HOT DEFORMATION BEHAVIOR OF BLADES STEEL 10Cr12Ni3Mo2VN FOR ULTRA- SUPERCRITICAL UNITS
Revised date: 2013-12-30
Online published: 2014-09-25
Supported by
Supported by National High Technology Research and Development Program of China(No.2012AA03A502)
10Cr12Ni3Mo2VN steel is mainly made by forging and usually used to make last stage blades of ultra-supercritical unit, demanding strict standards of microstructure property because of its hard service environment, so it is necessary to conduct deep research on its hot deformation behavior. The hot deformation behavior of 10Cr12Ni3Mo2VN steel was investigated through high temperature compression tests on the Gleeble-1500 thermal-mechanical simulator at 850~1200 ℃ and strain rate range of 0.01~10 s-1. The results show that dynamic recrystallization becomes more prone to happen and recrystallized grain size increases with increasing temperature and decreasing strain rate. Isometric crystal and mixed structure appear after compressed 60% at 1200 ℃ with high and low strain rate respectively. A new method of establishing the hot deformation hyperbolic sine constitutive equation by Levenberg-Marquardt algorithm is proposed. Parameters of the constitutive equations established by traditional linear fitting and Levenberg-Marquardt algorithm have a similar value, and both of the constitutive equations have a high prediction precision, so the method of establishing constitutive equation by Levenberg-Marquardt algorithm is credible. However, Levenberg-Marquardt algorithm can get all parameters at the same time with fewer and simpler steps compared to traditional linear fitting. In addition, the values of critical strain for dynamic recrystallization initiation are determined from the work hardening rate-strain curves and a model related to Zener-Hollomon parameter for predicting critical and peak strain under different deformation paraments is established.
Junru LI , Chen GONG , Lie CHEN , Hui ZUO , Yazheng LIU . HOT DEFORMATION BEHAVIOR OF BLADES STEEL 10Cr12Ni3Mo2VN FOR ULTRA- SUPERCRITICAL UNITS[J]. Acta Metall Sin, 2014 , 50(9) : 1063 -1070 . DOI: 10.11900/0412.1961.2013.00848
| [1] | Xie X L, Yang G, Chen J C, Yang G X, Fan H. Heat Treat, 2009; 24(5): 35 |
| [1] | (谢学林, 杨 钢, 陈敬超, 杨功显, 范 华. 热处理, 2009; 24(5): 35) |
| [2] | Masuyama F. ISIJ Int, 2001; 41: 612 |
| [3] | McQueen H J. Mater Sci Eng, 2004; A387: 203 |
| [4] | Fernández A I, Uranga P, Lopez B, Rodriguez-Ibabe J M. Mater Sci Eng, 2003; A361: 367 |
| [5] | Quan G Z, Li G S, Chen T, Wang Y X, Zhang Y W, Zhou J. Mater Sci Eng, 2011; A528: 4643 |
| [6] | Chen M S, Lin Y C, Ma X S. Mater Sci Eng, 2012; A556: 260 |
| [7] | Cao J R, Liu Z D, Cheng S C, Yang G, Xie J X. Acta Metall Sin, 2007; 43: 35 |
| [7] | (曹金荣, 刘正东, 程世长, 杨 钢, 谢建新. 金属学报, 2007; 43: 35) |
| [8] | Wu L Z, Li X S, Chen J, Zhang H B, Cui Z S. J Iron Steel Res Int, 2010; 17(7): 51 |
| [9] | Tan Z L, Xiang S. Trans Mater Heat Treat, 2013; 34(5): 42 |
| [9] | (谭智林, 向 嵩. 材料热处理学报, 2013; 34(5): 42) |
| [10] | Wei J, Tang G B, Liu Z D. J Iron Steel Res, 2008; 20(3): 31 |
| [10] | (魏 洁, 唐广波, 刘正东. 钢铁研究学报, 2008; 20(3): 31) |
| [11] | Dehghan-Manshadi A, Barnett M R, Hodgson P D. Metall Mater Trans, 2008; 39A: 1359 |
| [12] | Song R B, Zhang Y K, Wen X L, Jia Y S. Acta Metall Sin, 2011; 47: 34 |
| [12] | (宋仁伯, 张永坤, 文新理, 贾翼速. 金属学报, 2011; 47: 34) |
| [13] | Wei H L, Liu G Q, Xiao X, Zhang M H. Acta Metall Sin, 2013; 49: 731 |
| [13] | (魏海莲, 刘国权, 肖 翔, 张明赫. 金属学报, 2013; 49: 731) |
| [14] | Chen L, Wang L M, Du X J, Liu X. Acta Metall Sin, 2010; 46: 52 |
| [14] | (陈 雷, 王龙妹, 杜晓建, 刘 晓. 金属学报, 2010; 46: 52) |
| [15] | Wang Z X, Liu X F, Xie J X. Acta Metall Sin, 2008; 44: 1378 |
| [15] | (王智祥, 刘雪峰, 谢建新. 金属学报, 2008; 44: 1378) |
| [16] | McQueen H J, Ryan N D. Mater Sci Eng, 2002; A322: 43 |
| [17] | Jia B, Peng Y. Acta Metall Sin, 2011; 47: 507 |
| [17] | (贾 斌, 彭 艳. 金属学报, 2011; 47: 507) |
| [18] | Cao Y, Di H S, Zhang J Q, Ma T J, Zhang J C. Acta Metall Sin, 2013; 49: 811 |
| [18] | (曹 宇, 邸洪双, 张敬奇, 马天军, 张洁岑. 金属学报, 2013; 49: 811) |
| [19] | Kim S I, Yoo Y C. Mater Sci Eng, 2001; A311: 108 |
| [20] | Jonas J J, Quelennec X, Jiang L, Martin é. Acta Mater, 2009; 57: 2748 |
| [21] | Dehghan-Manshadi A, Barnett M R, Hodgson P D. Mater Sci Eng, 2008; A485: 664 |
| [22] | Belyakov A, Miura H, Sakai T. Mater Sci Eng, 1998; A255: 139 |
| [23] | El Wahabi M, Cabrera J M, Prado J M. Mater Sci Eng, 2003; A343: 116 |
| [24] | Cho J R, Jeong H S, Cha D J, Bae W B, Lee J W. J Mater Process Technol, 2005; 160: 1 |
| [25] | Poliak E I, Jonas J J. Acta Mater, 1996; 44: 127 |
| [26] | Laasraoui A, Jonas J J. Metall Trans, 1991; 22A: 1545 |
/
| 〈 |
|
〉 |