CRACK INITIATION AND PROPAGATION OF HIGH Nb-CONTAINING TiAl ALLOY IN FATIGUE-CREEP INTERACTION

  • Long YU ,
  • Xiping SONG ,
  • Min ZHANG ,
  • Hongliang LI ,
  • Zehui JIAO ,
  • Huichen YU
Expand
  • 1 State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083
    2 Science and Technology on Advanced High Temperature Structural Materials Laboratory, AVIC Beijing Institute of Aeronautical Materials, Beijing 100095

Received date: 2014-06-27

  Revised date: 2014-06-27

  Accepted date: 2014-08-13

  Online published: 2014-10-25

Supported by

Supported by National Basic Research Program of China (No.2011CB605506)

Abstract

TiAl-based alloys appear as potential competitors to steels and superalloys applied in aerospace and automotive industries due to their low density, high specific strength and stiffness and good oxidation resistance at elevated temperatures. As a new generation of TiAl-based alloys, high Nb-containing TiAl alloys have become a promising high temperature structural material due to their better high temperature strength and oxidation resistance than ordinary TiAl alloys. TiAl-based alloy components such as low pressure turbine blade and compressor impeller often serve in near steady conditions for a duration of time once peak operating conditions are achieved at high temperature. The components suffer not only from rapidly induced damage from start-up and shutdown cycles, but also from creep damage under sustained loading periods. Moreover, the possible interaction damage between fatigue and creep must be considered. Thus, the study of fatigue-creep interaction for TiAl-based alloys is of great practical importance. Large numbers of researches were focused on the fatigue or creep properties of TiAl-based alloys, however, the fatigue-creep interaction behavior was rarely reported. Therefore, the crack initiation and propagation behavior of a nearly lamellar Ti-45Al-8Nb-0.2W-0.2B-0.1Y alloy in fatigue-creep interaction was observed at 750 ℃. The cyclic loading tests were carried out using a mini servo-hydraulic fatigue machine in a SEM chamber. The entire process of crack initiation and propagation was observed. The load cycling was trapezoidal by applying a dwell time at the maximum tension stress. The results indicated that micro-cracks mainly occurred at internal grain boundaries in the form of creep void or fatigue micro-crack. The micro-cracks firstly extended along the grain boundary by absorbing the creep voids or the stress concentration around crack tips, then connected with each other forming a longer crack. As the crack was frustrated by grain boundaries of other orientations, the crack began to grow in the thickness direction. Meanwhile, the micro-cracks perpendicular to loading direction emerged. Eventually, the frustrated cracks interconnected resulting in fracture. Compared to the in situ SEM observations in fatigue deformation, the dwell time resulted in the increase of probability of grain boundary crack initiation and the changes of crack propagation path. Thus, the fracture mode transform from transcrystalline to intercrystalline and the fatigue lifetime significantly decreased. The model of the crack initiation and propagation behaviors of high Nb-containing TiAl alloys in fatigue-creep interaction was presented in this work.

Cite this article

Long YU , Xiping SONG , Min ZHANG , Hongliang LI , Zehui JIAO , Huichen YU . CRACK INITIATION AND PROPAGATION OF HIGH Nb-CONTAINING TiAl ALLOY IN FATIGUE-CREEP INTERACTION[J]. Acta Metall Sin, 2014 , 50(10) : 1253 -1259 . DOI: 10.11900/0412.1961.2014.00346

