A NEW METHOD FOR SIMULATING AND PREDICT- ING DYNAMIC RECRYSTALLIZATION IN METAL FORGING
Revised date: 2014-03-27
Online published: 2014-09-25
Supported by
Supported by National Natural Science Foundation of China (No.51164030)
The window of thermomechanical parameters where dynamic recrystallization occurs can be predicted according to the power dissipation map based on dynamic materials model, and the distribution of thermomechanical parameters in metal forging can be calculated by using finite element (FE) simulation. Thus, the zone of dynamic recrystallization and its evolution in metal forging not only can be simulated and predicted, but also the forging process parameters where dynamic recrystallization occurs can be optimized by the combination of the window of thermomechanical parameters where dynamic recrystallization occurs and finite element simulaton, which provides a new way for realizing the control of microstructure and property of forging. A method for simulating and predicting dynamic recrystallization in metal forging is proposed based on the combination of the thermomechanical parameter window of dynamic recrystallization predicted by power dissipation map and finite element simulation, and the method is already integrated into the commercial FE software Deform 3D. The zone of dynamic recrystallization and its evolution in compression of titanium alloy TC11 at process parameters (1020 ℃, 0.1 s-1), (1050 ℃, 0.1 s-1), (1050 ℃, 10 s-1) and constant strain rate are successfully simulated and predicted by using the modified FE software Deform 3D. The simulated and predicted result is in good agreement with experiment.
Shiqiang LU , Kelu WANG , Xin LI , Shibiao LIU . A NEW METHOD FOR SIMULATING AND PREDICT- ING DYNAMIC RECRYSTALLIZATION IN METAL FORGING[J]. Acta Metall Sin, 2014 , 50(9) : 1128 -1136 . DOI: 10.11900/0412.1961.2014.00142
| [1] | Lee C H, Kobayashi S. J Eng Ind, 1973; 95: 865 |
| [2] | Yue C X, Zhang L W, Liao S L, Gao H J. Comp Mater Sci, 2009; 45: 462 |
| [3] | Lin Y C, Chen M S. J Mater Process Technol, 2009; 209: 4578 |
| [4] | Reza R, Siamak S. Mater Des, 2007; 28: 2366 |
| [5] | Yeom J T, Lee C S, Kim J H, Park N K. Mater Sci Eng, 2007; A449-451: 722 |
| [6] | Serajzadeh S. Int J Mach Tool Manuf, 2003; 43: 1487 |
| [7] | Wang K L, Fu M W, Lu S Q, Li X. Mater Des, 2011; 32: 1283 |
| [8] | Gegel H L. In: Cinicnnati O H, Chen C C eds., Proc Symp on Experimental Verification of Process Models, Materials Park, Ohio: ASM, 1983: 25 |
| [9] | Prasad Y V, Gegel H L, Doraivelu S M, Malas J C, Morgan J T, Lark K A, Brarker D R. Metall Trans, 1984; 15A: 1883 |
| [10] | Gegel H L. Synthesis of Atomistics and Continuum Modeling to Describe Microstructure: Computer Simulation in Materials Science.?Materials Park, Ohio: ASM, 1986: 291 |
| [11] | Malas J C, Seetharaman V. JOM-J Min Met Mater Soc, 1992; 48: 8 |
| [12] | Alexander J M. Modelling of Hot Deformation of Steels. Berlin: Springer Verlag, 1989: 105 |
| [13] | Sun Y, Zeng W D, Ma X, Xu B, Liang X B, Zhang J W. Intermetallics, 2011; 19: 1014 |
| [14] | Peng W P, Li P J, Zeng P, Lei L P. Mater Sci Eng, 2008; A494: 173 |
| [15] | Luo J, Li M Q, Yu W X. Mater Sci Eng, 2009; A504: 90 |
| [16] | Wang K L, Lu S Q, Fu M W, Li X, Dong X J. Mater Sci Eng, 2010; A527: 7279 |
| [17] | Lu S Q, Li X, Wang K L, Dong X J, Li Z X, Cao C X. Chin J Mech Eng, 2007; 43(8): 77 |
| [17] | (鲁世强, 李 鑫, 王克鲁, 董显娟, 李臻熙, 曹春晓. 机械工程学报, 2007; 43(8): 77) |
| [18] | Murty S V, Rao B N. J Mater Process Technol, 2000; 104: 103 |
| [19] | Prasad Y V, Sastry D H, Deevi S C. Intermetallics, 2000; 8: 1067 |
| [20] | Prasad Y V, Sasidhara S. Hot Working Guide: A Compendium of Processing Maps. Ohio: ASM International, The Materials Information Society, 1997: 2 |
| [21] | Lu S Q, Li X, Wang K L, Dong X J, Fu M W. Trans Nonferrous Met Soc China, 2013; 23: 353 |
| [22] | Wang K L, Lu S Q, Fu M W, Li X, Dong X J. Mater Charact, 2009; 60: 492 |
| [23] | Li X, Lu S Q, Wang K L, Zhao W G, Li Z X, Cao C X. Acta Metall Sin, 2007; 43: 1268 |
| [23] | (李 鑫, 鲁世强, 王克鲁, 赵为纲, 李臻熙, 曹春晓. 金属学报, 2007; 43: 1268) |
| [24] | Rollett A D, Jonas J J. Acta Mater, 1996; 44: 127 |
| [25] | Prasad G V, Goerdeler M, Cottstein G. Mater Sci Eng, 2005; A400-401: 231 |
| [26] | Ouyang D L, Lu S Q, Cui X, Dong X J, Wu C, Qiu W. J Aeronaut Mater, 2010; 30(2): 17 |
| [26] | (欧阳德来, 鲁世强, 崔 霞, 董显娟, 吴 超, 邱 伟. 航空材料学报, 2010; 30(2): 17) |
/
| 〈 |
|
〉 |