [8] | Engelhard G R, McMillion L G, Macdonald D D. J Nucl Mater, 2008; 379: 48 |
| [9] | Naganuma A, Fushimi K, Azumi K, Habazaki H, Konno H. Corros Sci, 2010; 52: 1179 |
| [10] | Zhang J W, Wang W X, Huang Y P, Wang B D, Liu X. J Welding, 2007; 28: 103 |
| [10] | (张俊旺, 王文先, 黄延平, 王保东, 刘 旭. 焊接学报, 2007; 28: 103) |
| [11] | Liu C S. Master Thesis, Shenyang Aerospace University, 2011 |
| [11] | (柳春恕. 沈阳航空航天大学硕士学位论文, 2011) |
| [12] | Lv H W, Dong S G, Wang J J, Li N, Lin C J. Sci Technol Rev, 2013; 31(Z1): 25 |
| [12] | (吕虹玮, 董士刚, 王静静, 李 宁, 林昌健. 科技导报, 2013; 31(Z1): 25) |
| [13] | Qu J S, Wang Y L. Chin J Nonferrous Met, 2001; 11(S1): 194 |
| [13] | (屈金山, 王元良. 中国有色金属学报, 2001; 11(S1): 194) |
| [14] | Lei A L, Guo Q Q, Feng L J. Electrochemistry, 2006; 12: 195 |
| [14] | (雷阿利, 郭巧琴, 冯拉俊. 电化学, 2006; 12: 195) |
| [15] | Sun Q L, Cao B, Wu Y S. J Beijing Univ Sci Technol, 2009; 31: 41 |
| [15] | (孙齐磊, 曹 备, 吴荫顺. 北京科技大学学报, 2009; 31: 41) |
| [16] | Kong X D, Yang M B, Zhu M W. Development Appl Mater, 2010; 25(4): 1 |
| [16] | (孔小东, 杨明波, 朱梅五. 材料开发与应用, 2010; 25(4): 1) |
| [17] | Yin S A, Lai H Q, Weng B S, Sun X T. Chem Construction Technol, 1998; 20(04): 6 |
| [17] | (尹士安, 赖华强, 翁必生, 孙希桐. 化工施工技术, 1998; 20(04): 6) |
| [18] | Lai C X. Total Corros Control, 2004; 18(6): 10 |
| [18] | (赖春晓. 全面腐蚀控制, 2004; 18(6): 10) |
| [19] | Zhang X B, Lian J, Wang H H. Weld Product Appl, 2013; (7): 32 |
| [19] | (张心保, 连 杰, 王红鸿. 焊接生产应用, 2013; (7): 32) |
| [20] | Kennell G F, Evitts R W, Heppner K L. Corros Sci, 2008; 50: 1716 |
| [21] | Al-Zahrani A M, Pickering H W. Electrochim Acta, 2005; 50: 3420 |
| [22] | Yang W,Gu R X,Li Q S,Xiao J X. The Local Corrosion of Metals. Beijing: Chemical Industry Press, 1995: 139 |
| [22] | (杨 武,顾睿祥,黎樵燊,肖京先. 金属的局部腐蚀. 北京: 化学工业出版社, 1995: 139) |
| [23] | Laycock N J, Stewart J, Newman R C. Corros Sci, 1997; 39: 1791 |
| [24] | Huang A G, Wang Y S, Li Z Y, Zhang G D. Mater Protect, 2004; 37(3): 6 |
| [24] | (黄安国, 王永生, 李志远, 张国栋. 材料保护, 2004; 37(3): 6) |
/
| 〈 |
|
〉 |