TEMPERATURE EFFECT OF Xe ION IRRADIATION TO 316 AUSTENITIC STAINLESS STEEL

  • Hefei HUANG ,
  • Jianjian LI ,
  • Renduo LIU ,
  • Huaican CHEN ,
  • Long YAN
Expand
  • 1 Key Laboratory of Nuclear Radiation and Nuclear Energy Technology, Chinese Academy of Sciences, Shanghai 201800
    2 Shanghai Institute of Applied Physics, Chinese Academy of Sciences, Shanghai 201800

Received date: 2014-03-05

  Revised date: 2014-03-05

  Accepted date: 2014-07-03

  Online published: 2014-10-25

Supported by

Supported by National Basic Research Program of China (No.2010CB832903)

Abstract

Molten Salt Reactors (MSR) is one of the six most promising Generation IV fission reactors. In the ultimate goals, MSR should run at temperatures over 1000 K, and its neutron irradiation damage doses could reach 100 dpa or more for the core components. Hence, the evaluation of irradiation damage under high temperature for structural materials is of particular importance for ensuring the safe operation of MSR. It is generally accepted the structural materials used for MSR should be Ni-based alloys, especially the Hastelloy N alloy. Recently, the 316 austenitic stainless steel (316SS) was considered as a candidate structural material for MSR. In this study, bulk and TEM specimens of 316SS have been characterized by nanoindentation and TEM to determine the change of micro-hardness and microstructural evolution after 7 MeV Xe26+ and 1 MeV Xe20+ iron irradiation, respectively. The irradiation experiments were carried out at room temperature (about 22 ℃) and 600 ℃, and the ion fluences correspond to calculated peak damge dose of 0.62 and 3.7 dpa. The nanoindentation results for bulk specimens showed the irradiation induced hardening of 316SS irradiated at room temperature, and the hardenability increases with increasing ion damage dose. However, in the case of the irradiation at 600 ℃, the hardness of 316SS keep the same level with that of the unirradiated specimen. The recovery of irradiation induced hardening occurred at 600 ℃ compared with the room temperature irradiation. The TEM results showed that the presence of high number density of nanoscale dislocation loops, with the diameter of 3~8 nm, in 316SS irradiated at room temperature. The number density of these dislocation loops increase with the increase of ion damage dose. As far as the irradiated 316SS under 600 ℃, several solute clusters were observed with the size range from 4 to 12 nm, which a little larger than the dislocation loops. It should be noted that the number density is far smaller than that of the dislocation loops in former case. The radiation induced defects (dislocation loops, solute clusters) were believed to be responsible for the hardening in 316SS. The temperature effect of Xe ion irradiation to 316SS was discussed using the Orowan mechanism. The stronger diffusion of point defects caused by ion implantation at 600 ℃ was considered to be the main reason for the recovery of irradiation induced hardening, in which the vacancies and interstitials have greater probability for recombination and then disappear, resulting in the exiguous nucleation sites for the formation of solute clusters.

Cite this article

Hefei HUANG , Jianjian LI , Renduo LIU , Huaican CHEN , Long YAN . TEMPERATURE EFFECT OF Xe ION IRRADIATION TO 316 AUSTENITIC STAINLESS STEEL[J]. Acta Metall Sin, 2014 , 50(10) : 1189 -1194 . DOI: 10.11900/0412.1961.2014.00099

