PREPARATION AND CATALYTIC PROPERTIES OF SiC FOAM SUPPORTED Co-BASED STRUCTURED CATALYSTS

  • Xiaodan YANG ,
  • Chunhai JIANG ,
  • Zhenming YANG ,
  • Jinsong ZHANG
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Revised date: 2013-10-21

  Online published: 2014-06-20

Abstract

Co-based structured catalysts were prepared by coating Al-doped Co3O4 powder on SiC foam support using phenolic resin as the adhesion agent, followed by H2 reduction at moderate temperatures. XRD, SEM, N2 adsorption-desorption and H2 adsorption measurement were used to characterize the evolution of crystalline size of Co particles, morphology and phase assemblage of the coatings and the H2 adsorption capacities of the structured catalysts obtained at different reduction temperatures. The catalytic properties of the prepared Co-based structured catalysts were evaluated by taking the hydrolysis of NaBH4 as the model hydrogen generation reaction. Growing of the active Co particles in the coating as accompanied by the increase of crystallinity was observed with the increase of reduction temperature, which resulted in decreased chemical adsorption capacity of H2 at 120 ℃ and catalytic activity towards hydrogen generation rate. The highest hydrogen generation rate of 48.38 mL/(g·min) was achieved at the reduction temperature of 400 ℃.

Cite this article

Xiaodan YANG , Chunhai JIANG , Zhenming YANG , Jinsong ZHANG . PREPARATION AND CATALYTIC PROPERTIES OF SiC FOAM SUPPORTED Co-BASED STRUCTURED CATALYSTS[J]. Acta Metall Sin, 2014 , 50(6) : 762 -768 . DOI: 10.3724/SP.J.1037.2013.00662

References

[1] Shao Q,Long J,He Z F,Tian H P,Duan Q W,Li Y. Orderedly Structured Catalysts and Reactors. Beijing: Chemical Industry Press, 2005: 1
[1] (邵潜,龙军,贺振富,田辉平,段启伟,李阳. 规整结构催化剂及反应器. 北京: 化学工业出版社, 2005: 1)
[2] Cybulski A,Moulijn J A. Structured Catalysts and Reactors. 2nd Ed., New York: CRC Press, 2006: 1
[3] Akdim O, Demirci U B, Brioude A, Miele P. Int J Hydrogen Energy, 2009; 34: 5417
[4] Jeong S U, Kim R K, Cho E A, Kim H J, Nam S W, Oh I H, Hong S A, Kim S H. J Power Sources, 2005; 144: 129
[5] Bai Y, Wu F, Wu C, Yi B L, Zhang H M. Mod Chem Ind, 2006; 26(4): 28
[5] (白莹, 吴峰, 吴川, 衣宝廉, 张华民. 现代化工, 2006; 26(4): 28)
[6] Liu B H, Li Z P, Suda S. J Alloys Compd, 2006; 415: 288
[7] Sch?rringer P, Müller T E, Jentys A, Lercher J A. J Catal, 2009; 263: 34
[8] Sch?rringer P, Müller T E, Lercher J A. J Catal, 2008; 253: 167
[9] Schlesinger H I, Brown H C, Finholt A E, Gilbreath J R, Hoekstra H R, Hyde E K. J Am Chem Soc, 1953; 75: 215
[10] Tsai C W, Chen H M, Liu R S, Lee J F, Chang S M, Weng B J. Int J Hydrogen Energy, 2012; 37: 3338
[11] Xu D, Dai P, Liu X, Cao C, Guo Q. J Power Sources, 2008; 182: 616
[12] Zhang X, Zhao J, Cheng F, Liang J, Tao Z, Chen J. Int J Hydrogen Energy, 2010; 35: 8363
[13] Zhao Y, Ning Z, Tian J, Wang H, Liang X, Nie S, Yu Y, Li X. J Power Sources, 2012; 207: 120
[14] Ma H, Ji W, Zhao J, Liang J, Chen J. J Alloys Compd, 2009; 474: 584
[15] Lee J, Kong K Y, Jung C R, Cho E, Yoon S P, Han J, Lee T G, Nam S W. Catal Today, 2007; 120: 305
[16] Oh T H, Kwon S. Int J Hydrogen Energy, 2013; 38: 6425
[17] Sun L, Song Q H, Hu Z Q. Acta Metall Sin, 1996; 32: 63
[17] (孙笠, 宋启洪, 胡壮麒. 金属学报, 1996; 32: 63)
[18] Sun L, Song Q H, Hu Z Q. Acta Metall Sin, 1995; 31: B341
[18] (孙笠, 宋启洪, 胡壮麒. 金属学报, 1995; 31: B341)
[19] Zhang J S, Cao X M, Hu W P, Yang Y J. Chin Pat, 03134039.3, 2003
[19] (张劲松, 曹小明, 胡宛平, 杨永进. 中国专利, 03134039.3, 2003)
[20] Kondo S,Ishikawa T,Abe I. Translated by Li G X. Adsorption Science. 2nd Ed., Beijing: Chemical Industry Press, 2005: 31
[20] (近藤精一,石川达雄,安部郁夫. 李国希 译. 吸附科学. 第二版, 北京: 化学工业出版社, 2005: 31)
[21] Aristov Y I. Appl Therm Eng, 2013; 50: 1610
[22] Boomsma K, Poulikakos D, Ventikos Y. Int J Heat Fluid Flow, 2003; 24: 825
[23] Tan K K, Sam T, Jamaludin H. Int J Heat Mass Transfer, 2003; 46: 2857
[24] Tan K K, Tan Y W, Choong T S Y. Powder Technol, 2009; 191: 55
[25] Huang R F,Wan L Q. Phenolic Resin and Application. Beijing: Chemical Industry Press, 2011: 76
[25] (黄荣发,万里强. 氨酚醛树脂及其应用. 北京: 化学工业出版社, 2011: 76)
[26] Zhang J S, Jiang C H, Yang X D, Xu W G. Chin Pat, 201110156447.4, 2011
[26] (张劲松, 姜春海, 杨晓丹, 许卫刚. 中国专利, 201110156447.4, 2011)
Outlines

/

〈 〉