MICROSTRUCTURE AND MECHANICAL PROPERTIES OF A Ni-BASED SUPERALLOY WITH REFINED GRAINS

  • Jinxia YANG ,
  • Yuan SUN ,
  • Tao JIN ,
  • Xiaofeng SUN ,
  • Zhuangqi HU
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2013-11-19

  Revised date: 2014-01-21

  Online published: 2014-07-20

Abstract

A new Ni-based superalloy with the refined grains is to be used in industrial and aircraft turbines because of its high strength and excellent fatigue resistance at lower and medium temperatures (500~800 ℃). The grains with six different sizes have been made by decreasing the pouring temperature from 1460 to 1480 ℃ then 1500 ℃ and adding refiner to alloy and planting seed on the surface of mold. The size of equiaxed crystal grain is reduced to 0.5 mm in the center part of specimen with the columnar crystals in the outside of specimen made by the refining process which is finer than those of traditional process. It has been found that γ' phase and carbide are finer in refined grains than those in the coarse grains made by decreasing the pouring temperature. The room-temperature tensile properties and high cycle fatigue properties of tested alloy are improved with decreasing grain size. The stress-rupture properties are increased under the conditions of 760 ℃ and 662 MPa while are decreased with decreasing the grain size. The grain structure and size are refined by the refining process that dominated the excellent mechanical properties of tested alloy at lower and medium temperatures. However, it is not good for the mechanical properties at high temperatures.

Cite this article

Jinxia YANG , Yuan SUN , Tao JIN , Xiaofeng SUN , Zhuangqi HU . MICROSTRUCTURE AND MECHANICAL PROPERTIES OF A Ni-BASED SUPERALLOY WITH REFINED GRAINS[J]. Acta Metall Sin, 2014 , 50(7) : 839 -844 . DOI: 10.3724/SP.J.1037.2013.00745

References

[1] Ewing B A, Green K A. In: Gell M, Kortovin C S, Bricknell R H, Kent W B, Radavich J F eds., Superalloys, Champion: The Metallergical Society of AIME, 1984: 33
[2] McClean M. Mater Sci Technol, 1988; 4: 205
[3] Bouse G K, Behrend M R. In: Loria E ed., Mechanical Properties of Microcast-X Alloy 718 Fine Grain Investment Castings, Superalloy 718-Metallurgy and Applications, Warrendale, PA: The Metallurgical Society, 1989: 319
[4] Prichard P D, Dalal R P. In: Antolovich S D, Stusrud R W, Mackay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds., Superalloys, Champion: The Metallurgical Society of AIME, 1992: 205
[5] Liu L, Zhen B L, Banerlly A, Relf W. Scr Metall Mater, 1994; 30: 593
[6] Liu L, Huang T, Xiong Y, Yang A, Zhao Z, Zhang R, Li J. Mater Sci Eng, 2005; A394: 1
[7] Xiong Y, Yang A, Guo Y, Liu W, Liu L. Sci Technol Adv Mater, 2001; 2: 13
[8] Xiong Y H, Liu W, Yang A M, Zhang R, Liu L. Acta Metall Sin, 1999; 35: 689
[8] (熊玉华, 柳 伟, 杨爱民, 张 蓉, 刘 林. 金属学报, 1999; 35: 689)
[9] Ma Y, Sun J, Xie X, Hu Y, Zhao J, Yan P. J Mater Sci Technol, 2003; 137: 35
[10] Zhang B, Cui J, Liu G. Mater Sci Eng, 2003; A355: 325
[11] Paul P C, Nasar S A. Introduction of Electromagnetic Fields. New York: McGraw-Hill, 1987: 306
[12] Li T G, Cao Z Q, Jin J Z, Zhang Z F. Mater Trans, 2001; 42: 281
[13] Cao Z Q, Jia F, Zhang X G, Hao H, Jin J Z. Mater Sci Eng, 2002; A327: 133
[14] Zhou J, Xie F X, Wu X Q, Zhang J. Foundry, 2009; 58: 678
[14] (周俊, 谢发勤, 吴向清, 张军. 铸造, 2009; 58: 678)
[15] Zheng J B, Ding J, Guo Y P, Liu L, Liu W, Li X J. Acta Metall Sin, 1998; 34: 362
[15] (郑建邦, 丁 洁, 郭益平, 刘 林, 柳 伟, 李行建. 金属学报, 1998; 34: 362)
[16] Zhao H T, Shi C X. Acta Metall Sin, 1981; 17: 118
[16] (赵慧田, 师昌绪. 金属学报, 1981; 17: 118)
[17] EI-Bagoury N, Nofal A. Mater Sci Eng, 2010; A527: 7793
[18] Hu H Q. Principles of Metal Solidification. Beijing: Machinery Industry Press, 1991: 48
[18] (胡汉起. 金属凝固原理. 北京: 机械工业出版社, 1991: 48)
[19] Herlach D M. Mater Sci Eng, 1994; R12: 177
[20] Peng Z F. Acta Metall Sin, 2002; 23: 135
[20] (彭志方. 金属学报, 2002; 23: 135)
[21] Yin F S. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2003
[21] (殷凤仕. 中国科学院金属研究所博士学位论文, 沈阳, 2003)
[22] Jin W Z, Li J, Li T J, Yin G M. Rare Met Mater Eng, 2008; 37: 1012
[22] (金文中, 李 军, 李廷举, 殷国茂. 稀有金属材料与工程, 2008; 37: 1012)
[23] Qiu H, Qian H C, Samir H A, Wu S M. Foundry Technol, 2004; 25: 265
[23] (邱 华, 钱翰城, Samir H A, 吴仕明. 铸造技术, 2004; 25: 265)
[24] Nilsson J O, Thorvaldsson T. Fatigue Fract Eng Mater Struct, 1985; 8: 4
[25] Leverant G R. Trans Metall Soc AIME, 1969: 245
[26] Liu F X, Yuan W M, Tang X, Yang A D. Acta Metall Sin, 1995; 31(Suppl): S739
[26] (刘发信, 袁文明, 汤 鑫, 杨爱德. 金属学报, 1995; 31(增刊): S739)
Outlines

/