CHARACTERISTICS AND EVOLUTION OF THIN LAYER ELECTROLYTE ON PIPELINE STEEL UNDER CATHODIC PROTECTION SHIELDING DISBONDED COATING

  • Maocheng YAN ,
  • Jianqiu WANG ,
  • En-hou HAN ,
  • Cheng SUN ,
  • Wei KE
Expand
  • National Engineering Center for Corrosion Control, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Revised date: 2014-04-02

  Online published: 2014-09-25

Supported by

Supported by National Natural Science Foundation of China (No.51131001) and Scientific Research Foundation for the Returned Overseas Chinese Scholars, Ministry of Education

Abstract

External corrosion and stress corrosion cracking (SCC) have been observed in a thin layer electrolyte under disbonded coating shielding cathodic protection (CP). In this work, characteristic and evolution of the thin layer electrolyte environment (potential, pH, etc.) on pipeline steel under disbonded coatings were investigated by microelectrode technology in a simulating crevice cell at various CP levels and different atmosphere conditions (CO2 and O2). The results show that pH of the thin layer electrolyte under the disbondment varies from near neutral to the value as high as 12, depending on the amount of CP current and CO2. CP current on pipeline surface initiates a high pH environment on the steel surface. Due to the CP shielding effect and a high CO2 content, a near-neutral pH environment may exist under disbonded coating. The CP effectiveness and the shielding effect of the disbondment can be estimated by measuring pH of the thin layer electrolyte under disbonded coatings.

Cite this article

Maocheng YAN , Jianqiu WANG , En-hou HAN , Cheng SUN , Wei KE . CHARACTERISTICS AND EVOLUTION OF THIN LAYER ELECTROLYTE ON PIPELINE STEEL UNDER CATHODIC PROTECTION SHIELDING DISBONDED COATING[J]. Acta Metall Sin, 2014 , 50(9) : 1137 -1145 . DOI: 10.11900/0412.1961.2014.00156

References

[1] Sheng G J, Chen H Y, Xue Z Y, Zhao J. Corros Sci Prot Technol, 2013; 25: 246
[1] (沈光霁, 陈洪源, 薛致远, 赵 君. 腐蚀科学与防护技术, 2013; 25: 246)
[2] Tang Y P, Yan R J, Huang Z Y, Li J X, Wang L. Mater Prot, 2011; 44(12): 45
[2] (唐谊平, 晏荣军, 黄子阳, 李建新, 王 琍. 材料保护, 2011; 44(12): 45)
[3] Song F M, Kirk D W, Graydon J W, Cormack D E, Wong D. Mater Perform, 2003; 42: 24
[4] Nazarbeygi A E, Moeini A R. Mater Perform, 2009; 48: 32
[5] Argent C, Norman D. Corrosion' 2005, Houston, TX: NACE, 2005: Paper 05034 (CD)
[6] Hughes C, Norsworthy R. Corrosion' 2009, Houston, TX: NACE International, 2009: Paper 09043 (CD)
[7] Yan M C, Weng Y J. J Chin Soc Corros Prot, 2004; 24: 95
[7] (闫茂成, 翁永基. 中国腐蚀与防护学报, 2004; 24: 95)
[8] Zhang Y Y, Han W L, Li A G, Shao H Q, Xie B B. Corros Prot, 2010; 31: 787
[8] (张盈盈, 韩文礼, 李爱贵, 邵怀启, 解蓓蓓. 腐蚀与防护, 2010; 31: 787)
[9] Xu J, Sun C, Yan M C, Wang F H. Mater Chem Phys, 2013; 142: 692
[10] Fang B Y, Han E H, Wang J Q, Ke W. Corros Eng Sci Technol, 2007; 42: 123
[11] Song F M. Corros Sci, 2012; 55: 107
[12] Wang Z Y, Wang J Q, Han E-H, Ke W, Yan M C, Zhang J W, Liu C W. Acta Metall Sin, 2012; 48: 1267
[12] (王志英, 王俭秋, 韩恩厚, 柯 伟,?闫茂成, 张峻巍, 刘楚威. 金属学报, 2012; 48: 1267)
[13] Zhao B, Du C W, Liu Z Y, Li X G, Yang J K, Li Y Q. Acta Metall Sin, 2012; 48: 1530
[13] (赵 博, 杜翠薇, 刘智勇, 李晓刚, 杨吉可, 李月强. 金属学报, 2012; 48: 1530)
[14] Parkins R N. Corrosion' 2000, Houston, TX: NACE, 2000: Paper 363 (CD)
[15] Eslami A, Fang B, Kania R, Worthingham B, Been J, Eadie R, Chen W. Corros Sci, 2010; 52: 3750
[16] Martyn W, Brian E, Tom J, Robert W. Proceedings of the 1998 International Pipeline Conference, IPC. Part 1, New York: ASME, 1998: 399
[17] Perdomo J J, Song I. Corros Sci, 2000; 42: 1389
[18] Fessler R R, Markworth A J, Parkins R N. Corrosion, 1983; 39: 20
[19] Li Z F, Gan F X, Mao X H. Corros Sci, 2002; 44: 689
[20] Yan M C, Weng Y J. J Chin Soc Corros Prot, 2005; 25: 34
[20] (闫茂成, 翁永基. 中国腐蚀与防护学报, 2005; 25: 34)
[21] Yan M C, Wang J Q, Han E H, Ke W. Corros Eng Sci Technol, 2007; 42: 42
[22] Yan M C, Wang J Q, Ke W, Han E-H. J Chin Soc Corros Prot, 2007; 27: 257
[22] (闫茂成, 王俭秋, 柯 伟, 韩恩厚. 中国腐蚀与防护学报, 2007; 27: 257)
[23] Yan M C, Wang J Q, Han E-H, Ke W. Corros Sci, 2008; 50: 1331
[24] Song F M. Corrosion, 2010; 66: 095004-095004-14
[25] Charles E A, Parkins R N. Corrosion, 1995; 51: 518
[26] Chen X, Li X G, Du C W, Cheng Y F. Corros Sci, 2009; 51: 2242
[27] Yan M C, Sun C, Xu J, Dong J H, Ke W. Corros Sci, 2014; 80: 309
[28] Eslami A, Kania R, Worthingham B, Boven G V, Eadie R, Chen W. Corrosion, 2013; 69: 1103
Outlines

/

〈 〉