EFFECT OF Hf ON THE INTERFACIAL REACTION BETWEEN A NICKEL BASE SUPERALLOY AND A CERAMIC MATERIAL

  • Xiaoyan CHEN ,
  • Yizhou ZHOU ,
  • Chaowei ZHANG ,
  • Tao JIN ,
  • Xiaofeng SUN
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2014-01-16

  Revised date: 2014-03-20

  Online published: 2014-08-25

Supported by

Supported by National Natural Science Foundation of China (Nos.U1037601, 51271186, 51331005, 11332010 and 51001103), National Basic Research Program of China (No.2010CB631206), Fund of the State Key Labortary of Advanced Technologies for Comprehensive Utilization of Platinum Metals (No.SKL-SPM-201213)

Abstract

The influence of Hf content on the wettability and interfacial reaction between a nickel base superalloy and a ceramic material was investigated by using a sessile drop method. The wetting angle was measured through the geometric parameters of the metal drop. The interfacial morphology and elements distribution were studied by SEM and EPMA, respectively. XPS was employed to study the phase formation at the metal-ceramic interface. The relationship between wettability and interfacial reaction was discussed. It was found that the wetting angle of the metal drop on the ceramic substrate was decreased with increasing Hf content in the alloy and the wettability of the studied superalloy on the ceramic material was enhanced with increasing Hf content in the alloy. When the content of Hf increased from 0.1% to 2.0% (mass fraction), the wetting angle decreased from 132° to 112°. The interfacial reaction led to a sharp decrease in wetting angle as Hf content was 1.5%. The product of interfacial reaction was HfO2 and the thermodynamic analysis indicated that Hf was able to substitute Si in SiO2 in the ceramic material.

Cite this article

Xiaoyan CHEN , Yizhou ZHOU , Chaowei ZHANG , Tao JIN , Xiaofeng SUN . EFFECT OF Hf ON THE INTERFACIAL REACTION BETWEEN A NICKEL BASE SUPERALLOY AND A CERAMIC MATERIAL[J]. Acta Metall Sin, 2014 , 50(8) : 1019 -1024 . DOI: 10.11900/0412.1961.2014.00033

References

[1] Jones S, Yuan C. J Mater Process Technol, 2003; 135: 258
[2] Duarte T P, Neto R J, Felix R, Lino F J. Mater Sci Forum, 2008; 587-588: 157
[3] Gong R C. Foundry Technol, 2005; 26: 523
[3] (龚荣昌. 铸造技术, 2005; 26: 523)
[4] Mehan R L, Bolan R B. J Mater Sci, 1979; 14: 2471
[5] Slabkii V D, Traktuev O M, Khrulev A A, Yurovskikh Y N. At Energ, 2000; 88: 274
[6] Bruce E T, Michael C. US Pat, 4244551, 1981
[7] Topygo V K, Murphy K S, Clarke D R. Acta Mater, 2008; 56: 489
[8] Orlov M R. Russ Metall, 2008; 1: 70
[9] Xue M. Master Thesis, Qinghua University, Beijing, 2007
[9] (薛 明. 清华大学硕士学位论文, 北京, 2007)
[10] Zheng L, Xiao C B, Zhang G Q, Gu G H, Li X, Liu X G, Xue M, Tang D Z. J Aero Mater, 2012; 32(3): 10
[10] (郑 亮, 肖程波, 张国庆, 顾国红, 李 鑫, 刘晓光, 薛 明, 唐定中. 航空材料学报, 2012; 32(3): 10)
[11] Yao J S. Master Thesis, Tian Jin University, 2008
[11] (姚建省.天津大学硕士学位论文, 2008)
[12] Li R J. Ceramics-Metal Composites. 2nd Ed., Beijing: Metallurgical Industry Press, 2004: 2
[12] (李荣久. 陶瓷-金属复合材料. 第2版, 北京: 冶金工业出版社,2004: 2)
[13] Young T. Philos Trans, 1805; 95: 65
[14] Ding H S, Fu H Z, Jia J, Guo J J, Li J S. Mater Sci Technol, 2001; 9: 130
[14] (丁宏升, 傅恒志, 贾 均, 郭景杰, 李金山. 材料科学与工艺, 2001; 9: 130)
[15] Sangghaleh A, Halali M. Appl Surf Sci, 2009; 255: 8202
[16] Candan E. J Eng Environ Sci, 2002; 26: 1
[17] Shi Z X, Li J R, Liu S Z. J Iron Steel Res Int, 2012; 19: 66
[18] Hou J S, Guo J T, Wu Y X, Zhou L Z, Ye H Q. Mater Sci Eng, 2010; A527: 1548
[19] Zheng Y R. Aeronaut Mater, 1988; 8(2): 1
[19] (郑运荣. 航空材料, 1988; 8(2): 1)
[20] Li Q, Song J X, Wang D G, Yu Q, Xiao C B. Rare Met, 2011; 30: 405
[21] Aksay I A, Hoge C E, Pask J A. J Phys Chem, 1974; 78: 1178
[22] Eustathopoulos N. Acta Mater, 1998; 46: 2319
[23] Laurent V, Chatain D, Eustathopoulos N. Mater Sci Eng, 1991; A135: 89
[24] Liang Y J. Thermochemical Data of Inorganics. Shenyang: Northeastern University Press, 1993: 19
[24] (梁英教. 无机热力学数据手册. 沈阳: 东北大学出版社, 1993: 19)
Outlines

/

〈 〉