RESEARCH OF THE MAGNETOCALORIC PROPER- TIES IN Mn1.2Fe0.8P0.74Ge0.26-xSex COMPOUNDS

  • Shaobo WANG ,
  • Danmin LIU ,
  • Weiqiang XIAO ,
  • Zhenlu ZHANG ,
  • Ming YUE ,
  • Jiuxing ZHANG
Expand
  • 1 Institute of Microstructure and Property of Advanced Materials, Beijing University of Technology, Beijing 100124
    2 College of Materials Science and Engineering, Beijing University of Technology, Beijing 100124

Revised date: 2014-01-27

  Online published: 2014-09-25

Supported by

Supported by National Natural Science Foundation of China (Nos.51071007 and 51171003) and Key Research Project of Beijing Municipal Commission of Education (No.KZ201410005005)

Abstract

Magnetic refrigeration based on the magnetocaloric effect offers a potential energy saving, atmosphere friendly way to replace vapor-compression refrigeration. In this work, Mn1.2Fe0.8P0.74Ge0.26-xSex (x=0, 0.005, 0.01, 0.015, 0.02, 0.03) compounds were prepared by mechanical milling and subsequent spark plasma sintering (SPS) technique, their crystal structures, phase transition process and magnetocaloric properties were investigated by XRD, DSC, VSM and direct measurement equipment of magnetocaloric effect. The results show that the Mn1.2Fe0.8P0.74Ge0.26-xSex compounds possess a hexagonal Fe2P-type crystal structure. With increasing Se concentration, the lattice parameters a and c change significantly. It causes c/a ratio decreases firstly, keeps unchanging and followed by increasing again. And the Curie temperature (Tc) of the compounds is increased with the decrease of the c/a ratio. Either applied magnetic field or temperature change can induce the magnetic transformation between the paramagnetic phase and ferromagnetic phase. Low substitution of Se for Ge (x≤0.015) in the Mn1.2Fe0.8P0.74Ge0.26-xSex compounds leads to higher Tc, narrower temperature range of the two-phase coexistence (?Tcoex) and larger adiabatic temperature change (?Tad), in addition the thermal hysteresis (?Thys) and entropy change (?SDSC) remain almost unaffected. 0.01 Se substitution leads to 5.6 K increase in Tc, 10.6% decrease in ?Tcoex, and 10% increase in ?Tad. With a further increase in Se content, magnetocaloric properties of compound decrease.

Cite this article

Shaobo WANG , Danmin LIU , Weiqiang XIAO , Zhenlu ZHANG , Ming YUE , Jiuxing ZHANG . RESEARCH OF THE MAGNETOCALORIC PROPER- TIES IN Mn1.2Fe0.8P0.74Ge0.26-xSex COMPOUNDS[J]. Acta Metall Sin, 2014 , 50(9) : 1109 -1114 . DOI: 10.11900/0412.1961.2014.00059

