RESEARCH ON THE CORRELATION BETWEEN THE STATUS OF THREE-DIMENSIONAL WELD POOL SURFACE AND WELD PENETRATION IN TIG WELDING

  • Gang ZHANG ,
  • Yu SHI ,
  • Chunkai LI ,
  • Jiankang HUANG ,
  • Ding FAN
Expand
  • State Key Laboratory of Advanced Processing and Recycling of Nonferrous Metals, Lanzhou University of Technology, Lanzhou 730050

Received date: 2013-12-16

  Revised date: 2014-04-22

  Online published: 2014-08-25

Supported by

Supported by National Natural Science Foundation of China (No.61365011), Young Creative Talent Support Program of Long Yuan of China, Specialized Basic Scientific Research Program of University of Gansu Province and Hong Liu Outstanding Talent Training Plan of Lanzhou University of Technology (No.J201201)

Abstract

Measurement of the weld pool surface is a difficult but urgent task in the welding community. It plays an important role in developing the next generation intelligent welding machines, in particular, controlling the weld joint penetration in automatic welding. In this work, the images of front-side free surface and back-side width of the weld pool are synchronously captured with two CCD cameras in tungsten inert gas (TIG) arc welding process based on laser vision, and the three dimensional weld pool surface is reconstructed using designed algorithm. Then, the correlation between the weld pool surface under different weld joint penetration and its back-side width is analyzed qualitatively. The variation of reflected laser dots shape is reversely simulated under different depths of weld pool surface, which represents the different weld joint penetration, after established the standard model of weld pool, incident, reflected ray and imaging plan's mathematical model. It is found that the change of weld pool surface obtained by this method has an intimate immanent correlation with the weld joint penetration. When the weld joint penetration changes from partial penetration to complete joint penetration, the weld pool surface's shape changes from convexity to concave, and its depth is increasing with the increased back-side width. The row curvature of reflected laser dots is diminishing. When the penetration achieves excessive penetration, the depth of the weld pool surface is more rapidly increased, and the row curvature is also increased. The gathered laser dots is drawn back again at parallel direction. The simulated results associate with the measurement very well. The variations of reflected laser dots shape can represent the degree of weld joint penetration. This research lays a good foundation for the control of weld joint penetration using the characteristics of weld pool surface.

Cite this article

Gang ZHANG , Yu SHI , Chunkai LI , Jiankang HUANG , Ding FAN . RESEARCH ON THE CORRELATION BETWEEN THE STATUS OF THREE-DIMENSIONAL WELD POOL SURFACE AND WELD PENETRATION IN TIG WELDING[J]. Acta Metall Sin, 2014 , 50(8) : 995 -1002 . DOI: 10.11900/0412.1961.2013.00819

References

[1] Liu L M, Zhang Z D, Shen Y, Wang L. Acta Metall Sin, 2006; 42: 399
[1] (刘黎明, 张兆栋, 沈 勇, 王 来. 金属学报, 2006; 42: 399)
[2] Mills K C, Keene B J. Int Mater Rev, 1990; 35: 185
[3] Lucas W, Bertaso D, Melton G, Smith J, Balfour C. Weld Int, 2012; 4: 243
[4] Pal K, Pal S K. Mater Manuf Process, 2011; 26: 684
[5] Chokkalingham S, Chandrasekhar N, Vasudevan M. J Intell Manuf, 2012; 23: 1995
[6] Richardson R W, Gutow D A, Anderson R A, Farson D F. Weld J, 1984; 63: 43
[7] Bae K Y, Lee T H, Ahn K C. J Mater Process Technol, 2002; 120: 458
[8] Zhao D B, Chen Q, Chen S B, Wu L. Opt Technol, 2001; 27: 367
[8] (赵冬斌, 陈 强, 陈善本, 吴 林. 光学技术, 2001; 27: 367)
[9] Li L P, Lin T, Chen S B, Yang X Q. J Shanghai Jiaotong Univ, 2006; 40: 898
[9] (李来平, 林 涛, 陈善本, 杨学勤. 上海交通大学学报, 2006; 40: 898)
[10] Mnich C, Al-Bayat F, Debrunner C, Steele J, Vincent T. Proc 2004 Japan-USA Symposium on Flexible Automation, Denver, CO, 2004: 19
[11] Kovacevic R, Zhang Y M. J Manuf Sci Eng, 1997; 119: 161
[12] Kovacevic R, Zhang Y M, Ruan S. J Eng Ind, 1995; 117: 210
[13] Liu M Y. Master Thesis, Harbin Institute of Technology, 2007
[13] (刘鸣宇. 哈尔滨工业大学硕士学位论文, 2007)
[14] Ai X P, Liu N S, Wei Y Q, Hu X. Trans China Weld Inst, 2011; 32(3): 85
[14] (艾孝谱, 刘南生, 魏义庆, 胡 仙. 焊接学报, 2011; 32(3): 85)
[15] Saeed G, Zhang Y M. Meas Sci Technol, 2003; 14: 1671
[16] Song H S, Zhang Y M. Meas Sci Technol, 2007; 18: 3751
[17] Song H S, Zhang Y M. Weld J, 2008; 87: 85-s
[18] Xiao Y H, Denouden G. Weld J, 1993; 72: 428-s
[19] Shi Y, Zhang G, Ma X J, Fan D. Chin J Mech Eng, 2012; 48(24): 28
[19] (石 玗, 张 刚, 马小骥, 樊 丁. 机械工程学报, 2012; 48(24): 28)
[20] Wu C S, Zhao P C. Acta Metall Sin, 2006; 42: 865
[20] (武传松, 赵朋成. 金属学报, 2006; 42: 865)
[21] Zhao M, Wu C S, Chen J. Chin J Mech Eng, 2007; 43(6): 68
[21] (赵 明, 武传松, 陈 姬. 机械工程学报, 2007; 43(6): 68)
[22] He J S, Yang C L, Lin S B, Wang Q L. Mater Sci Technol, 2001; 9(1): 26
[22] (何景山, 杨春利, 林三宝, 王其隆. 材料科学与工艺, 2001; 9(1): 26)
[23] Rokhlin S I, Guu A C. Weld J, 1993; 72: 381-s
[24] Wang Z Z, Zhang Y M, Yang R G. J Manuf Process, 2013; 15: 34
[25] Liu Y K, Zhang W J, Zhang Y M. Weld J, 2013; 92: 313-s
[26] Ma H B, Wei S C. Sensor Rev, 2010; 30: 116
Outlines

/