References

[1] Abram T, Ion S. Energy Policy, 2008; 36: 4323
[2] Wanderka N, Bakai A, Abromeit C, Isheim D, Seidman D N. Ultramicroscopy, 2007; 107: 786
[3] Jiang M H, Xu H J, Dai Z M. Bull Chin Acad Sci, 2012; 27: 366
[3] (江绵恒, 徐洪杰, 戴志敏.中国科学院院刊, 2012; 27: 366)
[4] Murty K L, Charit I. J Nucl Mater, 2008; 383: 189
[5] Yvon P, Carre F. J Nucl Mater, 2009; 385: 217
[6] Zinkel S J, Was G S. Acta Mater, 2013; 61: 735
[7] Preliminary Fluoride Salt-Cooled High Temperature Reactor (FHR) Materials Components White Paper, UCBTH-1-003, 2012
[8] Was G S, Busby J T, Allen T, Kenik E A, Jensson A, Bruemmer S M, Gan J, Edwards A D, Scott P M, Andreson P L. J Nucl Mater, 2002; 300: 198
[9] Edwards D J, Simonen E P, Garner F A, Greenwood L R, Olivier B M, Bruemmer S M. J Nucl Mater, 2003; 317: 32
[10] Miura T, Fujii K, Fukuya K, Ito Y. J Nucl Mater, 2009; 386-388: 210
[11] Etienne A, Hernández-Mayoral M, Genevois C, Radiguet B, Pareige P. J Nucl Mater, 2010; 400: 56
[12] Etienne A, Radiguet B, Cunningham N J, Odette G R, Valiev R, Pareige P. Ultramicroscopy, 2011; 111: 659
[13] Pennell W E. Nucl Technol, 1972; 16: 332
[14] Mao L B, Yang Z Q, Shan R H, Shui Z W, Yin S J, Lu C L, Peng X M. China Nucl Sci Technol Rep, 2003; 3: 10
[14] (毛林彬, 杨治全, 单润华, 税忠伟, 尹顺玖, 鲁长龙, 彭小明.中国核科技报告, 2003; 3: 10)
[15] Muthukumaran V, Selladurai V, Nandhakumar S, Senthilkumar M. Mater Des, 2010; 31: 2813
[16] Zheng Y N, Zuo Y, Yuan D Q, Zhou D M, Xu Y J, Fan P, Zhu J Z, Wang Z Q, Zhu S Y. Nucl Phys, 2010; 834A: C761
[17] Nagy P M, Aranyi D, Horvath P, Peto G, Kalman E. Surf Interf Anal, 2008; 40: 875
[18] Ma X, Liu H P, Sun L T, Song M T, Zhu X L, Sha S, Feng W T, Zhang D C, Zhang S F, Li B, Li J Y, Qian D B, Xu S Y, Gao D Q, Wang P Z, Ma L Z, Man K D, Xiao G Q, Zhao H W, Zhan W L. J Phys Conf Ser, 2009; 163: 012104
[19] Stoller R E, Toloczko M B, Was G S, Certain A G, Dwaraknath S, Garner F A. Nucl Instrum Methods Phys Res, 2013; 310B: 75
[20] Lee E H, Lee Y, Oliver W C, Mansur L K. J Mater Res, 1993; 8: 377
[21] Nix W D, Gao H. J Mech Solids, 1998; 46: 411
[22] Kasada R, Takayama Y,?Yabuuchi K,?Kimura A. Fusion Eng Des, 2011; 86: 2658
[23] Takayama Y, Kasada R, Sakamoto Y, Yabuuchi K, Kimura A, Ando M, Hamaguchi D. J Nucl Mater, 2013; 442: S23
[24] Liu X B, Wang R S, Rei A, Jiang J, Xu C L, Huang P, Qian W J, Wu Y C, Zhang C H. J Nucl Mater, 2014; 444: 1
[25] Huang H F, Li D H, Li J J, Liu R D, Lei G H, He S X, Huang Q, Yan L. Mater Trans, 2014; 55: 1243
[26] Hernandez-Mayoral M, Yao Z, Jenkins M L, Kirk M A. Philos Mag, 2014; 88: 2881
[27] Jenkins M L, English C A, Eyre B L. Philos Mag, 1978; 38A: 97
[28] Calder A F, Bacon D J. J Nucl Mater, 1993; 207: 25
[29] OsetskyY N, Bacon D J, Singh B N, Wirth B. J Nucl Mater, 2002; 307-311: 852
[30] Radiguet B, Barbu A, Pareige P. J Nucl Mater, 2007; 360: 104
[31] Etienne A, Radiguet B, Cunningham N J, Odette G R, Pareige P. J Nucl Mater, 2010; 406: 244
[32] Huang H F. PhD Dissertation, University of Rouen, 2012
[33] Huang H F,Radiguet B,Todeschini P,Chas G,Pareige P. In: Gibson J K, McCall S K, Bauer E D, Soderholm L, Fanghaenel T, Devanathan R, Misra A, Trautmann C, Wirth B D eds., Proc MRS 2010 on Basic Actinide Science and Materials for Nuclear Applications, Pennsylvania: The Cambridge University Press, 2010: 235
[34] Gan J, Simonen E P, Bruemmer S M, Fournier L, Sencer B H, Was G S. J Nucl Mater, 2004; 325: 94
[35] Lambrecht M, Meslin E, Malerba L, Hernandez-Mayoral M, Bergner F, Pareige P, Radiguet B, Almazouzi A. J Nucl Mater, 2010; 406: 84
[36] Yang W D.Reactor Materials Science. 2nd Ed., Beijing: Atomic Energy Press, 2006: 1
[36] (杨文斗.反应堆材料学. 北京: 原子能出版社. 第2版, 2006: 1)
Outlines

/

〈 〉