References

[1] Cam Thanh D T, Brück E, Tegus O, Klaasse J C P, Gortenmulder T J, Buschow K H J. J Appl Phys, 2006; 99: 08Q107
[2] Yan A, Müller K H, Schultz L,Gutfleisch O. J Appl Phys, 2006; 99: 08K903
[3] Dagula W, Tegus O, Fuquan B, Zhang L, Si P Z, Zhang M, Zhang W S, Brück E,de Boer F R, Buschow K H J. IEEE Trans Magn, 2005; 41: 2778
[4] Ou Z Q, Wang G F, Lin S, Tegus O, Brück E, Buschow K H J. J Phys: Condens Matter, 2006; 18: 11577
[5] Tegus O, Fuquan B, Dagula W, Zhang L, Brück E, Si P Z,de Boer F R, Buschow K H J. J Alloys Compd, 2005; 396: 6
[6] Yue M, Li Z Q, Wang X L, Liu D M, Zhang J X, Liu X B. J Appl Phys, 2009; 105: 07A915
[7] Pecharsky V K, Gschneidner K A. Phys Rev Lett, 1997; 78: 4494
[8] Hu F X, Shen B G, Sun J R. Appl Phys Lett, 2001; 78: 3675
[9] Chen W, Zhong W. J Funct Mater, 1998; 29: 236
[9] (陈 伟, 钟 伟. 功能材料, 1998; 29: 236)
[10] Tegus O, Bruck E, Buschow K H J,de Boer F R. Nature, 2002; 415: 150
[11] Tegus O, Brück E, Li X W, Zhang L, Dagula W, de Boer F R, Buschow K H J. J Magn Magn Mater, 2004; 272: 2389
[12] Brück E, Kamarad J, Sechovsky V, Arnold Z, Tegus O, de Boer F R. J Magn Magn Mater, 2007; 310: e1008
[13] Trung N T, Qu Z Q, Gortenmulder T J, Tegus O, Buschow K H J, Brück E. Appl Phys Lett, 2009; 94: 102513
[14] Wang G F, Song L, Li F A, Ha S C L, Li X W, Tegus O. Acta Metall Sin, 2008; 43: 889
[14] (王高峰, 松 林, 李福安, 哈斯朝鲁, 李新文, 特古斯. 金属学报, 2008; 43: 889)
[15] Geng Y X, Tegus O. J Magn Mater Dev, 2011; 42(5): 17
[15] (耿遥祥, 特古斯. 磁性材料及器件, 2011; 42(5): 17)
[16] Ha S C L, Ning J, He X L, Yi R L T, Song L, Tegus O, Huang J H. J Magn Mater Dev, 2010; 41(4): 24
[16] (哈斯朝鲁, 宁 君, 何小龙, 伊日勒图, 松 林, 特古斯, 黄焦宏. 磁性材料及器件, 2010; 41(4): 24)
[17] Liu Y J, Geng Y X, Tegus O,Ha S C L, Song Z Q, Hai S, Li S. J Inner Mongolia Normal Univ, 2012; 41: 368
[17] (刘雨江, 耿遥祥, 特古斯, 哈斯朝鲁, 宋志强, 海 山, 利 胜. 内蒙古师范大学学报, 2012; 41: 368)
[18] Wang D M, Song L, Wang Y H, Zhang W, Geng Y X, Tegus O. Rare Met, 2012; 36: 87
[18] (王冬梅, 松 林, 王耀辉, 张 伟, 耿遥祥, 特古斯. 稀有金属, 2012; 36: 87)
[19] Wang D M, Song L, Wang Y H, Zhang W, Bi L G, Tegus O. Acta Metall Sin, 2011; 47: 344
[19] (王冬梅, 松 林, 王耀辉, 张 伟, 毕力格, 特古斯. 金属学报, 2011; 47: 344)
[20] Liu D M, Huang Q Z, Yue M, Lynn J W, Liu L J, Chen Y, Wu Z H, Zhang J X. Phys Rev, 2009; 80B: 174415
[21] Liu D M, Yue M, Zhang J X, McQueen T M, Lynn J W, Wang X L, Chen Y, Li J Y, Cava R J, Liu X B, Altounian Z, Huang Q. Phys Rev, 2009; 79B: 014435
[22] Gercsi Z, Delczeg-Czirjak E K, Vitos L, Wills A S, Daoud-Aladine A, Sandeman K G. Phys Rev, 2013; 88B: 024417
[23] Delczeg-Czirjak E K, Gercsi Z, Bergqvist L, Eriksson O, Szunyogh L, Nordblad P, Johansson B, Vitos L. Phys Rev, 2012; 85B: 224435
[24] Xu H, Yue M, Zhao C, Zhang D T, Zhang J X. Rare Met, 2012; 31: 336
[25] Zhang L, Liu D M, Deng X J, Yue M, Zhang J X. J Funct Mater, 2011; 42: 1951
[25] (张 雷, 刘丹敏, 邓晓军, 岳 明, 张久兴. 功能材料, 2011; 42: 1951)
[26] Yue M, Liu D M, Huang Q Z, Wang T, Hu F X, Li J B, Rao G H, Shen B G, Lynn J W, Zhang J X. J Appl Phys, 2013; 113: 043925
[27] Zhang M, Liu D M, Liu C X, Huang Q Z, Wang S B, Zhang H, Yue M. Acta Metall Sin, 2013; 49: 783
[27] (张 孟, 刘丹敏, 刘翠秀, 黄清镇, 王少博, 张 虎, 岳 明. 金属学报, 2013; 49: 783)
[28] Liu L J. Master Thesis, Beijing University of Technology, 2009
[28] (刘立江. 北京工业大学硕士学位论文, 2009)
Outlines

/

〈 〉