EFFECT OF ANODIZING TREATMENT ON BENDING FATIGUE PROPERTIES OF 2014-T6 ALUMINIUM ALLOY

  • Yanbin ZHANG ,
  • Limin ZHANG ,
  • Jiwang ZHANG ,
  • Jing ZENG
Expand
  • State Key Laboratory of Traction Power, Southwest Jiaotong University, Chengdu 610031

Received date: 2014-01-08

  Revised date: 2014-03-04

  Online published: 2014-06-20

Supported by

Supported by National Natural Science Foundation of China (No.51305363)

Abstract

Anodizing treatment was performed on the notched portion of fatigue specimens of the 2014-T6 aluminium alloy. The thicknesses of the oxide layer induced by the treatment were 5, 10 and 20 μm, respectively. Fatigue tests were carried out on the specimens with and without anodizing treatment using a rotating bending fatigue machine. According to experimental results, the effect of anodizing treatment on the bending fatigue properties of the aluminium alloy was analyzed. In addition, the dependence of the bending fatigue properties of the material upon the thickness of the oxide layer was discussed. The results indicate that the anodizing treatment decreases the bending fatigue life of the aluminium alloy under low and medium stress. With increasing thickness of the oxide layer, the crack initiation site transfers from the oxide layer surface to the substrate surface and the bending fatigue life of the alloy decreases; however, when the oxide layer thickness increases to a certain extent, the S-N curve above the fatigue limit of the alloy does not change even if the thickness continues to increase.

Cite this article

Yanbin ZHANG , Limin ZHANG , Jiwang ZHANG , Jing ZENG . EFFECT OF ANODIZING TREATMENT ON BENDING FATIGUE PROPERTIES OF 2014-T6 ALUMINIUM ALLOY[J]. Acta Metall Sin, 2014 , 50(6) : 715 -721 . DOI: 10.3724/SP.J.1037.2014.00021

References

[1] Heinz A, Haszler A, Keidel C. Mater Sci Eng, 2000; A280: 102
[2] Staley J T, Liu J, Hunt W H J. Adv Mater Proc, 1997; 10: 17
[3] Starke E A, Staley J T. Prog Aerospace Sci, 1996; 32: 131
[4] Liu C, Yao J, Lu W. J Jiamusi Univ, 2006; 24: 559
[4] (刘闯, 姚嘉, 卢伟. 佳木斯大学学报, 2006; 24: 559)
[5] Ding X Q, He G Q, Chen C S, Liu X S, Zhu Z Y. J Mater Sci Eng, 2005; 23: 302
[5] (丁向群, 何国求, 陈成澍, 刘小山, 朱正宇. 材料科学与工程学报, 2005; 23: 302)
[6] Sakai Y. J Jpn Inst Light Met, 2006; 55: 584
[7] Guzman L, Bonini G, Adami M, Ossi P M, Miotello A, Vittori-Antisari M, Serventi A M, Voltolini E. Surf Coat Technol, 1996; 83: 284
[8] Zhang G H, Huang G Q, Xu P, Yu M Z. J China Univ Metrology, 2010; 21: 174
[8] (张高会, 黄国青, 徐鹏, 于明洲. 中国计量学院学报, 2010; 21: 174)
[9] Chu X, Ren X, Hao S Z, Xu Y. Mater Heat Treat, 2010; 39: 123
[9] (初鑫, 任鑫, 郝胜智, 徐洋. 热加工工艺, 2010; 39: 123)
[10] Liu B, Fang Z G, Wang H B, Wang T. Corros Prot, 2012; 33: 1005
[10] (刘斌, 方志刚, 王虹斌, 王涛. 腐蚀与防护, 2012; 33: 1005)
[11] Critchlow G W, Brewis D M. Int J Adhes Adhes, 1996; 16: 255
[12] Fernandes J C S, Ferreira M G S, Haddow D B, Goruppa A, Short R, Dixon D G. Surf Coat Technol, 2002; 154: 8
[13] Critchlow G W, Yendall K A, Bahrani D, Quinn A, Andrews F. Int J Adhes Adhes, 2006; 26: 419
[14] Li Y L. PhD Dissertation, Chongqing University, 2003
[14] (李玉兰. 重庆大学博士学位论文, 2003)
[15] Rodopoilos C A, Romero J S, Curtis S A, Rios E R, Peyre P. ASM Int, 2003; 12: 414
[16] Honda T, Ramulu M, Kobayashi A S. J ASTM Int, 2005; 2: 39
[17] Lonyuk B, Apachitei I, Duszczyk J. Surf Coat Technol, 2007; 201: 8688
[18] Yakovleva N M, Anicai L, Yakovlev A N, Dima L, Khanina E Y, Buda M, Chupakhina E A. Thin Solid Films, 2002; 416: 16
[19] Yan C, Li L J, Jin X Z, Liu J C, Chen P. Chin J Nonferrous Met, 2008; 18: 254
[19] (鄢 锉, 李力钧, 金湘中, 刘继常, 陈 沛. 中国有色金属学报, 2008; 18: 254)
[20] Ferdinand P B, Johnston E R J, Dewolf J T, Mazurek D F. Mechanics of Materials. 6th Ed., New York: McGraw-Hill Companies, 2012: 242
[21] Murakami Y, Endo M. Int J Fatigue, 1994; 16: 163
[22] Nakamura Y, Sakai T, Hirano H, Chandran K S R. Int J Fatigue, 2010; 32: 621
Outlines

/

〈 〉