OXIDATION PROPERTY AND FAILURE MECHANISM OF A SINGLE PHASE PtAl2 COATING

  • Quan LIU ,
  • Yingfei YANG ,
  • Zebin BAO ,
  • Shenglong ZHU ,
  • Fuhui WANG
Expand
  • State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Revised date: 2014-02-10

  Online published: 2014-09-25

Supported by

Supported by National Natural Science Foundation of China (No.51301184), National Basic Research Program of China (No.2012CB625100) and High Technology Research and Development Program of China (No.2012AA03A512)

Abstract

Pt-modified aluminide coating has attracted great attention due to its advantage of the integrated property in resisting both high temperature oxidation and hot corrosion. By the presence of Pt, the spallation trend of the grown oxide scale and the detrimental effect of S can be restrained at a very low level. Besides, Pt could promote α-Al2O3 formation and stabilize β-NiAl phase. Thus Pt-modified aluminide (Pt-Al) coating has been widely used in some crucial applications requiring reliability and extended service life. There are mainly PtAl2, β-(Ni, Pt)Al and γ/γ ′-NiPtAl phases existing inside Pt-Al coating. In this work, a single phase PtAl2 coating was prepared on a Ni-based K38G superalloy through pulse-electroplating of Pt and pack aluminization under stepped heating mode. At 1100 ℃ , the isothermal oxidation behavior of the single phase PtAl2 coating was evaluated by thermogravimetric analysis (TGA). Cyclic oxidation test of the PtAl2 coating was performed within a vertical muffle furnace at the same temperature. The results indicate that the singular PtAl2 coating possesses quite good isothermal oxidation resistance. However, its resistance against cyclic oxidation is very poor. The cyclic stress induced by repeated heating and cooling has caused visible detachment of PtAl2 coating layer, and the spallation of PtAl2 in further would lead to a premature failure of the whole coating system. Partial spallation of PtAl2 layer, including undesirable consumption of Al inside β-NiAl nearby the spallation acts the main reason responsible for the final failure. Accordingly, it is not appropriate to apply single phase PtAl2 coating in the high temperature services involving stress and load. The degradation mechanism of the singular PtAl2 coating is investigated by discussing the stress generated from cyclic heating and cooling.

Cite this article

Quan LIU , Yingfei YANG , Zebin BAO , Shenglong ZHU , Fuhui WANG . OXIDATION PROPERTY AND FAILURE MECHANISM OF A SINGLE PHASE PtAl2 COATING[J]. Acta Metall Sin, 2014 , 50(9) : 1102 -1108 . DOI: 10.11900/0412.1961.2014.00064

References

[1] Padture N P, Gell M, Jordan E H. Science, 2002; 296: 280
[2] Cape T. US Pat, 3102004, 1963
[3] Boone D H, Deb P, Purivs L I, Rigney D V. J Vac Sci Technol, 1985; 3: 2557
[4] Boone D H, Streiff R. J Vac Sci Technol, 1985; 3: 2578
[5] Deb P, Boone D H, Manley T F. J Vac Sci Technol, 1987; 5: 3366
[6] Bai L X, Lou H Y, Wu W T. Mater Prot, 1988; 1: 11
[6] (白林祥, 楼翰一, 吴维弢. 材料保护, 1988; 1: 11)
[7] Bai L X, Wu W T. Precious Met, 1995; 16: 24
[7] (白林祥, 吴维弢. 贵金属, 1995; 16: 24)
[8] Liu G, Niu Y, Wang W, Wu W T. J Chin Soc Corros Prot, 2001; 21: 54
[8] (刘 刚, 牛 焱, 王 文, 吴维弢. 中国腐蚀与防护学报, 2001; 21: 54)
[9] Das D K, Singh V, Joshi S V. Metall Mater Trans, 2000; 31A: 2037
[10] Das D K, Singh V, Joshi S V. Oxid Met, 2002; 57: 245
[11] Vialas N, Monceau D. Surf Coat Technol, 2006; 201: 3846
[12] Angenete J, Stiller K. Surf Coat Technol, 2002; 150: 107
[13] Angenete J, Stiller K, Bakchinova E. Surf Coat Technol, 2004; 176: 272
[14] Hong S J, Kim Y D, Lee G H, Cho I S, Lee C S, Kang S G. Intermetallics, 2014; 46: 65
[15] Hopkin N, Wilson L F. Platinum Met Rev, 1960; 4: 56
[16] Shi G M, Zhang Z L, Shi F L, Yan X F. Mater Heat Treat, 2012; 41: 159
[16] (施国梅, 张尊礼, 史凤玲, 闫秀芬. 材料热处理技术, 2012; 41: 159)
[17] Gleeson B, Wang W, Hayashi S, Sordelet D J. Mater Sci Forum, 2004; 461-464: 213
[18] Hayashi S, Wang W, Sordelet D J, Gleeson B. Metall Mater Trans, 2005; 36A: 1769
[19] Lou H Y, Wang F H, Xia B J, Zhang L X. Corros Sci Prot Technol, 1993; 5: 101
[19] (楼翰一, 王福会, 夏邦杰, 张立新. 腐蚀科学与防护技术, 1993; 5: 101)
[20] Lou H Y, Wang F H, Zhu S L, Xia B J, Zhang L X. Surf Coat Technol, 1994; 63: 105
[21] Benoist J, Badawi K F, Malié A, Ramade C. Surf Coat Technol, 2005; 194: 48
[22] Wright P K. Mater Sci Eng, 1998; A245: 191
[23] Preis W, Sitte W. Solid State Ionics, 2008; 179: 765
[24] Chung Y C, Kim C K, Wuensch B J. J Appl Phys, 2000; 87: 2747
[25] Wen M, Jiang D H, Chen Z Q, Li Y Q, Zhang J M, Zhang K H, Hua W M. Precious Met, 2010; 31: 16
[25] (闻 明, 姜东慧, 陈志全, 李燕琼, 张俊敏, 张昆华, 华伟明. 贵金属, 2010; 31: 16)
[26] Bao Z B, Wang Q M, Li W Z, Liu X, Gong J, Xiong T Y, Sun C. Corros Sci, 2009; 51: 860
[27] Bao Z B, Wang Q M, Jiang S M, Gong J, Sun C. Corros Sci, 2008; 50: 2372
[28] Moretto P, Bressers J, Arrell D J. Mater Sci Eng, 1999; A272: 310
Outlines

/

〈 〉