MECHANICAL BEHAVIOR OF Al-20Mg ALLOY SOLIDIFIED UNDER HIGH PRESSURE

  • Jinchuan JIE ,
  • Chunming ZOU ,
  • Hongwei WANG ,
  • Zunjie WEI
Expand
  • 1 National Key Laboratory of Metal Precision Hot Forming, School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 115110
    2 School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024

Received date: 2013-11-25

  Revised date: 2014-03-15

  Online published: 2014-08-25

Supported by

Supported by National Natural Science Foundation of China (Nos.51171054 and 51001041) and China Postdoctoral Science Foundation (No.2013M530913)

Abstract

Pressure is, like temperature, a basic thermodynamic variable which can be used to alter the matter state. The atom volume, free energy of matter and other physical and chemical properties can be changed due to the application of high pressure. Many interesting materials including superconducting, super-hard, amorphous, nano-materials can be prepared under high pressures. Meanwhile, the application of high pressure during solidification of metallic materials has also attracted much attention of researchers in recent years. However, the understanding of high pressure on alloy solidification behavior is still lacked, and needs more experimental and theoretical investigation. In the present work, the effect of high pressure on solidification microstructure, phase constitution and mechanical properties of Al-20Mg alloy was investigated by OM, XRD and tensile test. Influence of solute distribution on mechanical properties of solid solution was analyzed and the corresponding mechanism was discussed based on the solute strengthening theory. The results showed that the amount of intermetallic compound b-Al3Mg2 decreases and the amount of Al(Mg) solid solution increases in the Al-20Mg alloy solidified under high pressure, resulting in the remarkable enhancement of the mechanical properties. The Al-20Mg alloy is fragile under 1.0×105 Pa. However, it can transform to be a ductile material with elongation of 11% when solidified under 2 and 3 GPa. Meanwhile, its strength can be also greatly improved. The ultimate tensile strength of Al-20Mg alloy solidified under 2 GPa is 8.9 times of that solidified under 1.0×105 Pa. The yield strength of Al-20Mg alloy solidified under 2 GPa is higher than that under 3 GPa. This phenomenon was explained by solute strengthening theory, and proved that the inhomogeneous distribution of Mg solute in the solid solution can enhance the mechanical properties. The fracture characteristic is essentially altered under the condition of high pressure solidification. The Al-20Mg alloy is cleavage fracture under 105 Pa, however, it transforms to the dimple fracture when solidified under 2 and 3 GPa. The present work provides a potential route to improve the mechanical properties of solid solution through the control of solute distribution in the solid solution.

Cite this article

Jinchuan JIE , Chunming ZOU , Hongwei WANG , Zunjie WEI . MECHANICAL BEHAVIOR OF Al-20Mg ALLOY SOLIDIFIED UNDER HIGH PRESSURE[J]. Acta Metall Sin, 2014 , 50(8) : 971 -978 . DOI: 10.11900/0412.1961.2013.00767

References

[1] Mcmillan P F. Nat Mater, 2002; 1: 19
[2] Sharma S M, Sikka S K. Prog Mater Sci, 1996; 40: 1
[3] Zaug J M, Soper A K, Clark S M. Nat Mater, 2008; 7: 890
[4] Liao S C, Mayo W E, Pae K D. Acta Mater, 1997; 45: 4027
[5] Wei Z J, Wang Z L,Wang H W, Cao L. J Mater Sci, 2007; 42: 7123
[6] He D W, He M, Kiminami C S, Kuo K H, Zhang F X, Xu Y F, Wang W K. J Mater Res, 2001; 16: 910
[7] Zhang G Z, Yu X F, Wang X Y, Jia G L, Gao Y Y, Hao Z Y, Guo X B. Acta Metall Sin, 1999; 35: 285
[7] (张国志, 于溪凤, 王向阳, 贾光霖, 高允彦, 郝兆印, 郭学彬. 金属学报, 1999; 35: 285)
[8] Zhang J, Zhang H F, Dong P, Quan M X, Hu Z Q. Acta Metall Sin, 2004; 40: 211
[8] (张 甲, 张海峰, 董 盼, 全明秀, 胡壮麒. 金属学报, 2004; 40: 211)
[9] Canadinc D, Maier H J, Gabor P, May J. Mater Sci Eng, 2008; A496: 114
[10] Cui G R, Ma Z Y, Li S X. Scr Mater, 2008; 58: 1082
[11] Jie J C, Zou C M, Wang H W, Wei Z J. Mater Lett, 2010; 64: 869
[12] Jie J C, Zou C M, Brosh E, Wang H W, Wei Z J, Li T J. J Alloys Compd, 2013; 578: 394
[13] Starink M J, Zahra A M. Acta Mater, 1998; 46: 3381
[14] Zhang D L, Massalski T B, Paruchuri M R. Metall Mater Trans, 1994; 25A: 73
[15] Schoenitz M, Dreizin E L. J Mater Res, 2003; 18: 1827
[16] Scudino S, Sperling S, Sakaliyska M, Thomas C, Feuerbacher M, Kim K B, Ehrenberg H, Eckert J. Acta Mater, 2008; 56: 1136
[17] Scudino S, Sakaliyska M, Surreddi K B, Eckert J. J Alloys Compd, 2009; 483: 2
[18] Mourik P V, Maaswinkel N M, Keijser T H D, Mittemeijer E J. J Mater Sci, 1989; 24: 3779
[19] Vacher P, Boudrahem S. Acta Mater, 2006; 54: 4365
[20] Hall E O. Proceedings Phys Soc London, 1951; 64B: 747
[21] Petch N J. J Iron Steel Inst, 1953; 174: 25
[22] Mukai T, Higashi K, Tanimura S. Mater Sci Eng, 1994; A176: 181
[23] Chen X, Yan J, Karlsson A. Mater Sci Eng, 2006; A416: 139
[24] Deng D. Mater Des, 2009; 30: 359
[25] Lados D A, Apelian D, Wang L. Mater Sci Eng, 2010; A527: 3159
[26] Wang T G, Zhao S S, Hua W G, Li J B, Gong J, Sun C. Mater Sci Eng, 2010; A527: 454
Outlines

/

〈 〉