Fe THIN FILMS GROWN ON SURFACE OF SrFe12O19 BY MOCVD METHOD AND ITS ABSORBING PROPERTIES

  • Yuan LIU ,
  • Xiangxuan LIU ,
  • Xuanjun WANG ,
  • Xin CHEN
Expand
  • No.603 Faculty, Xi'an Research Institute of High Technology, Xi'an 710025

Revised date: 2013-11-27

  Online published: 2014-09-25

Abstract

Nowadays, more and more researchers pay attention to the microwave absorbing materials with the increase of electromagnetic pollution and the development of stealth technology for military platforms. Traditional microwave absorbers, such as ferrite, metal powder, conductive magnetic fibers, magnetic flake powder, and nanoparticles and so on, are facing some common problems such as large specific gravity, narrow absorption bandwidth, large match thickness and poor absorption performance. Composites with core-shell structures are becoming promising microwave absorbing material because such structure can exhibit magnetic and dielectric characteristics through the proper selection of core and shell materials. Thus, Fe(CO)5 deposition on the SrFe12O19 surface has been considered for the fabrication of a new composite that possesses the advantages of these two materials. This new composite might also obtain remarkable microwave absorption through thin layer absorbers in the entire 2~18 GHz frequency range. The Fe-SrFe12O19 composites with core-shell structures were prepared by metal organic chemical vapor deposition (MOCVD) using the SrFe12O19 and iron pentacarbonyl [Fe(CO)5] as the precursors. XRD, SEM, EDS and a vector network analyzer were used to characterize the structure and electromagnetic properties of the samples. The structure and morphology analyses show that the composites have complete core-shell structures with SrFe12O19 as core and Fe layers as shell. Fe nanoparticles were uniformly deposited on the surface of SrFe12O19 with thickness of about 0.5 mm at the reaction temperature of 180 ℃ with N2 flow rate of 30 mL/min for 30 min. Simulation studies show that SrFe12O19 electromagnetic properties changed significantly and the absorbing properties got evidently improvement after Fe deposited on its surface. The samples prepared with deposition time of 30 min have the best absorbing properties. A reflection loss (RL) value exceeding -10 dB in the range of 6.8~18.0 GHz frequency was obtained by selecting an appropriate thickness of the absorber layer from 1.5 to 3.0 mm. Moreover, a minimum RL of -21.2 dB at was obtained for a 2.0 mm thick layer. Fe-deposited SrFe12O19 by MOCVD can significantly improve the electromagnetic properties of SrFe12O19 and Fe-SrFe12O19 composites could be used as an effective microwave absorption material.

Cite this article

Yuan LIU , Xiangxuan LIU , Xuanjun WANG , Xin CHEN . Fe THIN FILMS GROWN ON SURFACE OF SrFe12O19 BY MOCVD METHOD AND ITS ABSORBING PROPERTIES[J]. Acta Metall Sin, 2014 , 50(9) : 1095 -1101 . DOI: 10.11900/0412.1961.2013.00774

References

[1] Huang Y B, Qian J S, Zhang J Y. J Chin Coal Soc, 2010; 35: 135
[1] (黄煜镔, 钱觉时, 张建业. 煤炭学报, 2010; 35: 135)
[2] Hirata A, Morita M, Shiozawa T. IEEE Trans Electromagn, 2003; 45C: 109
[3] Liu Y, Liu X X, Wang X J, Zhang Z Y, Li R, Guo L. Chin J Nonferrous Met, 2013; 23: 168
[3] (刘 渊, 刘祥萱, 王煊军, 张泽洋, 李 茸, 郭 磊. 中国有色金属学报, 2013; 23: 168)
null ?Zhou J, Wang W, Sun Z G, Gong J G. Acta Metall Sin, 2010; 46: 967
null (周 静, 王 维, 孙志刚, 宫建国. 金属学报, 2010; 46: 967)
[5] Liu Y, Liu X X, Wang X J, Chen X. J Chin Ceram Soc, 2013; 41: 755
[5] (刘 渊, 刘祥萱, 王煊军, 陈 鑫. 硅酸盐学报, 2013; 41: 755)
[6] Wang Y F, Li Q L, Zhang C R, Jing H X. J Alloys Compd, 2009; 467: 284
[7] Yao X B, Hu G G, Yin P, Fang Q Q, Lv Q R. Funct Mater, 2002; 33: 633
[7] (姚学标, 胡国光, 尹 萍, 方庆清, 吕庆荣. 功能材料, 2002; 33: 633)
[8] Jing H X, Li Q L, Ye Y, Yang X F. Acta Mater Comp Sin, 2013; 30: 130
[8] (景红霞, 李巧玲, 叶 云, 杨晓峰. 复合材料学报, 2013; 30: 130)
[9] Liu Y, Liu X X, Wang X J. J Alloys Compd, 2014; 584: 249
[10] Tong G X, Gong J G, Zhang W Y, Zhang W, Wang W, Dong D M. Acta Metall Sin, 2008; 44: 1001
[10] (童国秀, 宫建国, 张五一, 张 巍, 王 维, 董德明. 金属学报, 2008; 44: 1001)
[11] Liu Y, Liu X X, Wang X J, Wen W. Chin Phys Lett, 2014; 31: 047702
[12] Cheng Y L, Dai J M, Wu Y P. J Magn Magn Mater, 2010; 32: 97
[13] Pan X F, Mu G H, Shen H G, Gu M Y. Appl Surf Sci, 2007; 253: 4119
[14] Pan X F, Shen H G, Qiu J X, Gu M Y. Mater Chem Phys, 2007; 101: 505
[15] Pan X F, Shen H G, Qiu J X, Gu M Y. J Mater Sci, 2007; 42: 2086
[16] Zhang Z Y, Liu X X, Wang X J, Wu Y P, Liu Y. J Magn Magn Mater, 2012; 324: 2177
[17] Zhang Z Y, Liu X X, Wang X J, Wu Y P, Rong L. J Alloys Compd, 2012; 525: 114
[18] Zhang S Y, Cao Q X. Mater Sci Eng, 2012; B177: 678
[19] Liu Y, Liu X X, Chen X, Wang X J. J Inorg Mater, 2013; 28: 1328
[19] (刘 渊, 刘祥萱, 陈 鑫, 王煊军. 无机材料学报, 2013; 28: 1328)
[20] Yang Y, Xu C L, Xia Y X, Wang T, Li F S. J Alloys Compd, 2010; 493: 549
[21] Zhang B S, Feng Y, Xiong J, Yang Y, Lu H X. IEEE Trans Magn, 2006; 42: 1778
[22] Naito Y, Suetake K. IEEE Trans Microwave Theory Technol, 1971; 19: 65
[23] Meshram M R, Agrawal N K, Sinha B, Misra P S. J Magn Magn Mater, 2004; 271: 207
[24] Maeda T, Sugimoto S, Kagotani T, Tezuka N, Inomata K. J Magn Magn Mater, 2004; 281: 195
Outlines

/