References

[1] Kim Y W. JOM, 1989; 41(7): 24
[2] Kim Y W. Acta Metall Mater, 1992; 40: 1121
[3] Zhang Y G,Han Y F,Chen G L,Guo J T,Wan X J,Feng D. Structural Intermetallics. Beijing: National Defense Industry Press, 2001: 705
[3] (张永刚,韩雅芳,陈国良,郭建亭,万晓景,冯 涤. 金属间化合物结构材料. 北京: 国防工业出版社, 2001: 705)
[4] Chen G L,Lin J P.Physical Metallurgy for the structural Ordered Intermetallics. Beijing: Metallurgical Industry Press, 1999: 285
[4] (陈国良,林均品. 有序金属间化合物结构材料物理金属学基础. 北京: 冶金工业出版社, 1999: 285)
[5] Chen G L, Wang X T, Ni K Q, Hao S M, Cao J X, Ding J J, Zhang X. Intermetallics, 1996; 4: 13
[6] Zhang W J, Deevi S C, Chen G L. Intermetallics, 2002; 10: 403
[7] Tetsui T. Intermetallics, 2002; 10: 239
[8] Chen G L, Sun Z Q, Zhou X. Mater Sci Eng, 1992; A153: 597
[9] Chen G L, Sun Z Q, Zhou X. Corrosion, 1992; 48: 939
[10] Li S J, Liu Z C, Lin J P, Chen G L, Zhang W J. Rare Met Mater Eng, 2002; 31: 31
[10] (李书江, 刘自成, 林均品, 陈国良, 张卫军. 稀有金属材料与工程, 2002; 31: 31)
[11] He S F, Lin J P, Xu X J, Gao J F, Wang Y L, Song X P, Chen G L. Rare Met Mater Eng, 2006; 35: 257
[11] (何素芳, 林均品, 徐向俊, 高建峰, 王艳丽, 宋西平, 陈国良. 稀有金属材料与工程, 2006; 35: 257)
[12] Chen W R, Triantafillou J, Beddoes J, Zhao L. Acta Metall Sin (Engl Lett), 1996; 9: 565
[13] Nagai H, Takahashi T, Oikawa H. J Mater Sci, 1990; 25: 629
[14] Kimm D I, Wolfenstine J. Scr Metall Mater, 1994; 30: 615
[15] Wang J N, Zhu J, Wu J S, Du X W. Acta Meter, 2002; 50: 1307
[16] Zhang W J, Chen G L, Appel F, Nieh T G, Deevi S C. Mater Sci Eng, 2001; A315: 250
[17] Sastry S M L, Lipsitt H A. Metall Trans, 1977; 8A: 299
[18] Malakondaiah G, Nicholas T. Metall Mater Trans, 1996; 27A: 2239
[19] Gloanec A L, Jouiad M, Bertheau D, Grange M, Henaff G. Intermetallics, 2007; 15: 520
[20] Gloanec A L, Milani T, Henaff G. Int J Fatigue, 2010; 32: 1015
[21] Cao R, Lin Y Z, Hu D, Chen J H. Eng Fract Mech, 2008; 75: 4343
[22] Kim S W, Kumar K S, Oh M H, Wee D M. Intermetallics, 2007; 15: 976
[23] Mine Y J, Fujisaki H, Matsuda M, Takeyama M, Takashima K. Scr Mater, 2011; 65: 707
[24] Li X D, Wang X S, Ren H H, Chen Y L, Mu Z T. Corros Sci, 2012; 55: 26
[25] Wang X S, Yan C K, Li Y, Xue Y B, Meng X K, Wu B S. Int J Fract, 2008; 151: 269
[26] Wang X S, Fan J H. Int J Fatigue, 2006; 28: 79
[27] Polak J, Man J, Petrenec M, Tobias J. Int J Fatigue, 2012; 39: 103
[28] Christ H J, Wamukwamba C K, Mughrabi H. Mater Sci Eng, 1997; A234-246: 382
[29] Zhang J S. Deformation and Fracture of Materials at High Temperature. Beijing: Science Press, 2007: 426
[29] (张俊善. 材料的高温变形与断裂. 北京: 科学出版社, 2007: 426)
[30] Yu L, Song X P, Zhang M, Lin J P, Jiao Z H, Yu H C. Rare Met Mater Eng, 2014; 43: 881
[30] (余 龙, 宋西平, 张 敏, 林均品, 焦泽辉, 于慧臣. 稀有金属材料工程, 2014; 43: 881)
Outlines

/

〈 〉