STUDY OF THE COARSENING AND HARDENING BEHAVIORS OF COHERENT g-Fe PARTICLES IN Cu-2.1Fe ALLOY

  • Qiyi DONG ,
  • Leinuo SHEN ,
  • Feng CAO ,
  • Yanlin JIA ,
  • Mingpu WANG
Expand
  • School of Materials Science and Engineering, Central South University, Changsha 410083

Received date: 2014-03-31

  Revised date: 2014-03-31

  Accepted date: 2014-07-27

  Online published: 2014-10-25

Supported by

Supported by Open-End Fund for the Valuable and Precision Instruments of Central South University (No.CSUZC20140012)

Abstract

As one of the most widely used integrated circuit (IC) lead frame materials, Cu-2.1Fe alloy (C19400) shows excellent comprehensive properties, such as 90° bend fatigue, 90° bend formability, corrosion-proof, solder ability and resistance of solder peeling off. As a successful medium-strength and high-conductivity copper alloy, the Cu-2.1Fe alloy is strengthened by precipitation hardening and work hardening. Metastable coherent g-Fe particles will precipitate from supersaturated copper matrix during aging. The effects of long-term aging at different temperatures on the g-Fe coarsening characteristics and the mechanical properties of Cu-2.1Fe alloy were investigated, by means of conventional TEM, SEM, hardness, tensile strength and electrical conductivity testing. The results show that solution-treated Cu-2.1Fe alloys can reach its peak hardness and maintain for a longer time when aging at 500 ℃. The maximum of strength occurred at a particle size of about 12 nm in mean diameter. The coarsening kinetics of g-Fe follows Lifshitz-Slyozov-Wagner (LSW) theory and the activation energy for growth is estimated to 222 kJ/mol. Furthermore, it is found that coherent Fe particles gradually evolve into semi-coherent and cubical particles after aging for a long time and at high temperatures. The aging strengthening effect of Fe particles is not significant, and the maximum increment of stress is about 100 MPa. The strengthening mechanism of undeformed Cu-Fe alloy is coherency strengthening during the under-aged stage and changes to Orowan mechanism during the over-aged stage. Experimental results are in agreement with theoretical predictions.

Cite this article

Qiyi DONG , Leinuo SHEN , Feng CAO , Yanlin JIA , Mingpu WANG . STUDY OF THE COARSENING AND HARDENING BEHAVIORS OF COHERENT g-Fe PARTICLES IN Cu-2.1Fe ALLOY[J]. Acta Metall Sin, 2014 , 50(10) : 1224 -1230 . DOI: 10.11900/0412.1961.2014.00152

References

[1] Song L N, Liu J B, Huang L Y, Zeng Y W, Meng L. Acta Metall Sin, 2012; 48: 1459
[1] (宋鲁南, 刘嘉斌, 黄六一, 曾跃武, 孟 亮. 金属学报, 2012; 48: 1459)
[2] Wu Z W, Liu J J, Chen Y, Meng L. J Alloys Compd, 2009; 467: 213
[3] Dong Q Y, Wang M P, Jia Y L, Chen C, Xia C D. Trans Mater Heat Treat, 2013; 34(6): 75
[3] (董琦祎, 汪明朴, 贾延琳, 陈 畅, 夏承东. 材料热处理学报, 2013; 34(6): 75)
[4] Dai J Y, Yin Z M, Song L P, Yuan Y. Chin J Nonferrous Met, 2009; 19: 1969
[4] (戴娇燕, 尹志民, 宋练鹏, 袁 远. 中国有色金属学报, 2009; 19: 1969)
[5] Cao H, Min J Y, Wu S D, Xian A P, Shang J K. Mater Sci Eng, 2006; A431: 86
[6] Lu D P, Wang J, Zeng W J, Liu Y, Lu L, Sun B D. Mater Sci Eng, 2006; A421: 254
[7] Kim H G, Lee T W, Han S Z, Euh K, Kim W Y, Lim S H. Met Mater Int, 2012; 18: 335
[8] Yan X D, Tu S J, Huang G J, Xie S S. Chin J Rare Met, 2005; 29: 635
[8] (闫晓东, 涂思京, 黄国杰, 谢水生. 稀有金属, 2005; 29: 635)
[9] Shigenori H, Shigeoki S. J Jpn Copper Brass Res Assoc, 1970; 9: 201
[9] (堀茂徳, 佐治重興. 伸銅技術研究會誌, 1970; 9: 201)
[10] Baker H.ASM Handbook-Alloy Phase Diagrams. Materials Park, Ohio: ASM International, 1992: 734
[11] Matsuura K, Tsukamoto M, Watanabe K. Acta Metall, 1973; 21: 1033
[12] Kinsman K R, Sprys J W, Asaro R J. Acta Metall, 1975; 23: 1431
[13] Easterling K E, Miekk-oja H M. Acta Metall, 1967; 15: 1133
[14] Lifshitz I M, Slyozov V V. J Phys Chem Solids, 1961; 19: 35
[15] Wagner C. Z Elektrochem, 1961; 65: 581
[16] Mackliet C A. Phys Rev, 1958; 109: 1964
[17] Ardell A J. Metall Trans, 1985; 16A: 2131
[18] Martienssen W, Warlimont H.Springer Handbook of Condensed Matter and Materials Data. Heidelberg, Berlin: Springer, 2005: 132
[19] Lee J, Jung J Y, Lee E S, Park W J, Ahn S, Kim N J. Mater Sci Eng, 2000; A277: 274
[20] Donoso E, Espinoza R, Dianez M J, Criado J M. Mater Sci Eng, 2012; A556: 612
[21] Pang Y, Xia C D, Wang M P, Li Z, Xiao Z, Wei H G, Sheng X F, Jia Y L, Chen C. J Alloys Compd, 2014; 582: 786
[22] Guo M X, Shen K, Wang M P. Acta Mater, 2009; 57: 4568
Outlines

/

〈 〉