INFLUENCE OF Ti/Al RATIOS ON γ′ COARSENING BEHAVIOR AND TENSILE PROPERTIES OF GH984G ALLOY DURING LONG-TERM THERMAL EXPOSURE

  • Meilin TAN ,
  • Changshuai WANG ,
  • Yongan GUO ,
  • Jianting GUO ,
  • Lanzhang ZHOU
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2014-03-24

  Revised date: 2014-03-24

  Accepted date: 2014-08-19

  Online published: 2014-10-28

Supported by

Supported by National High Technology Research and Development Program of China (No.2012AA03A501), National Natural Science Foundation of China (No.51301171), National Energy Administration Program of China (No.NY20110102-1) and Chinese Academy of Sciences and Sichuan Province Cooperation Program

Abstract

GH984G is a new Ni-Fe-Cr base alloy which has been designed for use as superheater, reheater and header materials for boilers in 700 ℃ advanced ultra-supercritical (A-USC) coal-fired power plants. Compared with the CCA617, Nimonic 263 and IN 740 alloys, the GH984G is an economic alloy due to the elimination of Co and it containing more than 20%Fe. As a precipitation hardened alloy, the size of γ′ precipitates has great influence on the tensile properties. The γ′ precipitates become coarse during long-term thermal exposure. The coarsening behavior of γ′ precipitates is closely related with Ti/Al ratio. However, there are few investigations about the influence of Ti/Al ratio on the coarsening behavior of γ′ precipitates of GH984G alloy. Therefore, in this work, the coarsening behavior of γ′ precipitates and its influence on tensile properties of GH984G alloy with two Ti/Al ratios was investigated during long-term thermal exposure. The results show that the growth kinetic of the γ′ precipitates can be explained by Lifshitz-Slyozov-Wagner's theory of element diffusion controlled coarsening during long-term thermal exposure at 700 and 750 ℃. The rate of γ′ precipitates growth of the alloy with high Ti/Al ratio is higher. At 800 ℃, the rate of γ′ precipitates growth decreases with increasing the thermal exposure time. The coarsening behavior does not follow the Lifshitz-Slyozov-Wagner's theory. The reasons are attributed to the effect of elastic interaction energy and the depletion of γ′-forming elements in γ matrix. The Ti/Al ratio has no obvious influence on 700 ℃ tensile properties during long-term thermal exposure between 700 and 800 ℃. The 700 ℃ yield strength has no obviously decreases even if after thermal exposure at 700 ℃ for 10480 h. The ductility increases after thermal exposure at 800 ℃. The variation of strength and ductility is attributed to the coarsening of γ′ precipitation. The deformation mechanism is the moving dislocations shear γ′ precipitates and the stacking faults form in γ′ precipitates. The fracture mode is the mixture fracture mode. The Ti/Al ratio has no significance influence on the deformation mechanism and the fracture mode.

Cite this article

Meilin TAN , Changshuai WANG , Yongan GUO , Jianting GUO , Lanzhang ZHOU . INFLUENCE OF Ti/Al RATIOS ON γ′ COARSENING BEHAVIOR AND TENSILE PROPERTIES OF GH984G ALLOY DURING LONG-TERM THERMAL EXPOSURE[J]. Acta Metall Sin, 2014 , 50(10) : 1260 -1268 . DOI: 10.11900/0412.1961.2014.00137

