ANALYSIS ON THE CONSTITUTIVE RELATIONSHIP OF TC18 TITANIUM ALLOY BASED ON THE SOFTENING MECHANISM

  • Houquan LIANG ,
  • Hongzhen GUO ,
  • Yongquan NING ,
  • Zekun YAO ,
  • Zhanglong ZHAO
Expand
  • School of Materials Science and Engineering, Northwestern Polytechnical University, Xi′an 710072

Received date: 2013-12-09

  Revised date: 2014-04-08

  Online published: 2014-07-20

Abstract

The true stress-true strain curves have been attained through the isothermal compression experiment of TC18 titanium alloy. The influence of deformation parameters on the shape of stress-strain curves and peak stress has been analyzed through the working-hardening and dynamic softening effects. The true stress-true strain curves show the similar characteristics under different deformation conditions. However, the peak stress is sensitive to the changes of deformation parameters. The type of dynamic softening mechanisms in hot deformation under certain conditions can be obtained through Poliak-Jonas criterion. The dynamic recrystallization process tends to take place during the deformation with lower strain rates. And the choice of the dynamic softening mechanisms is not sensitive to deformation temperatures. The suitable constitutive models under different softening mechanisms have been constructed based on the traditional Arrhenius equations. With the identification of the dynamic softening mechanisms in hot deformation of TC18 alloy with different conditions, the response of true stress, at strain of 0.7, to the deformation temperatures and strain rates can be described through the proposed models. And the sensitivity coefficient of strain rates and deformation activation energy, of the process with the dynamic recrystallization as the major softening mechanism, are much larger than the ones of process with dynamic recovery.

Cite this article

Houquan LIANG , Hongzhen GUO , Yongquan NING , Zekun YAO , Zhanglong ZHAO . ANALYSIS ON THE CONSTITUTIVE RELATIONSHIP OF TC18 TITANIUM ALLOY BASED ON THE SOFTENING MECHANISM[J]. Acta Metall Sin, 2014 , 50(7) : 871 -878 . DOI: 10.3724/SP.J.1037.2013.00801

References

[1] Moiseyer V N. Titanium Alloys-Russian Aircraft and Aerospace Applications. London: Taylor & Francis Group, 2005: 46
[2] Semiatin S L, Seetharaman V, Weiss I. Mater Sci Eng, 1999; A263: 257
[3] Bruschi S, Poggio S, Quadrini F. Mater Lett, 2004; 58: 3622
[4] Sumantra M, Rakesh V, Sivaprasad P V. Mater Sci Eng, 2007; A500: 114
[5] Cui J H, Yang H, Sun Z C. Rare Metall Mater Eng, 2012; 41: 0397
[6] Li X L. PhD Dissertation, Northwestern Polytechnical University, Xi′an, 2005
[6] (李晓丽. 西北工业大学博士学位论文, 西安, 2005)
[7] Sha W, Savko M. Titanium Alloys: Modelling of Microstructure, Properties and Applications. Cambridge: Woodhead Publishing, 2009: 265
[8] Jia B, Peng Y. Acta Metall Sin, 2011; 47: 507
[8] (贾 斌, 彭 艳. 金属学报, 2011; 47: 507)
[9] Zhang W F, Li X L, Sha W, Yan W, Wang W, Shan Y Y, Yang K. Mater Sci Eng, 2014; A590: 199
[10] Roberts W, Ahlblom B. Acta Metall, 1978; 26: 801
[11] Humphreys F J, Hatherly M. Recrystallization and Related Annealing Phenomena. 2nd Ed., Oxford: Elsevier, 2004: 431
[12] Wang B, Guo H Z, Yao Z K. Forg Stamp Technol, 2006; (6): 106
[12] (王 斌, 郭鸿镇, 姚泽坤. 锻压技术, 2006; (6): 106)
[13] Ouyang D L, Lu S Q, Cui X. J Aero Mater, 2010; 30(2): 17
[13] (欧阳德来, 鲁世强, 崔 霞. 航空材料学报, 2010; 30(2): 17)
[14] Fernández A I, Uranga P, López B, Rodriguez-Ibabe J M. Mater Sci Eng, 2003; A361: 367
[15] Taylor A S, Hodgson P D. Mater Sci Eng, 2011; A528: 3310
[16] McQueen H J, Sue Y, Ryan N D, Fry E J. Mater Process Technol, 1995; 53: 293
[17] Poliak E I, Jonas J J. Acta Mater, 1996; 44: 127
[18] Miura H, Sakai T, Mogawa R, Gottstein G. Scr Mater, 2004; 51: 671
[19] Chen X R, Li H X, Ge M Q, Chen Y H, Hu Y S. Acta Metall Sin, 1997; 33: 1275
[19] (程晓茹, 李虎兴, 葛懋琦, 陈贻宏, 胡衍生. 金属学报, 1997; 33: 1275)
[20] Galindo-Nava E I, Rivera-Díaz-del-Castillo P E J. Scr Mater, 2014; 72-73: 1
[21] Sellars C M, Tegart W J M. Mem Sci Rev Met, 1966; 63: 731
[22] Gottstein G, Kocks U F. Acta Meter, 1983; 31: 175
[23] Mahoney M W. Materials Properties Handbook: Titanium Alloys. Materials Park: ASM International, 1994: 154
[24] Gottstein G,Shvindlerman L S. Grain Boundary Migration in Metals. Boca Raton: CRC Press, 2010: 211
[25] Mao P L, Yang K, Su G Y. Acta Metall Sin, 2001; 37: 40
[25] (毛萍莉, 杨 柯, 苏国跃. 金属学报, 2001; 37: 40)
[26] Sellars C M, Whiteman J A. Acta Meter, 1979; 13: 187
[27] Sargent P M, Ashby M F. Scr Mater, 1982; 16: 1415
Outlines

/

〈 〉