LAVES PHASE EVOLUTION IN P92 STEEL DURING AGEING

  • Xue WANG ,
  • Shumin YU ,
  • Yaoyao REN ,
  • Hong LIU ,
  • Hongwei LIU ,
  • Lei HU
Expand
  • 1 School of Power and Mechanics, Wuhan University, Wuhan 430072
    2 Key Laboratory of Accoutrement Technique in Fluid Machinery & Power Engineering of Hubei Province, Wuhan University, Wuhan 430072
    3 Dongfang Boiler Group Co. Ltd., Zigong 643001

Received date: 2014-03-05

  Revised date: 2014-03-05

  Accepted date: 2014-06-06

  Online published: 2014-10-25

Supported by

Supported by National Natural Science Foundation of China (Nos.51074113 and 51374153) and Sichuan Province Fundamental Research Project (No.2013JY0123)

Abstract

ASME P92 (9Cr-0.5Mo-1.8WVNb) is a key material for the main steam pipe and header with larger diameter and thick wall in ultra-supercritical (USC) plant, because of its low thermal expansion coefficient, good corrosion resistance, good fabricability and especially its high creep rupture strength. The Laves phase (Fe2M) precipitates in service and plays complicated and controversial role in affecting and/or determining the creep strength of the P92 steel. The fine Laves phase particles may contribute to precipitation strengthening and decrease the creep rate in the primary and transient creep region, however, the subsequent coarsening of Laves phase reduces the precipitation strengthening. Thus, in order to provide a systematic and definite understanding of the creep properties, it is necessary to investigate the precipitation and coarsening behavior of the Laves phase in P92 steel. In this work, the Laves phase parameters of P92 steel, including volume fraction, mean diameter and number density, were measured using SEM-BSE and quantitative metallography methods during aging at 650 ℃ for 0~8000 h. The precipitate and coarsening kinetics were investigated based on the quantification of Laves phase in P92 steel. Furthermore, the martensitic lath stability during aging was observed by OM and TEM. Lastly, the influence of Laves phase evolution on the creep rupture strength was estimated from the change of Orowan stress during aging. The results indicate that SEM-BSE is a suitable method for measurement of Laves phase precipitates, and can achieve significantly statistical data when characterizing large particles comparing with the EFTEM, so that evaluate the kinetics of precipitation and coarsening of Laves phase. The Laves phase precipitates at grain boundaries preferentially during the 0~2000 h of aging and its final volume fraction is around 0.95%. Obvious coarsening of Laves phase is observed after aging for 3000 h and its rate is much greater than that of M23C6 carbides. Grain boundary diffusion may play significant role in much rapider coarsening of Laves phases than that of M23C6 carbides. The Laves phase has the most precipitate hardening in the P92 steel aged up to 1000~3000 h and this hardening would drop remarkably due to its fast coarsening after aging for 3000 h. The contribution of Laves phase particles to creep strength is much less than that of M23C6 carbides. The P92 steel has a sub-microstructure with clear lath and high density dislocations after aging at 650 ℃ for 8000 h due to the stable M23C6 carbides on sub-boundaries.

Cite this article

Xue WANG , Shumin YU , Yaoyao REN , Hong LIU , Hongwei LIU , Lei HU . LAVES PHASE EVOLUTION IN P92 STEEL DURING AGEING[J]. Acta Metall Sin, 2014 , 50(10) : 1195 -1202 . DOI: 10.11900/0412.1961.2014.00101

References

[1] Jorgen B, Sven K, Rudolph B. Energy, 2006; 31: 1437
[2] Richardot D, Vaillant J C, Arbab A, Bendick W. The T/P92 Book. 2nd Ed., Boulogne: Vallourec & Mabbesmann Tubes, 2002: 1
[3] Shen Q, Liu H G. Electr Power Constrc, 2010; 31(10): 71
[3] (沈 琦, 刘鸿国. 电力建设, 2010; 31(10): 71)
[4] Masuyama F. ISIJ Int, 2001; 41: 612
[5] Abe F. Mater Sci Eng, 2001; A319-321: 770
[6] Tsuchida Y, Okamoto K, Tokunaga Y. ISIJ Int, 1995; 35: 317
[7] Maruyama K, Sawada K, Koike J. ISIJ Int, 2001; 41: 641
[8] Abe F. Metall Mater Trans, 2005; 36A: 321
[9] Peng Z F, Cai L S, Peng F F, Hu Y P, Chen F Y. Acta Metall Sin, 2010; 46: 429
[9] (彭志方, 蔡黎胜, 彭芳芳, 胡永平, 陈方玉. 金属学报, 2010; 46: 429)
[10] Lee J S, Armaki H G, Maruyama K, Muraki T, Asahi H. Mater Sci Eng, 2006; A428: 270
[11] Wang X, Pan Q G, Tao Y S, Zhang Y L, Zeng H Q, Liu H. Acta Metall Sin, 2012; 48: 427
[11] (王学, 潘乾刚, 陶永顺, 章应霖, 曾会强, 刘 洪. 金属学报, 2012; 48: 427)
[12] Chen Y X, Yan W, Hu P, Shan Y Y, Yang K. Acta Metall Sin, 2011; 47: 1372
[12] (陈云翔, 严 伟, 胡 平, 单以银, 杨 柯. 金属学报, 2011; 47: 1372)
[13] Hofer P, Cerjak H, Warbichler P. Mater Sci Technol, 2000; 16: 1221
[14] Dimmler G, Weinert P, Kozeschnik E, Cerjak H. Mater Charact, 2003; 51: 341
[15] Hald J. J Pressure Vessels Piping, 2008; 85: 30
[16] Qing G Y. Quantity Metallography. Chendu: Sichuan Science and Technology Press, 1987: 1
[16] (秦国友. 定量金相. 成都: 四川科学技术出版社, 1987: 1)
[17] Fujita N, Ohmura K, Yamamoto A. Mater Sci Eng, 2003; A351: 272
[18] Yong Q L. Secondary Phase in Steels. Beijing: Metallurgical Industry Press, 2006: 303
[18] (雍歧龙.钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 303)
[19] Qi Z F. Diffusion and Phase Transformation in Solid Metals. Beijing: China Machine Press, 1998: 196
[19] (戚正风. 固态金属中的扩散与相变. 北京: 机械工业出版社, 1998: 196)
[20] ?gren J, Clavaguera-Mora M T, Golcheski J, Inden G, Kumar H, Sigli C. Calphad, 2000; 24: 41
[21] Abe F. Mater Sci Eng, 2004; A387-389: 565
[22] Hald J, Korcakova L. ISIJ Int, 2003; 43: 420
[23] Gustafson ?, H?ttestrand M. Mater Sci Eng, 2002; A333: 279
[24] Zhang J S.High Temperature Deformation and Fracture of Materials. Beijing: Science Press, 2007: 232
[24] (张俊善. 材料的高温变形与断裂.北京: 科学出版社, 2007: 232)
[25] Dejun L, Shinozaki K. Sci Technol Weld Joining, 2005; 10: 544
Outlines

/

〈 〉