References

[1] Evans N D, Maziasz P J, Swindeman R W, Smith G D. Scr Mater, 2004; 51: 503
[2] Rosler J, Gotting M, Genovese D. Adv Eng Mater, 2003; 5: 469
[3] Viswanathan V, Purgert R, Rawls P. Adv Mater Processes, 2008; 166: 47
[4] Zhao S Q, Xie X S, Smith G D, Patel S J. Mater Sci Eng, 2003; A355: 96
[5] Guo J T, Du X K. Acta Metall Sin, 2005; 41: 1221
[5] (郭建亭, 杜秀魁. 金属学报, 2005; 41: 1221)
[6] Wu Q, Song H, Swindeman R W, Shingledecher J P, Vasudevan V K. Metall Mater Trans, 2008; 39: 2569
[7] Krishna R, Hainsworth S V,Gill S P A, Strang A, Atrinson H V. Metall Mater Trans, 2013; 44: 1419
[8] Rautio R, Bruce S. Adv Mater Processes, 2008; 166: 35
[9] Shingledecker J P, Pharr G M. Metall Mater Trans, 2012; 43A: 1902
[10] Tokairin T, Dahl K V, Danielsen H K, Grumsen F B, Sato T, Hald J. Mater Sci Eng, 2013; A565: 285
[11] Li J, Wahi R P. Acta Metall Mater, 1995; 43: 507
[12] Sheng L Y, Wang L J, Xi T F, Zheng Y F, Ye H Q. Mater Des, 2011; 32: 4810
[13] Wang C S,Wang T T,Tan M L,Guo Y A,Guo J T,Zhou L Z. J Mater Sci Technol, 2014;
[14] Lifshitz I M, Slyozov V V. J Phys Chem Solids, 1961; 19: 35
[15] Wagner C. Z Elektrochem, 1961; 65: 581
[16] Ardell A J. Acta Metall, 1972; 20: 61
[17] Voorhees P W, Glicksman M E. Acta Metall, 1984; 32: 51
[18] Enomoto Y, Tokuyama M, Kawasaki K. Acta Metall, 1986; 34: 2119
[19] Muralidharan G, Chen H. Adv Mater, 2000; 1: 51
[20] Xiao X, Zhao H Q, Wang C S, Guo Y A, Guo J T, Zhou L Z. Acta Metall Sin, 2013; 49: 421
[20] (肖 旋, 赵海强, 王常帅, 郭永安, 郭建亭, 周兰章. 金属学报, 2013; 49: 421)
[21] Guo J T. Acta Metall Sin, 1978; 3: 227
[21] (郭建亭. 金属学报, 1978; 3: 227)
[22] Qin X Z. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2004
[22] (秦学智.中国科学院金属研究所博士学位论文, 沈阳, 2004)
[23] Hou J S, Guo J T, Zhou L Z. Acta Metall Sin, 2006; 42: 481
[23] (侯介山, 郭建亭, 周兰章. 金属学报, 2006; 42: 481)
[24] Grosdidier T, Hazotte A, Simon A. Mater Sci Eng, 1998; A256: 183
[25] Sims C T,Stoloff N S,Hagel W C,translated by Zhao J,Zhu S J,Li X G,Wang F G. Superalloy. Dalian: Dalian Uuniversity of Technology Press, 1992: 69
[25] (Sims C T,stoloff N S,Hagel W C著;赵 杰,朱世杰,李晓刚,王富岗 译. 高温合金. 大连: 大连理工大学出版社,1992: 69)
[26] Minamino Y, Jung S B, Yamane T, Hirao K. Metall Mater Trans, 1992; 23: 2783
[27] Gomez-Acebo T, Navarcorena B, Castro F. J Phase Equilib, 2004; 25: 237
[28] Ges A, Fornaro O, Palacio H. J Mater Sci, 1997; 32: 3687
[29] Berahmand M, Sajjadi S A. Taylor Francis Online, 2012; 8: 85
[30] Hou J S, Zhang Y L, Guo J T, Ji G, Zhou L Z, Ye H Q. Acta Metall Sin, 2004; 40: 579
[30] (侯介山, 张玉龙, 郭建亭, 冀 光, 周兰章, 叶恒强. 金属学报, 2004; 40: 579)
[31] Jackson M P, Reed R C. Mater Sci Eng, 1999; A259: 85
[32] Huther W, Reppich B. Z Metall, 1978; 69: 628
[33] Reppich B. Acta Metall, 1982; 30: 87
Outlines

/

〈 〉